Quantitative measurements of the number of cavities per unit area, mean cavity size, and cavitated area fraction are carried out on creep tested specimens of a 12Cr–Mo–V martensitic steel. Both interrupted and ruptured specimens are included. Cavities initiate at an early stage of tests. The number of cavities, mean cavity size, and cavitated area fraction exhibit a continued increase with increasing strain and time. At rupture, the number of cavities is about 30 000 mm−2, and the mean cavity size has a maximum value of about 2·5 μm.The cavitated area fraction is approximately 0·1% at 1% strain, 0·5% at 2% strain, and 10% at rupture. Cavity initiation and growth are analysed regarding temperature, stress, strain, and strain rate. A constrained cavity growth model is discussed and compared with the experimental results.MST/3097
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: High Temperature Alloys and Creep · Metallurgy and Material Forming · Microstructure and Mechanical Properties of Steels

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (12)

Show source-provided references
1. R. WU, P. J. HENDERSON, R. SANDSTROM, and B. G. IVARSSON: in ‘Proceedings of the international conference on materials for combined-cycle power plant’, 111–118; 1991, London, The Institute of Metals.
2. WU R. · Mater. High Temp., · 1994 · 12 · 27710.1080/09603409.1994.11752531 ↗
3. SANDSTROM R. · High Temp. Technol., · 1985 · 3 · 7110.1080/02619180.1985.11753285 ↗
4. De WIRRE M. · Mater. High Temp., · 1991 · 9 · 17810.1080/09603409.1991.11689658 ↗
5. HEDE A. · J. Iron Steel Inst., · 1969 · 207 · 1241
6. 10.1016/0308-0161(91)90090-O10.1016/0308-0161(91)90090-O ↗
7. 10.1016/0921-5093(90)90184-510.1016/0921-5093(90)90184-5 ↗
8. 10.1179/03063458279042719010.1179/030634582790427190 ↗
9. WU R. · Mater. High Temp., · 1992 · 10 · 15410.1080/09603409.1992.11689413 ↗
10. WU R. · Weld. World · 1992 · 30 · 329
11. H. E. EVANS: ‘Mechanisms of creep fracture’, 1984, London and New York, Elsevier Applied Science.
12. 10.1179/03063458179042667910.1179/030634581790426679 ↗