journal article·2005-09

Synthesis and some properties of Ti3SiC2by hot pressing of Ti, Si and C powders Part 2 – Mechanical and other properties of Ti3SiC2

S. B. Li, J. X. Xie, L. T. Zhang, L. F. Cheng

Materials Science and Technology· Volume 21· Issue 9
Publisher page

Abstract

Some properties of the remarkable Ti3SiC2 based ceramic synthesised by hot pressing of elemental Ti, Si, and C powders have been investigated. Its flexural strength by using three point bending tests and fracture toughness by using single edge notched beam tests were measured at room temperature to be in the range 310–427 MPa and about 7·MPa m1/2, respectively. This material is a relative 'soft' ceramic with a low hardness of 4 GPa. Ti3SiC2 is similar to the soft metals and is a damage tolerant material that is able to contain the extent of microdamage. An oxidation test has been performed in the temperature range 1000–1400°C in air for 20 h. The oxidation resistance below 1100°C was good. Two oxidized layers were formed, the outer layer consisting of pure rutile-type TiO2, and the inner layer a mixture of SiO2 and TiO2. The average coefficient of thermal expansion (CTE) of Ti3SiC2 was measured to be 9·29 × 10−6 K−1 in the temperature range 25–1400°C. The thermal shock resistance of Ti3SiC2 was evaluated by quenching the samples from 800°C, 1200°C, and 1400°C, respectively. The retained flexural strength drops dramatically at quenching temperature, but shows a slight increase after quenching from 1400°C compared with quenching from 800°C and 1200°C.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: MXene and MAX Phase Materials · Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (20)

Show source-provided references
1. 10.1007/BF0089994910.1007/BF00899949 ↗
2. 10.1111/j.1151-2916.1996.tb08018.x10.1111/j.1151-2916.1996.tb08018.x ↗
3. 10.1016/0025-5408(87)90128-010.1016/0025-5408(87)90128-0 ↗
4. Pampuch R. · J. Mater. Synth. Process · 1993 · 1 · 93
5. 10.1111/j.1151-2916.1997.tb02861.x10.1111/j.1151-2916.1997.tb02861.x ↗
6. 10.1111/j.1151-2916.1998.tb02320.x10.1111/j.1151-2916.1998.tb02320.x ↗
7. 10.1179/02670830122500065310.1179/026708301225000653 ↗
8. 10.1016/S1359-6454(99)00351-110.1016/S1359-6454(99)00351-1 ↗
9. Barsoum M. W. · J. Mater. Synth. Process · 1997 · 5 · 197
10. Rudnik T. · Arch. Metall · 1997 · 42 · 59
11. 10.1023/A:100466450025410.1023/A:1004664500254 ↗
12. 10.1111/j.1151-2916.1999.tb02166.x10.1111/j.1151-2916.1999.tb02166.x ↗
13. Zhou Y. C. · Metsllkd · 2000 · 91 · 329
14. 10.1016/S0925-8388(99)00003-110.1016/S0925-8388(99)00003-1 ↗
15. Barsoum M. W. · Adv. Mater. Process · 1997 · 7 · 51
16. 10.1179/02670830322500607910.1179/026708303225006079 ↗
17. S. B. Li: ‘Microstructure and mechanical properties of layered ceramic Ti3SiC2 and Ti3SiC2/SiC composite by hot-pressing synth-esis’, Postdoctoral research report, Northwestern Polytechnical University, Xi'an, China, 2001.
18. 10.1007/BF0120922110.1007/BF01209221 ↗
19. 10.1016/S0022-3697(98)00313-810.1016/S0022-3697(98)00313-8 ↗
20. El-Raghy T. · J. Am. Ceram. Soc · 1999 · 8 · 285510.1111/j.1151-2916.1999.tb02167.x ↗