Investigations of performance characteristics on direct metal laser sintered MONEL K-500 superalloy
Source abstract
Abstract
MONEL K-500 superalloy is difficult to manufacture precisely in traditional manufacturing processes like casting, forming and machining. The direct metal laser sintering (DMLS) process is one of the best metal additive manufacturing processes used in this work. In this work, Laser Power (LP), Scan Speed (SS), Hatch Distance (HD) and Layer Thickness (LT) are used as DMLS process parameters. L09 Orthogonal array is used for printing the MONEL K-500 metal parts. The performance characteristics like ultimate tensile strength (UTS) and surface toughness ( R a ) are improved by 2% and 17% for the Taguchi optimum parameter levels. Contour plots explained the interaction effects of DMLS process parameters on performance characteristics. The better microstructural characteristics obtained the higher optimum parameter level.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · Manufacturing Process and Optimization
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Mechanical Engineering, Sri Ranganathar Institute of Engineering and Technology, Coimbatore, India
Department of Mechanical Engineering, Hindusthan College of Engineering and Technology, Coimbatore, India
Department of Mechanical Engineering, Karpagam Institute of Technology, Coimbatore, India
Department of Mechanical Engineering, OASYS Institute of Technology, Trichy, India
References (45)
Show source-provided references
1. AlMangour B. Additive manufacturing of emerging materials. 1st ed. Cham: Springer; 2018.
2. 10.1080/14686996.2017.136130510.1080/14686996.2017.1361305 ↗
3. 10.1016/j.msea.2006.04.11710.1016/j.msea.2006.04.117 ↗
4. 10.1080/09506608.2016.117628910.1080/09506608.2016.1176289 ↗
5. 10.1007/s40516-019-00094-y10.1007/s40516-019-00094-y ↗
6. 10.21062/ujep/137.2018/a/1213-2489/MT/18/4/55910.21062/ujep/137.2018/a/1213-2489/MT/18/4/559 ↗
7. 10.1007/s00170-016-9367-910.1007/s00170-016-9367-9 ↗
8. 10.1016/j.ijleo.2019.16373510.1016/j.ijleo.2019.163735 ↗
9. 10.1016/j.addma.2018.07.01410.1016/j.addma.2018.07.014 ↗
10. 10.1016/B978-0-12-815732-9.00027-910.1016/B978-0-12-815732-9.00027-9 ↗
11. 10.1016/j.mtcomm.2020.10119510.1016/j.mtcomm.2020.101195 ↗
12. 10.1016/j.jallcom.2020.15756110.1016/j.jallcom.2020.157561 ↗
13. 10.1016/j.jmbbm.2019.10351710.1016/j.jmbbm.2019.103517 ↗
14. 10.1179/1743284715Y.000000005310.1179/1743284715Y.0000000053 ↗
15. 10.1016/j.matchar.2020.11046810.1016/j.matchar.2020.110468 ↗
16. 10.1016/j.jmapro.2021.04.04110.1016/j.jmapro.2021.04.041 ↗
17. 10.1007/s00170-018-2586-510.1007/s00170-018-2586-5 ↗
18. Zhang Y, , Zhang J. Finite element simulation and experimental validation of distortion and cracking failure phenomena in direct metal laser sintering fabricated component. Addit Manuf. 2017;16:49–57.
19. 10.1016/j.jmatprotec.2018.10.02310.1016/j.jmatprotec.2018.10.023 ↗
20. 10.1016/j.addma.2021.10207510.1016/j.addma.2021.102075 ↗
21. 10.1016/j.msea.2015.06.02110.1016/j.msea.2015.06.021 ↗
22. 10.1080/02670836.2021.188509410.1080/02670836.2021.1885094 ↗
23. 10.1016/j.matdes.2018.03.03510.1016/j.matdes.2018.03.035 ↗
24. 10.1016/j.addma.2020.10182110.1016/j.addma.2020.101821 ↗
25. 10.1179/1743284715Y.000000011710.1179/1743284715Y.0000000117 ↗
26. 10.1016/j.addma.2020.10182510.1016/j.addma.2020.101825 ↗
27. 10.1007/s11665-013-0658-010.1007/s11665-013-0658-0 ↗
28. 10.1080/10426914.2016.125780510.1080/10426914.2016.1257805 ↗
29. 10.1016/j.jallcom.2018.12.38010.1016/j.jallcom.2018.12.380 ↗
30. 10.1016/j.msea.2018.08.03710.1016/j.msea.2018.08.037 ↗
31. 10.1016/j.msea.2020.13994710.1016/j.msea.2020.139947 ↗
32. 10.1016/j.msea.2019.05.00710.1016/j.msea.2019.05.007 ↗
33. 10.1179/1743284715Y.000000010810.1179/1743284715Y.0000000108 ↗
34. 10.1002/adem.20140004410.1002/adem.201400044 ↗
35. 10.1016/j.jmst.2014.09.02010.1016/j.jmst.2014.09.020 ↗
36. 10.1016/j.msea.2017.12.04310.1016/j.msea.2017.12.043 ↗
37. 10.1016/B978-0-323-91230-3.00004-410.1016/B978-0-323-91230-3.00004-4 ↗
38. 10.1016/j.corsci.2019.06.03010.1016/j.corsci.2019.06.030 ↗
39. 10.1016/j.msea.2020.13945610.1016/j.msea.2020.139456 ↗
40. Gradl PR Greene SE Protz C . Additive manufacturing of liquid rocket engine combustion devices: a summary of process developments and hot-fire testing results. Proceedings of the Joint Propulsion Conference and American Institute of Aeronautics and Astronautics; 2018 July 9–11; Cincinnati Ohio; 2018 p. 4625.10.2514/6.2018-4625 ↗
41. 10.1016/j.actamat.2022.11830710.1016/j.actamat.2022.118307 ↗
42. 10.1016/j.powtec.2017.01.03010.1016/j.powtec.2017.01.030 ↗
43. 10.1016/j.msea.2015.05.03510.1016/j.msea.2015.05.035 ↗
44. 10.1016/j.jmapro.2020.09.07410.1016/j.jmapro.2020.09.074 ↗
45. 10.1016/j.actamat.2014.05.03910.1016/j.actamat.2014.05.039 ↗