Abstract

Metal matrix composites are known for their high strength, fatigue resistance, and wear resistance. The coefficient of thermal expansion between the reinforcement and matrix can result in thermal stresses during thermal cycling. In this paper we quantify the evolution of cavitation damage in SiC particle reinforced aluminium alloy matrix composite subjected to thermal cycling by X-ray synchrotron tomography at the advanced photon source at the Argonne National Laboratory. It will be shown that, while surface examination did not show significant damage, X-ray synchrotron tomography enabled us to resolve and quantify the amount and nature of cavitation with increasing thermal cycling. The influence of the microstructure in damage initiation and evolution is discussed.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Aluminum Alloys Composites Properties · Microstructure and mechanical properties · Aluminum Alloy Microstructure Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Materials Science and Engineering, Arizona State University, Tempe, AZ 85287, USA

Advanced Photon Source, Argonne National Laboratory, Argonne, IL, USA

References (28)

Show source-provided references
1. 10.1007/978-1-4614-9548-210.1007/978-1-4614-9548-2 ↗
2. 10.1016/0026-0800(73)90007-410.1016/0026-0800(73)90007-4 ↗
3. 10.1080/1478643730821746210.1080/14786437308217462 ↗
4. 10.1007/BF0119766510.1007/BF01197665 ↗
5. 10.1016/0921-5093(95)09847-X10.1016/0921-5093(95)09847-X ↗
6. 10.1016/S0921-5093(97)00351-110.1016/S0921-5093(97)00351-1 ↗
7. 10.1023/A:100678351231110.1023/A:1006783512311 ↗
8. 10.1007/s11661-011-0718-810.1007/s11661-011-0718-8 ↗
9. 10.1016/j.actamat.2010.07.03910.1016/j.actamat.2010.07.039 ↗
10. 10.1016/j.engfracmech.2011.07.00410.1016/j.engfracmech.2011.07.004 ↗
11. 10.1016/S1359-6454(96)00311-410.1016/S1359-6454(96)00311-4 ↗
12. 10.1146/annurev-matsci-070511-15511110.1146/annurev-matsci-070511-155111 ↗
13. 10.1016/S1359-6454(99)00024-510.1016/S1359-6454(99)00024-5 ↗
14. 10.1016/S1359-6454(01)00104-510.1016/S1359-6454(01)00104-5 ↗
15. 10.1016/j.ijfatigue.2012.06.00910.1016/j.ijfatigue.2012.06.009 ↗
16. 10.1007/s11661-011-0963-x10.1007/s11661-011-0963-x ↗
17. 10.1088/0953-8984/16/33/01210.1088/0953-8984/16/33/012 ↗
18. 10.1002/9781118533383.ch210.1002/9781118533383.ch2 ↗
19. Singh SS · Integr. Mater. Manufac. Innov. · 2014 · 3 · 9
20. Pyzalla A, Camin B, Lehrer B, Wichert M, Koch A, Zimnik K, Boller E and Reimers W: ‘In-situ observation of creep damage in Al-Al2O3 MMCs by synchrotron X-ray tomography’, International Centre for Diffraction Data, 2006, 1097–2102
21. 10.1016/j.msea.2007.05.10810.1016/j.msea.2007.05.108 ↗
22. 10.1007/s11661-998-0325-510.1007/s11661-998-0325-5 ↗
23. 10.1063/1.12522510.1063/1.125225 ↗
24. 10.1016/j.actamat.2012.03.04810.1016/j.actamat.2012.03.048 ↗
25. 10.1016/0956-716X(93)90201-310.1016/0956-716X(93)90201-3 ↗
26. 10.1007/BF0054954710.1007/BF00549547 ↗
27. 10.1016/0956-7151(94)90475-810.1016/0956-7151(94)90475-8 ↗
28. 10.1016/0921-5093(89)90345-610.1016/0921-5093(89)90345-6 ↗