Influence of nickel and cobalt on microstructure of silicon solution strengthened ductile iron
Source abstract
Abstract
‘Second Generation’ ductile iron with a silicon content of up to 4.3 wt- exhibits a fully ferritic matrix, which is solution strengthened by silicon. Outstanding advantages of these ductile iron grades result in their strongly increasing demand. However, due to a presumed formation of a silicon long range order, the maximum strength is limited to 600 MPa at 4.3 wt- silicon. At higher silicon content, the mechanical properties dramatically decrease. In order to increase the maximum achievable strength, the potential of additional solution strengthening elements is subject of present research. Initially, the effects of cobalt and nickel on matrix, graphite shape and nodule count are investigated. Cobalt and nickel are identified as promising candidates for further solid solution hardening.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Microstructure and Mechanical Properties of Steels · Metal Alloys Wear and Properties · Advanced Surface Polishing Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Foundry-Institute RWTH Aachen University, Intzestrasse 5, 52072 Aachen, Germany
References (43)
Show source-provided references
1. 10.1179/1743133613Y.000000009510.1179/1743133613Y.0000000095 ↗
2. 10.1016/j.msea.2006.09.02710.1016/j.msea.2006.09.027 ↗
3. 10.1007/BF0035588310.1007/BF00355883 ↗
4. 10.1016/j.msea.2012.12.08910.1016/j.msea.2012.12.089 ↗
5. 10.1016/j.msea.2012.06.06210.1016/j.msea.2012.06.062 ↗
6. Ismaeel AR · Asian J. Chem. · 2007 · 19 · 4665
7. 10.2355/isijinternational.42.25710.2355/isijinternational.42.257 ↗
8. Labrecque C · Trans. Am. Foundry Soc. · 2010 · 118 · 233
9. 10.1016/j.matchar.2007.09.00110.1016/j.matchar.2007.09.001 ↗
10. 10.1179/174328407X18591010.1179/174328407X185910 ↗
11. 10.1016/j.wear.2005.09.01510.1016/j.wear.2005.09.015 ↗
12. 10.1016/j.msea.2008.09.08210.1016/j.msea.2008.09.082 ↗
13. 10.1016/j.jmatprotec.2007.05.05610.1016/j.jmatprotec.2007.05.056 ↗
14. 10.1179/1743133612Y.000000004610.1179/1743133612Y.0000000046 ↗
15. 10.2320/matertrans.44.141910.2320/matertrans.44.1419 ↗
16. 10.1016/j.msea.2006.09.05810.1016/j.msea.2006.09.058 ↗
17. 10.2355/isijinternational.54.24810.2355/isijinternational.54.248 ↗
18. 10.2320/matertrans.45.246310.2320/matertrans.45.2463 ↗
19. 10.2355/isijinternational.52.113010.2355/isijinternational.52.1130 ↗
20. 10.1016/j.msea.2014.03.05710.1016/j.msea.2014.03.057 ↗
21. Bjorkegren LE and Hamberg K: ‘Silicon alloyed ductile iron with excellent ductility and machinability’, Keith D. Millis World Symp. on ‘Ductile iron’, Hilton Head, SC, USA, October 2003, Ductile Iron Society.
22. Larker R: ‘Solution strengthened ferritic ductile iron ISO 1083/JS/500-10 provides superior consistent properties in hydraulic rotators’, 2008.
23. 10.1007/BF0335558010.1007/BF03355580 ↗
24. 10.1016/j.jmatprotec.2005.02.04010.1016/j.jmatprotec.2005.02.040 ↗
25. Lekakh S · AFS Trans. · 2012 · 120 · 319
26. 10.1361/10599499877034786410.1361/105994998770347864 ↗
27. Menk W · Giesserei · 2005 · 92 · 66
28. 10.1007/BF0268058010.1007/BF02680580 ↗
29. Cho GS · J. Mater. Sci. Technol. · 2007 · 23 · 9710.1179/174328407X158488 ↗
30. Reynolds CF · AFS Trans. · 1952 · 60 · 635
31. 10.1016/j.msea.2008.10.01910.1016/j.msea.2008.10.019 ↗
32. Kawano Y · J. Jpn Foundrym. Soc. · 1987 · 59 · 531
33. Thury W · Giesserei-Praxis · 1967 · 1 · 273
34. Modl E · Giesserei · 1968 · 55 · 244
35. 10.1179/mst.1995.11.9.89310.1179/mst.1995.11.9.893 ↗
36. Kleinkroeger W, Stellmacher J, Warnke EP, Robertz H, Minkner U and Tenbrink HB: ‘Gusswerkstoff mit ferritischem Gefüge und Kugelgraphit, insbesondere ferritisches Gusseisen’, DE10101159A1, 2002.
37. Kleinkröger WDI and Warnke EPP: ‘Cast iron composition for high stress applications comprises (in wt.) 2.5–3.5 carbon, 2.5–4.5 silicon, maximum 2.5 nickel, 0.10–0.45 niobium, maximum 0.4 manganese, 0.01–0.10 magnesium, maximum 0.004 cerium, 0.001–0.004 antimony’, DE102004045612A1, 2006.
38. Velichko A: ‘Quantitative 3D characterization of graphite morphologies in cast iron using FIB microstructure tomography’, Dissertation, Saarbrucken, 2008.10.1002/adem.200600175 ↗
39. Gundlach R: ‘Nodularity, its measurement, and its correlation with mechanical properties of ductile iron’, DIS Research Project, 2006, (37).
40. 10.1016/j.jmatprotec.2007.10.07510.1016/j.jmatprotec.2007.10.075 ↗
41. 10.1007/BF0268058010.1007/BF02680580 ↗
42. Anon. ‘Gusswerkstoff mit ferritischem gefüge und kugelgraphit, insbesondere ferritisches gusseisen’, DE10101159C2, 2003.
43. Anon. ‘Cast iron with ferritic structure and containing spheroidal graphite also contains silicon, nickel, niobium, manganese, magnesium, cerium and antimony, remainder being iron and impurities’, DE102004045613A1, 2006.