Growth kinetics and abrasive wear resistance of boride layers on Fe–15Cr alloy
Source abstract
Abstract
Two boride layers based on the FeB and Fe2B compounds are formed at the interface between an Fe–15Cr alloy and boron at 850–950°C and reaction times up to 12 h, with the average chromium content being around 8 at- in the former and 12 at- in the latter. Both boride layers reveal a pronounced texture. Diffusional growth kinetics of the layers are close to parabolic and can alternatively be described by a system of two non-linear differential equations. Microhardness values are 17·4 GPa for the FeB layer, 14·4 GPa for the Fe2B layer and 0·95 GPa for the Fe–15Cr alloy base. The dry abrasive wear resistance of borided alloy samples is around 45 times greater than that of non-borided ones.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Advanced materials and composites · Metal Alloys Wear and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Physical Chemistry of Inorganic Materials Institute for Problems of Materials Science, Kyiv 03180, Ukraine
References (40)
Show source-provided references
1. Voroshnin LG · 1978
2. Matuschka AG · 1980
3. Voroshnin LG · 1981
4. Sinha AK · 1982
5. Kunst H · 1991 · 16
6. 10.1016/0043-1648(79)90184-410.1016/0043-1648(79)90184-4 ↗
7. 10.1007/BF0055173810.1007/BF00551738 ↗
8. 10.1016/0301-679X(81)90043-810.1016/0301-679X(81)90043-8 ↗
9. 10.1016/0025-5416(82)90078-710.1016/0025-5416(82)90078-7 ↗
10. 10.1016/0043-1648(83)90083-210.1016/0043-1648(83)90083-2 ↗
11. 10.1007/BF0239694610.1007/BF02396946 ↗
12. 10.1016/0040-6090(85)90324-410.1016/0040-6090(85)90324-4 ↗
13. 10.1007/BF0172916510.1007/BF01729165 ↗
14. 10.1557/JMR.1989.135410.1557/JMR.1989.1354 ↗
15. 10.1016/S0921-5093(02)00607-X10.1016/S0921-5093(02)00607-X ↗
16. 10.1016/S0921-5093(02)00910-310.1016/S0921-5093(02)00910-3 ↗
17. 10.1016/S0169-4332(03)00500-210.1016/S0169-4332(03)00500-2 ↗
18. 10.1023/B:JMSC.0000012924.74578.8710.1023/B:JMSC.0000012924.74578.87 ↗
19. 10.1016/j.wear.2003.10.00310.1016/j.wear.2003.10.003 ↗
20. 10.1016/j.jallcom.2004.04.01710.1016/j.jallcom.2004.04.017 ↗
21. 10.1016/j.wear.2005.04.00510.1016/j.wear.2005.04.005 ↗
22. 10.1007/s10853-006-0847-410.1007/s10853-006-0847-4 ↗
23. 10.1016/j.msea.2007.11.08210.1016/j.msea.2007.11.082 ↗
24. 10.1179/174328408X27844810.1179/174328408X278448 ↗
25. Hansen M · 1958
26. 10.1007/s11669-004-0128-310.1007/s11669-004-0128-3 ↗
27. 10.1016/j.jallcom.2005.02.03310.1016/j.jallcom.2005.02.033 ↗
28. 10.1016/S0925-8388(97)00342-310.1016/S0925-8388(97)00342-3 ↗
29. DybkovVI, Lengauer W, Barmak K: ‘Abrasive wear resistance of pack-borided iron–chromium alloys’, Proc. 16th Plansee Seminar, Reutte, Austria, Carl Hanser Verlag, May–June 2005, 999–1009.
30. Mirkin LI · 1961
31. Gorelik SS · 1970
32. 10.1002/pssa.221123021710.1002/pssa.2211230217 ↗
33. 10.1007/BF0110655110.1007/BF01106551 ↗
34. 10.1016/0022-4596(87)90285-410.1016/0022-4596(87)90285-4 ↗
35. Gianoglio C · Metall. Sci. Technol. · 1983 · 1 · 51
36. Bondar A · 2007
37. 10.1007/978-3-642-53297-910.1007/978-3-642-53297-9 ↗
38. 10.1007/978-3-642-52680-010.1007/978-3-642-52680-0 ↗
39. Dybkov · 2002
40. DybkovVI, Goncharuk LV, Khoruzha VG, Meleshevich KA, Samelyuk AV, Sidorko VR: ‘Growth kinetics of boride layers on iron–chromium alloys and their dry abrasive wear resistance’, in Proc. Conf. on ‘Materials science and technology’ (MS&T-2007): ‘Fundamentals and characterization: phase stability, diffusion and their applications’, Detroit, MI, USA, September 2007, American Ceramic Society, 513–524.