journal article·2009-07

Vacuum hot roll bonding of titanium alloy and stainless steel using nickel interlayer

J. C. Yan, D. S. Zhao, C. W. Wang, L. Y. Wang, Y. Wang, S. Q. Yang

Materials Science and Technology· Volume 25· Issue 7
Publisher page

Abstract

Vacuum hot roll bonding of titanium alloy and stainless steel using a nickel interlayer was investigated. No obvious reaction or diffusion layer occurs at the interface between stainless steel and nickel. The interface between titanium alloy and nickel consists of an occludent layer and diffusion layers, and there are the intermetallic compounds (TiNi3, TiNi, Ti2Ni and their mixtures) in the layers. The total thickness of intermetallic layers at the interface between titanium alloy and nickel increases with the bonding temperature, and the tensile strength of roll bonded joints decreases with the bonding temperature. The maximum tensile strength of 440·1 MPa was obtained at the bonding temperature of 760°C, the reduction of 20% and the rolling speed of 38 mm s–1.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Advanced Welding Techniques Analysis · Microstructure and Mechanical Properties of Steels · Metal Alloys Wear and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

State Key Laboratory of Advanced Welding Production TechnologyDepartment of Welding Science and Engineering, Harbin Institute of Technology, Harbin, 150001, China;, Email: jcyan@hit.edu.cn

State Key Laboratory of Advanced Welding Production TechnologyDepartment of Welding Science and Engineering, Harbin Institute of Technology, Harbin, 150001, China

References (18)

Show source-provided references
1. 10.1016/j.matchar.2005.09.01510.1016/j.matchar.2005.09.015 ↗
2. 10.1016/j.jnucmat.2003.07.00410.1016/j.jnucmat.2003.07.004 ↗
3. 10.1016/S1044-5803(02)00306-610.1016/S1044-5803(02)00306-6 ↗
4. Can G. · Mater. Re · 1998 · 1
5. 10.1007/BF0036790310.1007/BF00367903 ↗
6. 10.1016/j.msea.2004.08.03910.1016/j.msea.2004.08.039 ↗
7. 10.1016/j.msea.2005.07.01010.1016/j.msea.2005.07.010 ↗
8. 10.1016/S1359-6462(01)01041-710.1016/S1359-6462(01)01041-7 ↗
9. 10.1016/j.jmatprotec.2005.06.04510.1016/j.jmatprotec.2005.06.045 ↗
10. 10.1016/0022-5088(90)90347-M10.1016/0022-5088(90)90347-M ↗
11. 10.1179/174328407X15861310.1179/174328407X158613 ↗
12. Kamat G. R.: Weld. 1, 1988, 67, /11 46.10.3406/rebyz.1988.2221 ↗
13. 10.1016/j.msea.2006.03.03410.1016/j.msea.2006.03.034 ↗
14. 10.1016/S1044-5803(99)00008-X10.1016/S1044-5803(99)00008-X ↗
15. Zhao D. S. · Trans. Chn Weld. Inst · 2007 · 27 · 99
16. Zhao D. S. · Sci. Technol. Weld. Join · 2008 · 10 · 4
17. Barlow C. Y., Nielsen P., and Hansen N.: Acta Mater. 2004, 52, 3967–3972.10.1016/j.actamat.2004.05.012 ↗
18. Le H. R., Sutcliffe M. P. F., and Wang P. Z.: Acta Mater. 2004, 52, 911–920.10.1016/j.actamat.2003.10.027 ↗