Microstructure evolution of conventionally cast nickel base superalloy
Source abstract
Abstract
The microstructure evolution of a conventionally cast nickel base superalloy has been investigated during aging treatment at 900°C. It shows that two kinds of γ′ particles existed in the as heat specimens. The finer spherical γ′ ones became notably coarsening. The coarsening kinetics can be approximated by a linear volumetric growth as predicted by LSW theory. The larger cubic γ′ ones sphericised and grew at the expense of finer ones. The primary MC decomposition course was shown in detail, which occurred by the formation of γ′ films, Cr rich M23C6 and Mo rich M6C.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: High Temperature Alloys and Creep · Intermetallics and Advanced Alloy Properties · Advanced Materials Characterization Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (31)
Show source-provided references
1. 10.1016/0956-7151(93)90019-O10.1016/0956-7151(93)90019-O ↗
2. 10.1016/0001-6160(76)90101-210.1016/0001-6160(76)90101-2 ↗
3. 10.1016/0001-6160(78)90035-410.1016/0001-6160(78)90035-4 ↗
4. Johnson W. C. · Metall · 1988 · 2
5. 10.1016/S1359-6462(99)00094-910.1016/S1359-6462(99)00094-9 ↗
6. Cai Y. L., and Zheng Y. R.: in ‘Metallographical investigation in superalloys’, (ed. Y. L. Cai et al., 223-225; 1986, Peking, National Technology Press.
7. 10.1016/0025-5416(79)90157-510.1016/0025-5416(79)90157-5 ↗
8. Ross E. W., and Sims C. T.: in ‘Superalloys II’, (ed.Sims C. T. et al), 97-133; 1984, New York, John Wiley and Sons.
9. 10.1007/BF0264520810.1007/BF02645208 ↗
10. 10.1007/s11661-004-0076-x10.1007/s11661-004-0076-x ↗
11. Zheng Y. R., and Zhang D. T.: in ‘Color metallographic investigation of superalloys and steels’, (ed.Zheng Y. R. et al), 153-161; 1999, Peking, National Technology Press.
12. 10.1007/BF0337876110.1007/BF03378761 ↗
13. 10.2320/jinstmet1952.63.6_72310.2320/jinstmet1952.63.6_723 ↗
14. Morozova G. E. · Metally (Russia) · 1993 · 1 · 38
15. 10.1007/BF0264652310.1007/BF02646523 ↗
16. Zhu P. · Mater. Sci. Frog. (China) · 1989 · 3 · 210
17. Chen Z. Q. · J. Aero. Mater. (China) · 1998 · 18 · 13
18. 10.1016/j.msea.2005.01.01210.1016/j.msea.2005.01.012 ↗
19. 10.1023/A:101538891272910.1023/A:1015388912729 ↗
20. 10.1023/A:101540811601610.1023/A:1015408116016 ↗
21. 10.1016/0956-7151(94)90293-310.1016/0956-7151(94)90293-3 ↗
22. 10.1023/A:101869471675610.1023/A:1018694716756 ↗
23. 10.1007/s11661-002-0325-910.1007/s11661-002-0325-9 ↗
24. 10.1063/1.37155810.1063/1.371558 ↗
25. 10.1016/0022-3697(61)90054-310.1016/0022-3697(61)90054-3 ↗
26. Wagner C. · Electrochem. Z · 1961 · 65 · 581
27. 10.1557/jmr.2005.030910.1557/jmr.2005.0309 ↗
28. Wagner R., Kampmann R., and Voorhees P. W.: in ‘Phase transformation in materials’, (ed. Kostorz G.), 370; 2001, Weinheim, WILEY—VCH.
29. Huang Q. R., and Li H. K.: in ‘Superalloys’, (ed.Huang Q. R. et al), 74; 2000, Peking, Metallurgical Technology Press.
30. Li Y. Q. · 1990 · 26
31. 10.1016/S1359-6454(01)00383-410.1016/S1359-6454(01)00383-4 ↗