journal article·2011-05

On preventing HAZ cracking in laser welded DS Rene 80 superalloy

L O Osoba, R K Sidhu, O A Ojo

Materials Science and Technology· Volume 27· Issue 5
Publisher page

Abstract

The heat affected zone (HAZ) cracking behaviour in a laser beam directionally solidified (DS) Rene 80 nickel based superalloy subjected to preweld heat treatments was studied. The HAZ cracks in the alloy are grain boundary liquation cracks caused by liquation reaction of both non-equilibrium secondary solidification product, MC carbides and equilibrium solid state reaction product, γ′ precipitates. In contrast to theoretical prediction based a preweld heat treatment that reduced grain boundary liquid film thickness did not result in a lower HAZ cracking, which can be related to concomitant reduction in the ability of the base alloy to relax welding stress. In addition, formation of intergranular M5B3 boride particles in preweld alloy appeared to have aided cracking susceptibility by lowering grain boundary liquation temperature and widening the brittle temperature range in the HAZ during cooling. Based on the analysis of the results, application of a new preweld heat treatment that prevents the formation of the intergranular borides and induces moderate base alloy hardness resulted in a nearly crack free HAZ in laser welded DS Rene 80 superalloy.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · High Temperature Alloys and Creep · High Entropy Alloys Studies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Mechanical and Manufacturing Engineering University of Manitoba, Winnipeg, Manitoba R3T 5V6, Canada

References (26)

Show source-provided references
1. Schafrik R · Adv. Mater. Process. · 2004 · 162 · 33
2. 10.1016/j.actamat.2003.08.02310.1016/j.actamat.2003.08.023 ↗
3. Hashizume R, Yoshinari A, Kiyono T, Murata Y, Morinaga M:in ‘Superalloys 2004’(, Green K A, et al.), 53–62; 2004, Warrendale, PA, TMS.10.7449/2004/Superalloys_2004_53_62 ↗
4. Thamburaj R · Int. Met. Rev. · 1983 · 28 · 110.1179/imr.1983.28.1.1 ↗
5. 10.1179/174328406X13105510.1179/174328406X131055 ↗
6. Krenz D, Egbewande AT, Zhang HR, Ojo OA: Mater. Sci. Technol., In Press.
7. Kelly TJ: ‘Welding metallurgy of investment cast nickel-based superalloys’, in ‘Weldability of materials’, 151–157; 1990, Materials Park, OH, ASM International.
8. 10.1179/imr.1998.43.1.110.1179/imr.1998.43.1.1 ↗
9. Shahsavari HA · Mater. Sci. Technol. · 2007 · 23 · 54810.1179/174328407X179539 ↗
10. Owczarski WA · Weld. J. · 1966 · 45 · 145s
11. 10.1016/j.scriptamat.2003.11.02510.1016/j.scriptamat.2003.11.025 ↗
12. Hillier GS, Bhadeshia HKDH: Proc. Sheffield Centenary Conf. on ‘Perspectives in metallurgical developments’, 183–187; 1984, London, The Metals Society.
13. Sponseller DL: Proc. Superalloys Conf. 1996, (ed. , Kissinger RD, et al.), 259–270; 1996, Warrendale, PA, TMS.10.7449/1996/Superalloys_1996_259_270 ↗
14. 10.1016/0001-6160(67)90104-610.1016/0001-6160(67)90104-6 ↗
15. 10.1016/S0921-5093(97)80011-110.1016/S0921-5093(97)80011-1 ↗
16. 10.1016/j.actamat.2008.09.01010.1016/j.actamat.2008.09.010 ↗
17. 10.1179/imtr.1976.21.1.110.1179/imtr.1976.21.1.1 ↗
18. 10.1016/j.scriptamat.2007.09.04910.1016/j.scriptamat.2007.09.049 ↗
19. 10.1007/s11661-008-9646-710.1007/s11661-008-9646-7 ↗
20. 10.1179/03071698480327480010.1179/030716984803274800 ↗
21. 10.1016/S1359-6454(97)00017-710.1016/S1359-6454(97)00017-7 ↗
22. 10.1007/s11661-001-0350-010.1007/s11661-001-0350-0 ↗
23. 10.1179/13621719910153776110.1179/136217199101537761 ↗
24. 10.1016/j.scriptamat.2005.11.05510.1016/j.scriptamat.2005.11.055 ↗
25. McLean D: ‘Grain boundaries in metals’; 1957, Oxford, Clarendon Press.
26. 10.2320/matertrans1960.22.10910.2320/matertrans1960.22.109 ↗