Investigation on fatigue crack propagation behaviour of novel TiZr-based alloy
Source abstract
Abstract
Fatigue crack propagation behaviour of a novel TiZr-based alloy with two different microstructures was studied at room temperature. The measurements at increasing stress intensity factor range were conducted with loading ratios of 0.1 and 0.6. Based on the measurements, it is found that the alloy with the lamellar microstructure shows fatigue striations and secondary cracks. As to the equiaxed microstructure, many facets are generated instead of striations. Compared with the two cases, the alloy with the lamellar structure exhibits a better resistance to fatigue crack propagation, and the resistance increases with a decrease of stress ratio for both microstructures. Combined with electron backscatter diffraction analysis, the lower crack propagation rate of the lamellar microstructure can be ascribed to crack bifurcation and striation growth.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Titanium Alloys Microstructure and Properties · Intermetallics and Advanced Alloy Properties · Nuclear Materials and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
National United Engineering Laboratory for Advanced Bearing Tribology, Henan University of Science and Technology, Luoyang, People's Republic of China
State Key Laboratory of Metastable Materials Science and Technology, Yanshan University, Qinhuangdao, People's Republic of China
Funding
NSFC
References (38)
Show source-provided references
1. 10.1016/j.cossms.2014.03.00110.1016/j.cossms.2014.03.001 ↗
2. Meyers MA, Chawla KK. Mechanical behavior of materials, 2nd ed. New York:Cambridge University Press; 2009, pp. 713–964.
3. Wood HA · 1979
4. 10.1016/j.ijfatigue.2015.10.00910.1016/j.ijfatigue.2015.10.009 ↗
5. 10.1002/978352761068610.1002/9783527610686 ↗
6. 10.1016/j.msea.2020.13999310.1016/j.msea.2020.139993 ↗
7. 10.1016/j.msea.2010.12.00210.1016/j.msea.2010.12.002 ↗
8. 10.1016/j.msea.2018.09.07310.1016/j.msea.2018.09.073 ↗
9. 10.1557/jmr.2018.19110.1557/jmr.2018.191 ↗
10. 10.1016/j.msea.2017.11.01010.1016/j.msea.2017.11.010 ↗
11. 10.3390/met1009113310.3390/met10091133 ↗
12. 10.1007/s11661-012-1228-z10.1007/s11661-012-1228-z ↗
13. 10.1016/j.matpr.2015.05.01110.1016/j.matpr.2015.05.011 ↗
14. 10.1016/j.ijfatigue.2020.10586810.1016/j.ijfatigue.2020.105868 ↗
15. 10.1016/j.ijplas.2017.09.01210.1016/j.ijplas.2017.09.012 ↗
16. 10.1016/j.ijfatigue.2014.12.01310.1016/j.ijfatigue.2014.12.013 ↗
17. 10.1111/j.1460-2695.2004.00825.x10.1111/j.1460-2695.2004.00825.x ↗
18. 10.1016/j.actamat.2010.11.01510.1016/j.actamat.2010.11.015 ↗
19. 10.1016/j.ijfatigue.2005.07.00110.1016/j.ijfatigue.2005.07.001 ↗
20. 10.1016/j.matdes.2013.06.03910.1016/j.matdes.2013.06.039 ↗
21. 10.1016/j.corsci.2015.08.03810.1016/j.corsci.2015.08.038 ↗
22. 10.1016/j.msea.2016.09.11610.1016/j.msea.2016.09.116 ↗
23. 10.1016/j.matdes.2016.03.06510.1016/j.matdes.2016.03.065 ↗
24. 10.1016/j.jallcom.2016.11.30310.1016/j.jallcom.2016.11.303 ↗
25. ASTM E647-08 · 2008
26. 10.1016/j.msea.2012.04.11410.1016/j.msea.2012.04.114 ↗
27. 10.1007/s12598-012-0531-610.1007/s12598-012-0531-6 ↗
28. Ma Y · Acta Metall Sinica · 2008 · 44 · 973
29. 10.1016/j.msea.2014.09.11210.1016/j.msea.2014.09.112 ↗
30. 10.1007/BF0264687710.1007/BF02646877 ↗
31. 10.1016/0013-7944(70)90028-710.1016/0013-7944(70)90028-7 ↗
32. 10.1016/j.engfracmech.2007.01.01910.1016/j.engfracmech.2007.01.019 ↗
33. Wen AL. · 2011
34. 10.1002/adem.20170070210.1002/adem.201700702 ↗
35. 10.1002/352760211910.1002/3527602119 ↗
36. 10.1016/j.ijfatigue.2008.03.03610.1016/j.ijfatigue.2008.03.036 ↗
37. 10.1016/j.scriptamat.2012.10.04110.1016/j.scriptamat.2012.10.041 ↗
38. 10.1016/j.scriptamat.2011.11.03310.1016/j.scriptamat.2011.11.033 ↗