Microstructure of alumina ceramic/Ag–Cu–Ti brazing alloy/Kovar alloy joint
Source abstract
Abstract
The microstructure of the alumina ceramic/Kovar alloy joint brazed with Ag–35·2Cu–1·8Ti (wt-%) was studied. The effects of brazing temperature on the microstructure were also discussed. It was found that the microstructure of the joint brazed at 1173 K for 5 min was TiO + TiNi3 + TiFe/eutectic Ag–Cu/TiFe2 + TiNi3/TiFe2 + Cu (s.s) +Ag (s.s). When the brazing temperature was >1193 K, there was no TiO formed on the alumina ceramic/brazing alloy interface.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Intermetallics and Advanced Alloy Properties · Advanced ceramic materials synthesis · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (12)
Show source-provided references
1. Signliano R. · Elect. Pack. Prod · 1996 · 9 · 47
2. Mangin C. G. E. · J. Met · 1993 · 6 · 23
3. 10.1002/9780470294741.ch9510.1002/9780470294741.ch95 ↗
4. 10.1016/S0167-577X(99)00212-810.1016/S0167-577X(99)00212-8 ↗
5. 10.1016/S0955-2219(02)00011-010.1016/S0955-2219(02)00011-0 ↗
6. Durov A. V. · Mater. Sci Eng. A · 2000 · 290 · 8610.1016/S0921-5093(00)00916-3 ↗
7. Vianceo P. T., Stephens J. J., Hlava P. F., and Wlaker C. A.: Weld Res. 2003, 82, 268–277.
8. 10.1016/S1044-5803(00)00095-410.1016/S1044-5803(00)00095-4 ↗
9. 10.1016/S0921-5093(02)00046-110.1016/S0921-5093(02)00046-1 ↗
10. 10.1016/0924-0136(94)01701-210.1016/0924-0136(94)01701-2 ↗
11. 10.1016/S0924-0136(97)00372-510.1016/S0924-0136(97)00372-5 ↗
12. 10.1016/S0272-8842(97)00009-610.1016/S0272-8842(97)00009-6 ↗