Review of bioresorbable AZ91, AZ31 and Mg–Zn–Ca implants and their manufacturing methods
Source abstract
Abstract
In this paper, the magnesium alloys, such as AZ91, AZ31 and Mg–Zn–Ca are reviewed for the bioimplants application. A perspective of controlling the high degradation rate of Mg alloys is discussed by alloying, manufacturing methods, surface coating and surface treatment. The major constraint while using magnesium as an implant is the stress-shielding effect, which can be resolved by producing the Mg implant with Young's modulus closer to the cortical bones. The latest development for minimising the stress-shielding effect is by creating a porous magnesium scaffold although a change in fatigue resistance is unavoidable. The influence of manufacturing methods, such as die-casting, powder metallurgy, rolling and additive manufacturing is also discussed on the mechanical strength and degradation behaviour.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Magnesium Alloys: Properties and Applications · Aluminum Alloys Composites Properties · Corrosion Behavior and Inhibition
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Mechanical Engineering, Mepco Schlenk Engineering College, Sivakasi, India
Centre for Biomaterials, Cellular and Molecular Theranostics, VIT University, Vellore, India
Department of Mechanical Engineering, SRM Institute of Science and Technology, Chennai, India
Department of Mechanical Engineering, Rajalakshmi Institute of Technology, Chennai, India
Faculty of Mechanical Engineering, Kalasalingam Academy of Research and Education, Krishnankoil, Tamil Nadu, India
References (100+)
Show source-provided references
1. 10.1016/j.pmatsci.2017.04.01110.1016/j.pmatsci.2017.04.011 ↗
2. 10.1097/00004669-199701000-0000910.1097/00004669-199701000-00009 ↗
3. 10.1016/j.eng.2020.04.01510.1016/j.eng.2020.04.015 ↗
4. 10.1016/j.jallcom.2016.05.25610.1016/j.jallcom.2016.05.256 ↗
5. 10.1016/j.jma.2018.02.00310.1016/j.jma.2018.02.003 ↗
6. 10.1007/s11706-013-0210-z10.1007/s11706-013-0210-z ↗
7. 10.1016/B978-0-08-100497-5.00003-310.1016/B978-0-08-100497-5.00003-3 ↗
8. 10.3109/1745367810899177610.3109/17453678108991776 ↗
9. 10.3390/ijms1604747810.3390/ijms16047478 ↗
10. Pogorielov M · Int Med Appl Sci · 2017 · 9 · 27
11. 10.1016/j.jma.2021.06.02410.1016/j.jma.2021.06.024 ↗
12. Bilezikian JP · 2008
13. 10.1002/adem.20050001310.1002/adem.200500013 ↗
14. 10.1080/0951192X.2013.83447510.1080/0951192X.2013.834475 ↗
15. 10.1007/978-3-319-48223-1_7810.1007/978-3-319-48223-1_78 ↗
16. 10.1016/j.actbio.2012.01.01810.1016/j.actbio.2012.01.018 ↗
17. 10.1016/j.msec.2015.01.02910.1016/j.msec.2015.01.029 ↗
18. 10.3390/ma1008088410.3390/ma10080884 ↗
19. 10.1016/j.matlet.2018.12.01310.1016/j.matlet.2018.12.013 ↗
20. 10.1016/j.surfin.2018.11.01110.1016/j.surfin.2018.11.011 ↗
21. 10.3109/1745367860899439310.3109/17453678608994393 ↗
22. 10.1166/jbt.2012.105910.1166/jbt.2012.1059 ↗
23. 10.1016/j.msea.2020.14034110.1016/j.msea.2020.140341 ↗
24. 10.1016/j.ceramint.2020.09.19710.1016/j.ceramint.2020.09.197 ↗
25. 10.1016/j.jma.2019.09.01110.1016/j.jma.2019.09.011 ↗
26. 10.5772/4833510.5772/48335 ↗
27. 10.1016/j.corsci.2007.11.00510.1016/j.corsci.2007.11.005 ↗
28. 10.3390/met902018610.3390/met9020186 ↗
29. 10.1016/j.actbio.2012.04.02810.1016/j.actbio.2012.04.028 ↗
30. Krause C, Bormann D, Hassel T Mechanical properties of degradable magnesium implants in dependence of the implantation duration. In: Magnesium technology in the global age; 2007. p. 329–370.
31. 10.1088/1748-6041/6/4/04500310.1088/1748-6041/6/4/045003 ↗
32. 10.3390/ma704253410.3390/ma7042534 ↗
33. 10.1016/j.corsci.2009.09.03310.1016/j.corsci.2009.09.033 ↗
34. 10.1002/adem.20070020010.1002/adem.200700200 ↗
35. 10.1177/228080001775035910.1177/2280800017750359 ↗
36. 10.1002/maco.20130758810.1002/maco.201307588 ↗
37. Zhang X-b · Chin J Nonferrous Met · 2013 · 23 · 905
38. 10.1557/jmr.2018.31110.1557/jmr.2018.311 ↗
39. 10.1007/s10856-017-5973-910.1007/s10856-017-5973-9 ↗
40. 10.1002/jbm.a.3127310.1002/jbm.a.31273 ↗
41. Istrate B · 2016
42. 10.1016/S1003-6326(11)60705-X10.1016/S1003-6326(11)60705-X ↗
43. 10.1016/j.actbio.2017.11.03210.1016/j.actbio.2017.11.032 ↗
44. 10.1007/s10103-017-2174-110.1007/s10103-017-2174-1 ↗
45. 10.3390/app808130610.3390/app8081306 ↗
46. 10.1016/j.actbio.2009.10.00610.1016/j.actbio.2009.10.006 ↗
47. 10.1093/rb/rbx00410.1093/rb/rbx004 ↗
48. 10.1016/j.actbio.2014.07.00510.1016/j.actbio.2014.07.005 ↗
49. 10.1016/j.matdes.2008.04.01710.1016/j.matdes.2008.04.017 ↗
50. 10.1016/S0921-5093(03)00334-410.1016/S0921-5093(03)00334-4 ↗
51. 10.1007/s11665-008-9259-810.1007/s11665-008-9259-8 ↗
52. 10.1016/j.msea.2009.06.02110.1016/j.msea.2009.06.021 ↗
53. Metals ACG-oCo. Standard practice for laboratory immersion corrosion testing of metals. ASTM International; 2004.
54. Tomashov ND. Theory of corrosion and protection of metals. New York: Macmillan; 1965.
55. 10.1016/S1369-7021(09)70273-110.1016/S1369-7021(09)70273-1 ↗
56. 10.1016/S0010-938X(03)00190-210.1016/S0010-938X(03)00190-2 ↗
57. 10.1016/j.colsurfb.2014.02.03010.1016/j.colsurfb.2014.02.030 ↗
58. 10.1116/1.269937110.1116/1.2699371 ↗
59. 10.1016/j.apsusc.2012.09.11610.1016/j.apsusc.2012.09.116 ↗
60. 10.1016/S0257-8972(02)00671-010.1016/S0257-8972(02)00671-0 ↗
61. 10.1016/j.surfcoat.2004.07.05610.1016/j.surfcoat.2004.07.056 ↗
62. 10.1016/j.msec.2013.05.01410.1016/j.msec.2013.05.014 ↗
63. 10.1016/j.apsusc.2017.01.02210.1016/j.apsusc.2017.01.022 ↗
64. 10.1016/j.surfcoat.2008.01.00410.1016/j.surfcoat.2008.01.004 ↗
65. 10.1016/j.matpr.2018.04.16910.1016/j.matpr.2018.04.169 ↗
66. 10.1016/j.msec.2014.11.02010.1016/j.msec.2014.11.020 ↗
67. 10.1016/j.surfcoat.2009.02.07410.1016/j.surfcoat.2009.02.074 ↗
68. 10.1016/j.msec.2017.03.01910.1016/j.msec.2017.03.019 ↗
69. 10.1016/B0-08-042993-9/00017-610.1016/B0-08-042993-9/00017-6 ↗
70. 10.1007/s11665-018-3278-x10.1007/s11665-018-3278-x ↗
71. 10.1016/j.electacta.2013.12.10910.1016/j.electacta.2013.12.109 ↗
72. 10.3390/ma911092510.3390/ma9110925 ↗
73. Spange S. · 2006
74. Avedesian MM · 1999
75. 10.1016/j.msec.2011.07.01510.1016/j.msec.2011.07.015 ↗
76. Baker H · 1999 · 1
77. 10.1016/j.corsci.2019.01.02410.1016/j.corsci.2019.01.024 ↗
78. 10.1016/S0010-938X(98)00121-810.1016/S0010-938X(98)00121-8 ↗
79. 10.1016/j.jma.2019.01.00510.1016/j.jma.2019.01.005 ↗
80. 10.1155/2015/94360310.1155/2015/943603 ↗
81. 10.1016/S1003-6326(18)64819-810.1016/S1003-6326(18)64819-8 ↗
82. 10.1016/j.corsci.2011.05.03510.1016/j.corsci.2011.05.035 ↗
83. 10.1155/2010/41212910.1155/2010/412129 ↗
84. Suman C. · SAE Trans · 1990 · 849
85. 10.1109/TNB.2014.233893110.1109/TNB.2014.2338931 ↗
86. 10.2320/matertrans.M201019210.2320/matertrans.M2010192 ↗
87. 10.1088/1757-899X/98/1/01202710.1088/1757-899X/98/1/012027 ↗
88. 10.1016/S0257-8972(98)00399-510.1016/S0257-8972(98)00399-5 ↗
89. 10.1016/j.matlet.2007.12.05210.1016/j.matlet.2007.12.052 ↗
90. 10.1007/s11837-012-0341-110.1007/s11837-012-0341-1 ↗
91. 10.1016/j.surfcoat.2019.01.05210.1016/j.surfcoat.2019.01.052 ↗
92. 10.1016/j.jtice.2015.07.02810.1016/j.jtice.2015.07.028 ↗
93. 10.1016/j.surfin.2018.12.00610.1016/j.surfin.2018.12.006 ↗
94. 10.1016/j.corsci.2018.06.01810.1016/j.corsci.2018.06.018 ↗
95. 10.1016/j.jmbbm.2018.02.00110.1016/j.jmbbm.2018.02.001 ↗
96. 10.1016/S1003-6326(10)60232-410.1016/S1003-6326(10)60232-4 ↗
97. Weijiu Huang ML, Li Z Thickness effects on corrosion and wear resistance properties of micro-arc discharge oxide coatings on AZ91D magnesium alloys. Trans Nonferrous Met Soc China. 2006;3.
98. 10.1016/S1003-6326(18)64873-310.1016/S1003-6326(18)64873-3 ↗
99. 10.1016/j.jallcom.2019.01.12110.1016/j.jallcom.2019.01.121 ↗
100. 10.1039/C3TB21746A10.1039/C3TB21746A ↗