Abstract

The purpose of the research reported here was to establish how plug shape influences the size and porosity of hollow shells produced by Mannesmann piercing of an ingot. Ingots were cast from 6060 aluminium alloy and then pierced with a solid plug, a plug with a cavity or a hollow plug. Computer simulation of these processes was carried out using ProCast and QForm software and showed that a hollow plug should produce hollow shells with minimal porosity. However, the results of the experimental piercing revealed that the hollow plug in fact produced hollow shells with higher porosity than that of shells produced using either of the other two plugs. This appears to be consequence of the hollow plug losing stability.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Metal Forming Simulation Techniques · Aluminum Alloy Microstructure Properties · Metallurgy and Material Forming

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

National University of Science and Technology ‘MISiS’, Leninskiy pr. 4, Moscow 119049, Russia

Quantorform, Limited Liability Company, Vtoroy Yuzhnoportoviy proezd 16, Building 2, Moscow 115088, Russia

References (35)

Show source-provided references
1. Jaouen O. · Proc. 1st Int. Conf. on ‘Ingot Casting, Rolling and Forging’, Aachen, Germany · 2012 · 1
2. De Micheli P. · Proc. Int. Conf. on ‘New development in forging technology’, Stuttgart, Germany · 2015 · 1
3. 10.1007/s11015-014-9873-710.1007/s11015-014-9873-7 ↗
4. 10.1007/s11015-014-9913-310.1007/s11015-014-9913-3 ↗
5. 10.1007/s11015-015-0002-z10.1007/s11015-015-0002-z ↗
6. 10.1016/j.ijheatmasstransfer.2013.08.07910.1016/j.ijheatmasstransfer.2013.08.079 ↗
7. Tkadlečková M. · J. Achiev. Mater. Manuf. Eng. · 2013 · 56 · 29
8. Heidarzadeh M. · Int. J. Sci. Adv. Technol. · 2011 · 1 · 37
9. 10.1007/s11771-008-0475-z10.1007/s11771-008-0475-z ↗
10. 10.1016/j.jcrysgro.2014.07.03910.1016/j.jcrysgro.2014.07.039 ↗
11. 10.1007/s11661-999-0284-510.1007/s11661-999-0284-5 ↗
12. 10.1016/j.matdes.2013.07.07710.1016/j.matdes.2013.07.077 ↗
13. 10.1016/j.cirp.2009.03.09910.1016/j.cirp.2009.03.099 ↗
14. Chiluveru S. ‘Computational modeling of crack initiation in crossroll piercing’, PhD thesis, Massachusetts Institute of Technology, MA, USA, 2007, 1–89.
15. 10.1007/s12289-008-0068-210.1007/s12289-008-0068-2 ↗
16. 10.1002/srin.20100008510.1002/srin.201000085 ↗
17. 10.5228/KSPP.2008.17.1.06810.5228/KSPP.2008.17.1.068 ↗
18. 10.1007/s12289-012-1099-210.1007/s12289-012-1099-2 ↗
19. 10.1007/s11015-013-9683-310.1007/s11015-013-9683-3 ↗
20. 10.1016/j.msea.2012.07.05210.1016/j.msea.2012.07.052 ↗
21. 10.3103/S106782121105007510.3103/S1067821211050075 ↗
22. 10.1016/S1359-4311(01)00093-X10.1016/S1359-4311(01)00093-X ↗
23. Zhao Y. Q. · Appl. Therm. Eng. · 2015 · 47 · 29
24. 10.1016/j.jmatprotec.2006.03.20510.1016/j.jmatprotec.2006.03.205 ↗
25. 10.2478/amm-2013-006010.2478/amm-2013-0060 ↗
26. 10.1007/s10483-009-0509-710.1007/s10483-009-0509-7 ↗
27. 10.4028/www.scientific.net/AMR.97-101.307910.4028/www.scientific.net/AMR.97-101.3079 ↗
28. 10.4028/www.scientific.net/AMR.26-28.6910.4028/www.scientific.net/AMR.26-28.69 ↗
29. 10.1016/j.jmatprotec.2011.01.01710.1016/j.jmatprotec.2011.01.017 ↗
30. 10.1016/j.jmatprotec.2011.01.00110.1016/j.jmatprotec.2011.01.001 ↗
31. 10.1016/j.jmatprotec.2009.09.02210.1016/j.jmatprotec.2009.09.022 ↗
32. 10.1016/S1006-706X(13)60130-210.1016/S1006-706X(13)60130-2 ↗
33. 10.1016/j.jmatprotec.2009.12.01010.1016/j.jmatprotec.2009.12.010 ↗
34. 10.1088/1757-899X/27/1/01206310.1088/1757-899X/27/1/012063 ↗
35. ‘2015 QForm V8 Simulation Suite, QUANTORFORM’, http://www.qform3d.ru.