journal article·2012-06

Effect of different solution heattreatments on hot ductility of superalloysPart 2 – Allvac 718Plus

J Andersson, G P Sjöberg, L Viskari, M Chaturvedi

Materials Science and Technology· Volume 28· Issue 6
Publisher page

Abstract

The hot ductility of Allvac 718Plus for different solution heat treatments (954°C–15 h, 954°C–1 h, 982°C–1 h and 1050°C–3 h+954°C–1 h) has been investigated using Gleeble testing. Substantial variations in the microstructure among the heat treatments affected the Gleeble test hot ductility only to a very limited extent. Constitutional liquation of the NbC phase was found to be the main cause for the poor ductility at high testing temperatures in the on-heating cycle as well as at the lower temperatures on-cooling. Grain boundary δ phase was seen to assist the constitutional liquation of the NbC phase. Based on established evaluation criteria for Gleeble ductility testing, a ranked indicator for weldability is suggested.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: High Temperature Alloys and Creep · Aluminum Alloy Microstructure Properties · Microstructure and Mechanical Properties of Steels

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Materials Technology, Volvo Aero Corporation, Trollhättan, Sweden

Department of Materials and Manufacturing Technology, Chalmers University of Technology, Gothenburg, Sweden

Department of Applied Physics, Chalmers University of Technology, Gothenburg, Sweden

Department of Mechanical and Industrial Engineering, University of Manitoba, Winnipeg, MB, Canada

References (25)

Show source-provided references
1. Sims CT, Stoloff NS, Hagel WC: ‘Superalloys II’; 1987, Hoboken, NJ, John Wiley & Sons.
2. 10.1002/adem.20090028210.1002/adem.200900282 ↗
3. 10.7449/2005/Superalloys_2005_179_19110.7449/2005/Superalloys_2005_179_191 ↗
4. Andersson J, Hatami S, Sjöberg G: ‘Notch sensitivity and intergranular crack growth in the Allvac 718Plus superalloy’, Proc. 18th Int. Symp. on ‘Air breathing engines’, International Association of Airbreathing Engines, Beijing, China, September 2007, Paper 1293.
5. Qian M: ‘An investigation of the repair weldability of Waspaloy and alloy 718’, PhD thesis, The Ohio State University, Columbus, OH, USA, 2002.
6. Vishwakarma K: ‘Microstructural analysis of weld cracking in 718 Plus superalloy’, PhD thesis, University of Manitoba, Winnipeg, MB, Canada, 2007.
7. 10.1007/BF0265899910.1007/BF02658999 ↗
8. 10.1051/metal/19767312081710.1051/metal/197673120817 ↗
9. 10.1016/0001-6160(85)90231-710.1016/0001-6160(85)90231-7 ↗
10. Andersson J · 2012 · 28 · 609
11. ‘Aerospace material specification no. AMS 5441’, SAE International, Warrendale, PA, USA, 2006.
12. Andersson J, Hatami S: ‘Notch sensitivity and grain boundary embrittlement in Allvac 718Plus – effect of δ-phase morphology’, Master's thesis, The Royal Institute of Technology, Stockholm, Sweden, 2006.
13. 10.1016/j.msea.2010.11.08010.1016/j.msea.2010.11.080 ↗
14. Lippold JC, Kiser SD, DuPont JN: ‘Welding metallurgy and weldability of nickel-base superalloys’; 2009, Hoboken, NJ, John Wiley & Sons.
15. Nippes EF · Weld. J. · 1949 · 28 · 534
16. Yeniscavich W: ‘Correlation of hot ductility curves with cracking during welding’, Proc. Symp. on ‘Methods of high alloy weldability evaluation’, New York, USA, April 1969, WRC, 2–12.
17. Lundin CD · Weld. J. · 1993 · 72 · 189
18. 10.7449/2005/Superalloys_2005_165_17710.7449/2005/Superalloys_2005_165_177 ↗
19. 10.1179/174328408X31108010.1179/174328408X311080 ↗
20. 10.1016/j.msea.2007.08.00210.1016/j.msea.2007.08.002 ↗
21. 10.1179/174328407X24303210.1179/174328407X243032 ↗
22. Ojo OA · Mater. Sci. Technol. · 2011 · 27 · 161010.1179/026708311X13081465539881 ↗
23. 10.1007/s11661-002-0033-510.1007/s11661-002-0033-5 ↗
24. Dieter GE: ‘Mechanical metallurgy, SI metric edition’; 1988, Singapore, McGraw-Hill.
25. 10.1179/1362171811Y.000000007710.1179/1362171811Y.0000000077 ↗