Abstract

The microstructure, mechanical properties, and electrical conductivity (EC) of Cu–4Ti–Cr–Fe alloy aged at 773 K in vacuum are studied in this work. The results show that the multiple trace alloying elements have little effect on the microstructure evolution during the aging treatment at 773 K. However, with prolonged aging, the hardness, yield strength, and tensile strength first increase, then decrease. The Cu–4Ti–Cr–Fe alloys show superior hardness and strength performance than other alloys. In both the solid-solution treated and aged cases, the EC decreases if multiple trace alloying elements are added to the Cu–4wt-%Ti alloys, which indicates the CuTi intermetallic compound may have a large negative influence on the EC of copper alloy.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Microstructure and mechanical properties · Aluminum Alloys Composites Properties · Aluminum Alloy Microstructure Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

College of Architecture and Civil Engineering, Taiyuan University of Technology, Taiyuan, People's Republic of China

College of Materials Science and Engineering, Taiyuan University of Technology, Taiyuan, People's Republic of China

Department of Materials Science and Engineering, Missouri University of Science and Technology, Rolla, MO, USA

College of Materials Science and Engineering, Taiyuan University of Science and Technology, Taiyuan, People's Republic of China

Funding

the National Natural Science Foundation of China

References (38)

Show source-provided references
1. 10.1109/TASC.2019.290678110.1109/TASC.2019.2906781 ↗
2. Han K · IEEE Trans Appl Supercond · 2018 · 28 · 1
3. 10.1109/20.51148710.1109/20.511487 ↗
4. 10.1016/j.scriptamat.2004.05.03710.1016/j.scriptamat.2004.05.037 ↗
5. 10.1016/j.jallcom.2014.03.02110.1016/j.jallcom.2014.03.021 ↗
6. 10.1109/20.12002110.1109/20.120021 ↗
7. 10.1016/S0079-6425(03)00029-X10.1016/S0079-6425(03)00029-X ↗
8. 10.1016/j.actamat.2006.07.01310.1016/j.actamat.2006.07.013 ↗
9. 10.1016/j.cub.2009.10.03710.1016/j.cub.2009.10.037 ↗
10. 10.1016/j.scriptamat.2012.11.03310.1016/j.scriptamat.2012.11.033 ↗
11. 10.1016/0001-6160(89)90338-610.1016/0001-6160(89)90338-6 ↗
12. 10.1016/j.msea.2009.03.04710.1016/j.msea.2009.03.047 ↗
13. 10.1016/j.actamat.2007.06.03010.1016/j.actamat.2007.06.030 ↗
14. 10.1016/j.msea.2008.08.02910.1016/j.msea.2008.08.029 ↗
15. 10.1023/A:100460390635910.1023/A:1004603906359 ↗
16. 10.1007/s11661-002-0051-310.1007/s11661-002-0051-3 ↗
17. Piotrowski W · Met Sci J · 2013 · 7 · 502
18. 10.1016/0025-5416(76)90104-X10.1016/0025-5416(76)90104-X ↗
19. 10.1023/A:101527861054310.1023/A:1015278610543 ↗
20. 10.1016/j.msea.2003.12.00210.1016/j.msea.2003.12.002 ↗
21. 10.1007/s11665-007-9082-710.1007/s11665-007-9082-7 ↗
22. 10.1016/j.matchar.2004.12.01010.1016/j.matchar.2004.12.010 ↗
23. 10.1023/A:101791693045910.1023/A:1017916930459 ↗
24. 10.1016/j.msea.2016.01.02710.1016/j.msea.2016.01.027 ↗
25. 10.1371/journal.pcbi.100003210.1371/journal.pcbi.1000032 ↗
26. 10.1016/S1359-6454(02)00594-310.1016/S1359-6454(02)00594-3 ↗
27. 10.1126/science.aar694110.1126/science.aar6941 ↗
28. 10.1023/A:101799140819310.1023/A:1017991408193 ↗
29. 10.1016/j.msea.2017.09.07210.1016/j.msea.2017.09.072 ↗
30. Semboshi S, Numakura H, Gao WL, ‘Effect of Prior Cold-Working on Strength and Electrical Conductivity of Cu-Ti Dilute Alloy Aged in a Hydrogen Atmosphere’, 2010, 1315–1318.10.4028/www.scientific.net/MSF.654-656.1315 ↗
31. 10.1016/S0921-5093(98)00882-X10.1016/S0921-5093(98)00882-X ↗
32. 10.1016/0001-6160(75)90125-X10.1016/0001-6160(75)90125-X ↗
33. 10.1016/j.corsci.2016.05.02910.1016/j.corsci.2016.05.029 ↗
34. 10.1007/BF0264316410.1007/BF02643164 ↗
35. 10.1016/0001-6160(76)90129-210.1016/0001-6160(76)90129-2 ↗
36. 10.1007/BF0077554310.1007/BF00775543 ↗
37. 10.1016/0001-6160(73)90180-610.1016/0001-6160(73)90180-6 ↗
38. 10.1557/jmr.2015.14310.1557/jmr.2015.143 ↗