Abstract

With the aim of improving the surface properties of copper, WC/Ni60A composite coatings were successfully prepared by plasma cladding. A good metallurgical bonding was formed between composite coating and copper substrate. The large amount of dispersed WC and W 2 C phases in the coating significantly increased the microhardness (17 times that of the copper substrate). With the rise in temperature, the wear resistance of the coating first increased and then decreased. At 400°C, the coating had the best wear resistance due to the lubricating effect of the oxide layer. However, due to the simultaneous occurrence of various wear mechanisms, the wear resistance at 600°C was significantly reduced, so the service temperature must be controlled below 600°C.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Advanced materials and composites · Metal and Thin Film Mechanics · High Entropy Alloys Studies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

State Key Laboratory of Advanced Special Steel & Shanghai Key Laboratory of Advanced Ferrometallurgy & School of Materials Science and Engineering, Shanghai University, Shanghai, People's Republic of China

Changli Xingguo Precision Machinery Co., Ltd., Changli, People's Republic of China.

References (20)

Show source-provided references
1. 10.1007/s11015-018-0663-510.1007/s11015-018-0663-5 ↗
2. 10.1016/j.engfailanal.2022.10629410.1016/j.engfailanal.2022.106294 ↗
3. 10.1515/htmp-2014-014910.1515/htmp-2014-0149 ↗
4. 10.1016/j.jmrt.2021.08.11410.1016/j.jmrt.2021.08.114 ↗
5. 10.1016/j.apsusc.2010.02.07810.1016/j.apsusc.2010.02.078 ↗
6. 10.1016/S1672-6529(14)60149-910.1016/S1672-6529(14)60149-9 ↗
7. 10.1016/j.matlet.2006.03.10310.1016/j.matlet.2006.03.103 ↗
8. 10.1016/S0043-1648(03)00526-X10.1016/S0043-1648(03)00526-X ↗
9. 10.1016/j.surfcoat.2019.12523210.1016/j.surfcoat.2019.125232 ↗
10. 10.1016/j.matpr.2019.09.04410.1016/j.matpr.2019.09.044 ↗
11. 10.1016/j.ijrmhm.2016.11.00110.1016/j.ijrmhm.2016.11.001 ↗
12. 10.1016/j.matlet.2021.13088310.1016/j.matlet.2021.130883 ↗
13. 10.1016/j.surfcoat.2005.11.09310.1016/j.surfcoat.2005.11.093 ↗
14. 10.1016/j.wear.2014.12.02110.1016/j.wear.2014.12.021 ↗
15. 10.1016/j.wear.2003.10.01910.1016/j.wear.2003.10.019 ↗
16. 10.1016/j.surfcoat.2020.12564610.1016/j.surfcoat.2020.125646 ↗
17. 10.1016/j.mtcomm.2020.10134210.1016/j.mtcomm.2020.101342 ↗
18. 10.1016/j.surfcoat.2011.07.05710.1016/j.surfcoat.2011.07.057 ↗
19. 10.1016/j.actamat.2020.11654510.1016/j.actamat.2020.116545 ↗
20. 10.1016/j.triboint.2018.06.02210.1016/j.triboint.2018.06.022 ↗