journal article·2007-03

Origin of fissures on fracture surfaces of impact samples of HSLA steels with ferrite/pearlite microstructures

B. Mintz, E. Maina, W. B. Morrison

Materials Science and Technology· Volume 23· Issue 3
Publisher page

Abstract

A microstructural examination was carried out investigating the early stages of fissure formation. It was found, in certain steels particularly control rolled, that the tendency to start a fissure, i.e. initiate a crack, which could then propagate parallel to the surface plane in impact tested specimens, was very common. However, whether these grew sufficiently to form deep cracks and relieve the triaxial stress system associated with a notch depended on the degree of grain elongation. Cracks in the early stages of fissure formation were always intergranular, initiated at inclusions or carbide particles that were situated at the boundaries. The further development of the cracks to form a fissure occurred by the decohesion of the grain surfaces until the crack length was sufficient for normal brittle behaviour to take place or the crack had widened to such a degree that the leverage was great enough to make unpeeling of the grain surfaces very easy. Heavily control rolled steels in which the grains had become markedly elongated making crack propagation along the boundaries relatively easy, were therefore, most prone to forming deep fissures. For normalised steels which had essentially an equiaxed grain structure, although cracks initiated at the grain boundaries, they were not able to spread to adjacent grains and growth was stopped abruptly.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Microstructure and Mechanical Properties of Steels · High-Velocity Impact and Material Behavior · Fatigue and fracture mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (20)

Show source-provided references
1. Mintz B., and Morrison W. B.: Mater. Set Technol, to be published (DOT 10.1179/174328407X168801).
2. 10.1179/03071697580327763610.1179/030716975803277636 ↗
3. 10.1179/03071697480328811210.1179/030716974803288112 ↗
4. Korchynsky M., and Stuart H.: Proc. Symp. on ‘Low alloy high strength steels’, Nuremberg, Germany, May 1970, The Metallurgical Companies, pp. 17.
5. 10.1007/BF0264282310.1007/BF02642823 ↗
6. Coleman T., Dulieu D., and Gouch A.: in ‘The microstructure and design of alloys’,Vol. 1, 70; 1973, London, Iron and Steel Institute.
7. Speich G. R., and Dablowski D. S.: in ‘Hot deformation of austenite’, (ed.Ballance J.), 557-597; 1977, New York, AIME.
8. 10.1007/BF0266889010.1007/BF02668890 ↗
9. 10.1179/mt.1978.5.1.3710.1179/mt.1978.5.1.37 ↗
10. Miyoshi E., Fukuda M., Iwanaga H., and Okazawa T.: Proc. Conf. on ‘Crack propagation in pipelines’, Newcastle, UK, March 1974, Institute of Gas Engineering, Paper no. 5.
11. 10.2355/tetsutohagane1955.61.7_99110.2355/tetsutohagane1955.61.7_991 ↗
12. Bramfitt B., and Marder A. R.: in ‘Processing and properties of low C steel’, (ed. Gray J. M.), 191; 1973, New York, AIME.
13. Morrison W. B., Mintz B., and Cochrane R. C.: Proc. Conf. on ‘Controlled processing of HSLA steels’, York, UK, September 1976, British Steel Corporation.
14. 10.1179/mst.1988.4.8.71910.1179/mst.1988.4.8.719 ↗
15. Mintz B., Morrison W. B., Welch P.I., and Davies G. J.: in ‘Texture of materials’, (ed.Gottstein G., and Lucke K.), Vol. 2, 465; 1978, Berlin, Springer-Verlag.
16. 10.1007/BF0264384110.1007/BF02643841 ↗
17. 10.1179/00084437579505032810.1179/000844375795050328 ↗
18. Frier K., Vlad C. M., Kugler J., and Feldman U.: Proc. Conf. on ‘HSLA steels technology and applications’, Philadelphia, PA, USA, October 1983, ASM, 733
19. Rittman R., and Freier K.: Proc. Int. Symp. on ‘Nb’, Orlando, FL, USA, December 2001,571–586.
20. Mintz B., Morrison W. B., Morris P. P., and Davies G. J.: in ‘Texture and properties of materials’, (ed.Davies G. J.), 224-234; 1976, London, The Metals Society.