journal article·2017-11

Sulphide stress cracking of 17-4 PH for applications in oilfield components

Mario Sergio Della Roverys Coseglio

Materials Science and Technology· Volume 33· Issue 16
Publisher page

Abstract

The precipitation-hardening stainless steel 17-4 PH is widely used for oilfield components (tubing hangers and valve stems) due to its favourable combination of high strength and corrosion resistance. In oil and gas production systems containing hydrogen sulphide (H 2 S), however, this material is highly susceptible to sulphide stress cracking (SSC). Numerous investigations conducted in the past decades outlined its corrosion performance and confirmed its cracking propensity. These studies indicated failures by SSC at low stress levels and highlighted the effects of the main environmental variables: partial pressure of H 2 S, environment pH, temperature and chloride content. This review describes a series of surface modification techniques, particularly the low-temperature plasma nitriding, which can potentially be used to prevent SSC. This review was submitted as part of the 2017 Materials Literature Review Prize of the Institute of Materials, Minerals and Mining run by the Editorial Board of MST. Sponsorship of the prize by TWI Ltd is gratefully acknowledged
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Material Properties and Failure Mechanisms

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

School of Metallurgy and Materials, University of Birmingham, Birmingham, UK

Funding

Coordenação de Aperfeiçoamento de Pessoal de Nível Superior · University of Birmingham

References (100+)

Show source-provided references
1. Slunder CJ, Hoenie AF, Hall AM. Thermal and mechanical treatment for precipitation-hardening stainless steel. 1967. (NASA-SP-50).10.2172/4551454 ↗
2. Badrak RP. Investigation of limits for UNS S17400 in H 2 S containing environments. In: NACE Corrosion 2017. NACE International; 2014. (Paper 3816).10.5006/C2014-3816 ↗
3. Rashmi Bhavsar PE, Silverman S, MacWilliam D. Successful use of 17-4PH components in well equipment in sour oilfield environments. In: NACE Corrosion 2004. NACE International; 2004. (Paper 04120).10.5006/C2004-04120 ↗
4. Ikeda A · Chem Econ Eng Rev · 1978 · 10 · 12
5. Fraser JP · Eight Annual Conference · 1952 · 29
6. NACE MR0175/ISO 15156-3. Petroleum and natural gas industries – environments in oil and gas production – Part 3: Cracking-resistant CRAs (corrosion-resistant alloys) and other alloys. American National Standards Institute (ANSI)/NACE International 2009; 2009.
7. Prepared by the Working Party on Corrosion in Oil and Gas Production. Guidelines on Materials Requirements for Carbon and Low Alloy Steels for H 2 S-Containing Environments in Oil and Gas Production (EFC 16 – 3rd Edition); 2009.
8. Prepared by the Working Party on Corrosion in Oil and Gas Production. Corrosion Resistant Alloys for Oil and Gas Production – Guidance on General Requirements and Test Methods for H 2 S Service: (EFC 17 – 2nd Edition); 2002.
9. NACE International Work Group T-1F-21g. Use of corrosion-resistant alloys in oilfield environments. 2000. (192).
10. United States Environmental Protection Agency. Report to Congress on Hydrogen Sulfide Air Emissions Associated With the Extraction of Oil and Natural Gas. 1993. Available from:
11. 10.1139/cjc-2015-042510.1139/cjc-2015-0425 ↗
12. NACE MR0175/ISO 15156-1. Petroleum and natural gas industries – Materials for use in H 2 S-containing environments in oil and gas production – Part 1: general principles for selection of cracking-resistant materials. American National Standards Institute (ANSI)/NACE International; 2009.
13. 10.1787/weo-2008-en10.1787/weo-2008-en ↗
14. International Energy Agency. Resources to reserves 2013 – oil, gas and coal technologies for the energy markets of the future. 2013. Available from:
15. Guyer HH. · 1998 · 4
16. Smith L, Craig B. Corrosion mechanisms and material performance in environments containing hydrogen sulfide and elemental sulfur. In: SACNUC Workshop, Brussels; 2008 Oct 22–23; 2008.
17. 10.1016/j.ijggc.2012.12.02810.1016/j.ijggc.2012.12.028 ↗
18. 10.1016/j.corsci.2012.03.00610.1016/j.corsci.2012.03.006 ↗
19. 10.1520/A0564_A0564M-1310.1520/A0564_A0564M-13 ↗
20. 10.1016/j.corsci.2013.11.03910.1016/j.corsci.2013.11.039 ↗
21. 10.1016/j.corsci.2013.12.01510.1016/j.corsci.2013.12.015 ↗
22. 10.1007/s11663-012-9781-910.1007/s11663-012-9781-9 ↗
23. 10.1016/j.msea.2013.01.01110.1016/j.msea.2013.01.011 ↗
24. 10.1016/S0010-938X(02)00023-910.1016/S0010-938X(02)00023-9 ↗
25. 10.1002/maco.1995046060510.1002/maco.19950460605 ↗
26. 10.1016/j.msea.2011.12.00410.1016/j.msea.2011.12.004 ↗
27. 10.1016/S1359-6462(02)00310-X10.1016/S1359-6462(02)00310-X ↗
28. 10.1016/j.matchar.2007.04.01810.1016/j.matchar.2007.04.018 ↗
29. 10.2320/matertrans.48.49010.2320/matertrans.48.490 ↗
30. 10.1016/S0254-0584(01)00460-610.1016/S0254-0584(01)00460-6 ↗
31. 10.1016/j.surfcoat.2007.06.06910.1016/j.surfcoat.2007.06.069 ↗
32. 10.1016/S1350-6307(03)00041-410.1016/S1350-6307(03)00041-4 ↗
33. 10.1179/1743278213Y.000000008210.1179/1743278213Y.0000000082 ↗
34. 10.1016/j.matchar.2009.09.01710.1016/j.matchar.2009.09.017 ↗
35. 10.1016/j.corsci.2010.07.01610.1016/j.corsci.2010.07.016 ↗
36. 10.2478/amm-2014-016210.2478/amm-2014-0162 ↗
37. 10.1016/j.matdes.2009.10.00510.1016/j.matdes.2009.10.005 ↗
38. Shoushtari MRT. · Int J ISSI · 2010 · 7 · 33
39. 10.1016/S0963-8695(96)00041-210.1016/S0963-8695(96)00041-2 ↗
40. 10.1016/j.matdes.2010.05.05210.1016/j.matdes.2010.05.052 ↗
41. 10.1016/j.surfcoat.2005.11.03410.1016/j.surfcoat.2005.11.034 ↗
42. 10.1016/S0167-577X(02)01298-310.1016/S0167-577X(02)01298-3 ↗
43. 10.1016/j.engfailanal.2008.12.00310.1016/j.engfailanal.2008.12.003 ↗
44. 10.1016/0025-5416(88)90420-X10.1016/0025-5416(88)90420-X ↗
45. 10.1016/j.matdes.2009.11.06910.1016/j.matdes.2009.11.069 ↗
46. 10.1007/s11665-014-1085-610.1007/s11665-014-1085-6 ↗
47. 10.1179/174329406X9836810.1179/174329406X98368 ↗
48. 10.1179/02670840322500754510.1179/026708403225007545 ↗
49. Nice P, Martin J. Application limits for super martensitic and precipitation hardened stainless steel bar-stock materials. In: NACE Corrosion 2005. Houston, TX: NACE International; 2005. (Paper 05091).10.5006/C2005-05091 ↗
50. 10.1016/0257-8972(93)90307-A10.1016/0257-8972(93)90307-A ↗
51. Gaugh RR. · Mater Perform · 1977 · 16 · 24
52. 10.1179/bcj.1995.30.1.7710.1179/bcj.1995.30.1.77 ↗
53. 10.1016/j.matdes.2011.10.04110.1016/j.matdes.2011.10.041 ↗
54. 10.1016/S0151-9107(99)80044-010.1016/S0151-9107(99)80044-0 ↗
55. 10.1016/j.nucengdes.2006.03.01710.1016/j.nucengdes.2006.03.017 ↗
56. 10.1016/j.matchar.2013.05.00210.1016/j.matchar.2013.05.002 ↗
57. 10.1520/E0975-1310.1520/E0975-13 ↗
58. Cassagne T, Bonis M, Duret C, Limitations of 17-4 PH metallurgical, mechanical and corrosion aspects. In: NACE Corrosion 2003. San Diego, CA: NACE International; 2003. (Paper 03102).10.5006/C2003-03102 ↗
59. 10.1520/G0193-12D10.1520/G0193-12D ↗
60. 10.1016/0016-7037(94)90022-110.1016/0016-7037(94)90022-1 ↗
61. Singer M, Brown B, Camacho A, Combined effect of CO 2 , H 2 S and acetic acid on bottom of the line corrosion. In: NACE Corrosion 2007. Nashville, TN: NACE International; 2007. (Paper 07661).10.5006/C2007-07661 ↗
62. Takeno N. · 2005
63. 10.1149/1.212388210.1149/1.2123882 ↗
64. 10.1007/BF0264411810.1007/BF02644118 ↗
65. Crolet JL, Bonis MR. Revisiting hydrogen in steel, part I: theoretical aspects of charging, stress cracking and permeation. In: NACE Corrosion 2001. Houston, TX: NACE International; 2001. (Paper 01067).10.5006/C2001-01067 ↗
66. Crolet JL, Bonis MR. Revisiting hydrogen in steel, part II: experimental verifications. In: NACE Corrosion 2001. NACE International; 2001. (Paper 01072).10.5006/C2001-01072 ↗
67. Dean FWH. A review of hydrogen flux promoters. In: NACE Corrosion 2010. San Antonio, TX: NACE International; 2010 (Paper 10182).10.5006/C2010-10182 ↗
68. 10.2118/6144-PA10.2118/6144-PA ↗
69. 10.5006/0010-9312-28.2.3910.5006/0010-9312-28.2.39 ↗
70. 10.1051/mattech/201600710.1051/mattech/2016007 ↗
71. 10.1051/mattech/201601310.1051/mattech/2016013 ↗
72. 10.1051/mattech/201602010.1051/mattech/2016020 ↗
73. 10.1051/mattech/201602610.1051/mattech/2016026 ↗
74. 10.1016/S0010-938X(00)00003-210.1016/S0010-938X(00)00003-2 ↗
75. 10.1149/1.212980810.1149/1.2129808 ↗
76. NACE TM-0177. Laboratory testing of metals for resistance to sulfide stress cracking and stress corrosion cracking in H 2 S environments. NACE International 1, Item 21212; 2005.
77. NACE TM-0198. Slow strain rate test method for screening Corrosion-Resistant Alloys (CRAs) for stress corrosion cracking in sour oilfield service. 2016.
78. Nisbet WJ, Hartman RHC, Handel G. Rippled strain rate test for CRA sour service materials selection. In: NACE Corrosion 1997. Houston, TX: NACE International; 1997. (Paper 58).10.5006/C1997-97058 ↗
79. ASTM G49 – 85 (Reapproved 2011) · ASTM B Stand · 2000 · 85 · 6
80. ASTM G39 – 99 (Reapproved 2011) · ASTM Int · 2005 · 99 · 1
81. 10.1520/G0038-01R1310.1520/G0038-01R13 ↗
82. BS EN ISO 7539-2:1995. Corrosion of metals and alloys – stress corrosion testing –part 2: preparation and use of bent-beam specimens. 3, (2003). Technical Committee ISO/TC 156, Corrosion of metals and alloys.
83. ISO 7539-5. Corrosion of metals and alloys – stress corrosion testing – part 5: preparation and use of C-ring specimens. 1989. Technical Committee ISO/TC 156, Corrosion of metals and alloys.
84. ISO 7539-7. Corrosion of metals and alloys – stress corrosion testing – part 7: method for slow strain rate testing. 2005. Technical Committee ISO/TC 156, Corrosion of metals and alloys.
85. Dent P, Fowler C, Bond S, New axially loaded full ring test method for assessment of susceptibility of girth welds and parent pipe to sour service cracking. In: NACE Corrosion 2017. New Orleans, LA: NACE International; 2017. (Paper 8965).10.5006/C2017-08965 ↗
86. OTI 95 635. A test method to determine the susceptibility to cracking of linepipe steels in sour service. 1996. Health and Safety Executive. Available from:
87. 10.1179/bcj.1992.27.4.27110.1179/bcj.1992.27.4.271 ↗
88. Henthorne M. · Corrosion · 2016 · 9312 · 1
89. 10.1520/STP1210-EB10.1520/STP1210-EB ↗
90. 10.1016/S1359-6454(02)00306-310.1016/S1359-6454(02)00306-3 ↗
91. Cíhal V · Chem Biochem Eng Q · 2007 · 21 · 47
92. 10.1023/A:102444621657610.1023/A:1024446216576 ↗
93. 10.5006/1.329030210.5006/1.3290302 ↗
94. ASTM G148 · ASTM Int · 2011 · 1
95. 10.1179/02670830077300264510.1179/026708300773002645 ↗
96. 10.1179/174328405X2921210.1179/174328405X29212 ↗
97. 10.1016/j.talanta.2010.06.04510.1016/j.talanta.2010.06.045 ↗
98. Kumar PG · Trans JWRI · 2013 · 42 · 39
99. 10.1088/1468-6996/14/1/01420110.1088/1468-6996/14/1/014201 ↗
100. Tuttle RN. · Mater Prot · 1970 · 9 · 2