Hot strength of creep resistant ferritic steels and relationship to creep rupture data
Source abstract
Abstract
Experimental data on the tensile strength of ferritic steels designed for prolonged service at elevated temperatures have been assessed as a function of many variables, including the testing temperature. The resulting model has been combined with other data on the intrinsic strength of pure ferritic iron and substitutional solute strengthening to show that there is a regime in the temperature range 780–845 K beyond which there is a rapid decline in the microstructural contribution to strength. This decline cannot be attributed to changes in microstructure, but possibly to the ability of dislocations to overcome obstacles with the help of thermal activation. There is evidence of an approximate relationship between the temperature dependence of hot tensile strength and creep rupture stress.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: High Temperature Alloys and Creep · Nuclear Materials and Properties · Fusion materials and technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (29)
Show source-provided references
1. Narayan V., Abad R., Lopez B., Bhadeshia H. K. D. H., and MacKay D. J. C.: ISIJ Int. 1999, 39, 999–1005.10.2355/isijinternational.39.999 ↗
2. 10.1016/S0924-0136(98)00344-610.1016/S0924-0136(98)00344-6 ↗
3. 10.1016/S0965-9978(00)00059-410.1016/S0965-9978(00)00059-4 ↗
4. 10.1016/S0924-0136(00)00461-110.1016/S0924-0136(00)00461-1 ↗
5. 10.1016/j.jmatprotec.2005.05.04010.1016/j.jmatprotec.2005.05.040 ↗
6. Murugananth M., and Bhadeshia H. K. D. H.: in ‘Mathematical modelling of weld phenomena 6’, (ed. H. Cerjak and H. K. D. H. Bhadeshia), 243-260; 2002, London, Maney.
7. 10.1162/neco.1992.4.3.44810.1162/neco.1992.4.3.448 ↗
8. 10.1162/neco.1992.4.3.41510.1162/neco.1992.4.3.415 ↗
9. 10.2355/isijinternational.39.96610.2355/isijinternational.39.966 ↗
10. MacKay D. J. C. ‘Information theory, inference, and learning algorithms’; 2003, Cambridge, Cambridge University Press.
11. 10.1179/mst.1995.11.10.104610.1179/mst.1995.11.10.1046 ↗
12. 10.2355/isijinternational.36.35410.2355/isijinternational.36.354 ↗
13. 10.1016/S0921-5093(97)00701-610.1016/S0921-5093(97)00701-6 ↗
14. Vitek J. M., Iskander Y. S., and Oblow E. M.: Weld J, 2000, 79, 33s-50s.
15. 10.1179/irs.2001.28.1.1510.1179/irs.2001.28.1.15 ↗
16. 10.2355/isijinternational.44.159910.2355/isijinternational.44.1599 ↗
17. Guo Z. · Mater. Sc · 2004 · 12
18. Mukherjee M. · Mater. Sci. Eng. A, 2006, A434 · 237
19. Kojchi Y., Hiroshi I., Hideo T., Masayoshi Y., Osamu K., Kiyoshi K., and Kazuhio K.: INTRIM data sheets lb, 3b, 8b, 1 1 b, 12b, 17b, 18b, 19b, 20b and 21b'; 1994, Tokyo, National Research Institute for Metals.
20. NPL: ‘MTDATA: software’; 2006, Teddington, National Physical Laborator y.
21. 10.1007/BF0267403410.1007/BF02674034 ↗
22. Kalish D. · J. Met · 1965 · 17 · 157
23. 10.1016/0001-6160(82)90075-X10.1016/0001-6160(82)90075-X ↗
24. 10.1016/j.scriptamat.2004.02.02410.1016/j.scriptamat.2004.02.024 ↗
25. 10.1016/j.actamat.2006.08.03310.1016/j.actamat.2006.08.033 ↗
26. 10.1007/BF0268058010.1007/BF02680580 ↗
27. 10.1016/0022-5096(55)90054-510.1016/0022-5096(55)90054-5 ↗
28. 10.1063/1.172187510.1063/1.1721875 ↗
29. Komai N., Masuyama F., Ishihara I., Yokoyama T., Yamadera Y., Okada H., Miyata K., and Sawaragi Y.: in ‘Advanced heat resistant steels for power generation’, 96-109; 1999, London, IOM Communications.