Reducing machining distortion in AA 6061 alloy through re-heating technique
Source abstract
Abstract
Solution-treated AA 6061 alloy contains residual stresses which cause unwanted deformation during the machining operation rendering the parts unacceptable for use. Usually for AA 6061 alloy, stress relieving is performed by re-heating the parts at 343°C for 1 h. This stress relieving is however accompanied by a considerable loss of material strength which subsequently reduces the functionality of the parts. This paper is based on an effort to evaluate the effectiveness of lower re-heating temperatures for stress relieving without significant loss of strength. Temperatures within the range of 200–343°C were used and treated samples were tested for both the strength and machining distortion. The experimental results indicate 60% reduction in machining distortions with 21% decrease in the strength.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties · Metal Forming Simulation Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Industrial and Manufacturing Engineering, PN Engineering College, National University of Sciences and Technology, PNS Jauhar, Karachi 75350, Pakistan
Department of Engineering Sciences, PN Engineering College, National University of Sciences and Technology, PNS Jauhar, Karachi 75350, Pakistan
Manufacturing and Laser Processing Research Group, School of Mechanical, Aerospace and Civil Engineering, The University of Manchester, Manchester M60 1QD, UK
References (22)
Show source-provided references
1. 10.1016/j.matdes.2014.01.05310.1016/j.matdes.2014.01.053 ↗
2. 10.1016/j.jmatprotec.2004.04.06510.1016/j.jmatprotec.2004.04.065 ↗
3. Fink W. L. · Trans. AIME (Am. Inst. Min. Eng.) · 1948 · 175 · 414
4. 10.1016/S1003-6326(13)62426-710.1016/S1003-6326(13)62426-7 ↗
5. 10.1520/JAI10177010.1520/JAI101770 ↗
6. 10.1007/s11663-013-9997-310.1007/s11663-013-9997-3 ↗
7. DeGarmo P. · 2003
8. Chandler H. · 1996
9. 10.1016/S1044-5803(99)00051-010.1016/S1044-5803(99)00051-0 ↗
10. 10.1007/s12613-013-0721-810.1007/s12613-013-0721-8 ↗
11. 10.1016/S1003-6326(15)63894-810.1016/S1003-6326(15)63894-8 ↗
12. 10.1016/j.msea.2010.12.01110.1016/j.msea.2010.12.011 ↗
13. 10.1016/S0921-5093(02)00073-410.1016/S0921-5093(02)00073-4 ↗
14. 10.1016/j.jmrt.2015.01.00710.1016/j.jmrt.2015.01.007 ↗
15. 10.1016/S1359-6462(00)00577-710.1016/S1359-6462(00)00577-7 ↗
16. 10.5545/sv-jme.2014.189710.5545/sv-jme.2014.1897 ↗
17. Denkena B. · 25th International Congress of the Aeronautical Sciences · 2006
18. Sridhar G. · Adv. Prod. Eng. Manag. · 2015 · 10 · 140
19. Department of Defense USA, Military Standardization Handbook: Aluminum and Aluminum Alloys. US Army Material Research Agency, Department of Defense, 1966.
20. 10.2172/92207310.2172/922073 ↗
21. Sae I. · 2006
22. 10.1179/02670830110151031110.1179/026708301101510311 ↗