Dry sliding wear of TiB2particle reinforced aluminium alloy composites
Source abstract
Abstract
Al–4 wt-%Cu alloy and composites reinforced with 10 and 20 vol.-% of TiB2 particles were prepared by powder metallurgy followed by hot isostatic pressing. The dry sliding wear behaviour of specimens of these materials was investigated. Pin-on-disc measurements showed that the wear resistance of Al–4Cu alloy can be improved dramatically by the addition of 20 vol.-%TiB2 particles. This was due to the high hardness of the TiB2 particles, and to strong particle–matrix bonding. The wear data were found to correlate with SEM observations.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Aluminum Alloys Composites Properties · Microstructure and mechanical properties · Aluminum Alloy Microstructure Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (18)
Show source-provided references
1. 10.1007/978-1-4684-6099-510.1007/978-1-4684-6099-5 ↗
2. 10.1007/s11661-997-0123-510.1007/s11661-997-0123-5 ↗
3. TAHERI-NASSAJ E. · Ser. Mater · 1996 · 34 · 1257
4. 10.1007/BF0115214610.1007/BF01152146 ↗
5. 10.1007/BF0035301810.1007/BF00353018 ↗
6. 10.1016/1359-6454(95)00217-010.1016/1359-6454(95)00217-0 ↗
7. 10.1016/0043-1648(95)06908-910.1016/0043-1648(95)06908-9 ↗
8. 10.1016/S0266-3538(97)00074-210.1016/S0266-3538(97)00074-2 ↗
9. 10.1007/s11661-999-0265-810.1007/s11661-999-0265-8 ↗
10. 10.1179/mst.1993.9.8.72510.1179/mst.1993.9.8.725 ↗
11. 10.1016/0956-716X(92)90107-P10.1016/0956-716X(92)90107-P ↗
12. 10.1007/s11661-999-0213-710.1007/s11661-999-0213-7 ↗
13. 10.1016/S0266-3538(98)00172-910.1016/S0266-3538(98)00172-9 ↗
14. 10.1016/S0266-3538(96)00101-710.1016/S0266-3538(96)00101-7 ↗
15. 10.1007/s11661-997-0237-910.1007/s11661-997-0237-9 ↗
16. 10.1179/mst.1996.12.4.36210.1179/mst.1996.12.4.362 ↗
17. 10.1016/S0266-3538(99)00056-110.1016/S0266-3538(99)00056-1 ↗
18. 10.1063/1.172144810.1063/1.1721448 ↗