Abstract

In this study, the effects of Mo content and aging temperature on the corrosion characteristics of newly designed hyper duplex stainless steel welds were investigated. Each specimen was aged at 600°C for 1–100 h, and weld cracking occurred when the 6 wt-% Mo specimen was aged for more than 40 h. In addition, electron backscatter diffraction and X-ray diffraction analysis found that the number of secondary phases increased as aging time increased. Based on the potentiodynamic polarisation test for assessing the corrosion characteristics according to the aging time, the corrosion resistance decreased sharply after 40 h, when cracking occurred. Highlights When aging treatment for more than 40 h was performed on 6 wt-% Mo specimen, weld crack occurred. High hardness values above 450 Hv0.5 were measured in specimens aged more than 40 h. Secondary phases such as σ-phase and χ-phase were observed in specimens aged for more than 40 h. The specimens aged for more than 40 h showed a rapid decrease in corrosion resistance.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Welding Techniques and Residual Stresses

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Metallurgical Engineering, Dong-A University, Busan, Republic of Korea

Fundamental Production Engineering Team, Hyundai Mobis, Geyeonggi-do, Republic of Korea

Funding

National Research Foundation of Korea · Ministry of Education

References (31)

Show source-provided references
1. 10.1016/j.msea.2011.12.08710.1016/j.msea.2011.12.087 ↗
2. 10.1016/j.corsci.2011.02.01310.1016/j.corsci.2011.02.013 ↗
3. 10.1016/j.corsci.2014.06.00510.1016/j.corsci.2014.06.005 ↗
4. 10.1016/j.corsci.2009.08.01510.1016/j.corsci.2009.08.015 ↗
5. 10.1007/s40194-018-0548-z10.1007/s40194-018-0548-z ↗
6. 10.1007/s12540-013-3026-610.1007/s12540-013-3026-6 ↗
7. 10.5402/2012/73247110.5402/2012/732471 ↗
8. 10.1016/j.corsci.2012.11.02410.1016/j.corsci.2012.11.024 ↗
9. 10.1016/j.matchar.2008.12.00510.1016/j.matchar.2008.12.005 ↗
10. 10.1590/S1516-1439201300500017010.1590/S1516-14392013005000170 ↗
11. 10.1016/j.msea.2018.05.06310.1016/j.msea.2018.05.063 ↗
12. 10.1016/j.msea.2017.11.07910.1016/j.msea.2017.11.079 ↗
13. 10.1179/1743284713Y.000000036510.1179/1743284713Y.0000000365 ↗
14. Topolska S · J Achiev Mater Manuf Eng · 2009 · 36 · 142
15. 10.5781/KWJS.2010.28.1.02210.5781/KWJS.2010.28.1.022 ↗
16. 10.1016/S1452-3981(23)17369-X10.1016/S1452-3981(23)17369-X ↗
17. 10.1016/j.corsci.2013.04.03310.1016/j.corsci.2013.04.033 ↗
18. 10.1016/j.matdes.2011.07.04110.1016/j.matdes.2011.07.041 ↗
19. Ogawa T · Weld J · 1982 · 61 · 82
20. 10.1016/j.jallcom.2010.12.17410.1016/j.jallcom.2010.12.174 ↗
21. 10.1016/j.msea.2014.04.06510.1016/j.msea.2014.04.065 ↗
22. 10.3390/ma707526810.3390/ma7075268 ↗
23. 10.1007/s11665-015-1793-610.1007/s11665-015-1793-6 ↗
24. 10.1016/j.matchar.2012.10.00610.1016/j.matchar.2012.10.006 ↗
25. 10.12656/jksht.2012.25.2.07410.12656/jksht.2012.25.2.074 ↗
26. 10.1016/j.corsci.2010.10.00910.1016/j.corsci.2010.10.009 ↗
27. 10.5781/KWJS.2013.31.5.2010.5781/KWJS.2013.31.5.20 ↗
28. 10.1016/S1452-3981(23)10854-610.1016/S1452-3981(23)10854-6 ↗
29. 10.1016/j.matchar.2015.12.00410.1016/j.matchar.2015.12.004 ↗
30. 10.5695/JKISE.2015.48.6.32910.5695/JKISE.2015.48.6.329 ↗
31. 10.1016/j.corsci.2016.12.00710.1016/j.corsci.2016.12.007 ↗