High cyclic fatigue behaviour of ultrafine grained Al 5083 alloy
Source abstract
Abstract
The effects of cryorolling (CR) and CR followed by warm rolling (WR) on high cycle fatigue behaviour of Al 5083 alloy have been investigated in the present work. The Al 5083 alloy samples were rolled for different thickness reductions of 50 and 85 at cryogenic (liquid nitrogen) temperature. Fifty per cent cryorolled samples were subsequently warm rolled at 175°C for 70 reduction (WR). Hardness, tensile strength and fatigue life using constant amplitude stress controlled fatigue were investigated. The microstructural evolution of the alloy was characterised using optical microscopy, SEM and TEM techniques. The cryorolled Al alloy after 85 thickness reduction exhibits high dislocation density due to suppression of dynamic recovery, whereas WR alloy has shown fine subgrain structure in the range of 100–150 nm, associated with dynamic recovery and dynamic aging during WR. The Al 5083 alloy after WR has shown significant enhancement in fatigue strength as compared to the coarse grained solution treated (ST) bulk alloy and CR material. It can be attributed to the formation of fine precipitates during WR, which inhibits dynamic recovery during cyclic deformation; precipitate–dislocation tangled zones inhibits the crack propagation in the alloy.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Microstructure and mechanical properties · Aluminum Alloys Composites Properties · Metal Alloys Wear and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Metallurgical and Materials Engineering Indian Institute of Technology Roorkee, Roorkee 247667, India
References (33)
Show source-provided references
1. 10.1016/S0921-5093(01)01288-610.1016/S0921-5093(01)01288-6 ↗
2. 10.1016/j.actamat.2006.02.04610.1016/j.actamat.2006.02.046 ↗
3. 10.1063/1.164405110.1063/1.1644051 ↗
4. 10.1016/j.scriptamat.2011.10.00510.1016/j.scriptamat.2011.10.005 ↗
5. 10.1038/nature0113310.1038/nature01133 ↗
6. 10.1016/j.scriptamat.2004.02.03710.1016/j.scriptamat.2004.02.037 ↗
7. 10.1016/j.msea.2005.07.04510.1016/j.msea.2005.07.045 ↗
8. 10.1016/j.actamat.2012.10.03810.1016/j.actamat.2012.10.038 ↗
9. 10.1016/S1359-6462(03)00393-210.1016/S1359-6462(03)00393-2 ↗
10. 10.1016/S0921-5093(02)00010-210.1016/S0921-5093(02)00010-2 ↗
11. 10.1016/S0921-5093(00)01682-810.1016/S0921-5093(00)01682-8 ↗
12. 10.1016/S0965-9773(99)00392-X10.1016/S0965-9773(99)00392-X ↗
13. Mughrabi H, Lowe TC, Valiev RZ: ’Investigations and Applications of Severe Plastic Deformation‚, 2000, NATO Science, 241–253.10.1007/978-94-011-4062-1_31 ↗
14. 10.1016/j.scriptamat.2004.05.01210.1016/j.scriptamat.2004.05.012 ↗
15. 10.1007/s11661-007-9110-010.1007/s11661-007-9110-0 ↗
16. 10.1016/j.actamat.2006.09.00210.1016/j.actamat.2006.09.002 ↗
17. 10.1016/j.ijfatigue.2007.04.01510.1016/j.ijfatigue.2007.04.015 ↗
18. 10.1080/0141861020823960110.1080/01418610208239601 ↗
19. 10.1016/j.ijfatigue.2005.08.01410.1016/j.ijfatigue.2005.08.014 ↗
20. 10.1016/j.ijfatigue.2010.11.02510.1016/j.ijfatigue.2010.11.025 ↗
21. 10.1007/s12613-013-0794-410.1007/s12613-013-0794-4 ↗
22. 10.1016/j.matdes.2013.02.06810.1016/j.matdes.2013.02.068 ↗
23. 10.1016/j.msea.2009.11.05610.1016/j.msea.2009.11.056 ↗
24. 10.1016/j.matdes.2012.02.01010.1016/j.matdes.2012.02.010 ↗
25. 10.1007/s10853-010-4573-610.1007/s10853-010-4573-6 ↗
26. 10.1016/j.msea.2009.10.00710.1016/j.msea.2009.10.007 ↗
27. 10.1016/j.msea.2012.11.01010.1016/j.msea.2012.11.010 ↗
28. 10.1016/S0921-5093(99)00716-910.1016/S0921-5093(99)00716-9 ↗
29. 10.1016/S0921-5093(00)00796-610.1016/S0921-5093(00)00796-6 ↗
30. Suresh S: 1998, Cambridge, Cambridge University Press.
31. Yelagin V · Met. Sci. Heat Treat. · 2002 · 9 · 10
32. 10.1007/BF0270422510.1007/BF02704225 ↗
33. 10.1007/s11661-998-0325-510.1007/s11661-998-0325-5 ↗