Formation of eutectic-type microconstituent during transient liquid phase bonding of nickel: Influence of process parameters
Source abstract
Abstract
Transient liquid phase bonding of nickel by a filler material containing phosphorus as a melting point depressant was performed to study the effects of process parameters on the joint microstructure. Insufficient holding time for complete isothermal solidification of liquated insert resulted in formation of eutectic-type microconstituent along the joint centreline region. An increase in the eutectic thickness with increase in initial filler gap size was observed in joints prepared at a constant temperature and holding time. The eutectic was observed to serve as a preferred continuous path for crack initiation and/or propagation. Two different observation of influence of bonding temperature on the eutectic formation was made, one in which increase in bonding temperature resulted in formation of thicker centreline eutectic and the second in which preclusion of the eutectic was achieved at a shorter time relative to a lower temperature.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Electronic Packaging and Soldering Technologies · Advanced Welding Techniques Analysis · Aluminum Alloy Microstructure Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (23)
Show source-provided references
1. 10.1016/j.scriptamat.2006.02.04410.1016/j.scriptamat.2006.02.044 ↗
2. 10.1007/s11661-006-0013-210.1007/s11661-006-0013-2 ↗
3. 10.1179/13621710422501709910.1179/136217104225017099 ↗
4. 10.1016/0924-0136(95)02103-510.1016/0924-0136(95)02103-5 ↗
5. 10.1179/mst.1985.1.8.60810.1179/mst.1985.1.8.608 ↗
6. Demo W. A., and Ferrigno S. J.: Adv. Mater. Process., 1992, 141, 43.
7. Lugscheider E., and Broich U.: Weld. J., 1995, 74, 169s–176s.
8. Lugsscheider E. Schmoor H. and Eritt U.: ‘Brazing high temperature brazing and diffusion welding’ 259-261; 1995 Duesseldorf Deutscher Verlag fur Schweisstechnik GmbH.
9. Duvall D. S. Owczarski W. A. and Paulonis D. F.: Weld. 1 1974 53 203s-214s.
10. 10.1007/s11661-000-0114-210.1007/s11661-000-0114-2 ↗
11. 10.1361/10549719977033572110.1361/105497199770335721 ↗
12. Gale W. F., and Wallach E. R.: Mater. Sci. Eng., 1991, 7, 1143–1148.
13. 10.1007/BF0286899610.1007/BF02868996 ↗
14. 10.1007/BF0258611110.1007/BF02586111 ↗
15. Ramirez J. E. and Liu S.: Weld 1 1992 71 365s.
16. 10.1023/A:101091481387510.1023/A:1010914813875 ↗
17. Ojo O. A. Richards N. L. and Chaturvedi M. C.: Scl Technot Weld Join. 2004 9 532–540.10.1179/174329304X8702 ↗
18. 10.1179/imr.1995.40.5.18110.1179/imr.1995.40.5.181 ↗
19. 10.1007/BF0264928210.1007/BF02649282 ↗
20. Liu S., , Olson D. L., , Martin G. P., and Edwards G. R.: Weld J., 1991, 70, 207s–215s.
21. Crank J.: ‘The mathematics of diffusion’ 2nd edn 37; 1975 Oxford Oxford University Press.
22. Nishimoto K. Saida K. Kim D. and Nakao Y.: ISIJ Int. 1995 35 (10) 1298–1306.10.2355/isijinternational.35.1298 ↗
23. Moelwyn-Hughes E. A.: ‘The kinetics of reaction in solution’ 374; 1947 Oxford Clarredon Press.