journal article·2018-07

Phase transformations in Fe–Ni–Cr heat-resistant alloys for reformer tube applications

Franck Tancret, Johanne Laigo, Frédéric Christien, René Le Gall, Jader Furtado

Materials Science and Technology· Volume 34· Issue 11
Publisher page

Abstract

Fe–35Ni–25Cr–0.4C alloys with different compositions are aged between 750 and 1150°C up to ∼10,000 h. As-cast microstructure contains interdendritic carbides of type M 7 C 3 (‘Cr 7 C 3 ’) and MC (‘NbC’). At service temperatures, M 7 C 3 transform into M 23 C 6 (‘Cr 23 C 6 ’) within hours. Then, a hardening precipitation of secondary intragranular M 23 C 6 occurs over hundreds of hours, the nose of the ‘temperature-time-hardening’ curve being around 1000°C. G phase forms after long aging; its solvus temperature and formation kinetics depend on silicon content. Z phase is observed after long aging at 950°C or above. G and Z phases form at the expense of MC. Very long aging causes nitridation under air, with first a transformation of M 23 C 6 into chromium-rich M 2 X carbonitrides (X = C,N), then of MC into chromium-rich MX carbonitrides.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Metal and Thin Film Mechanics · Advanced materials and composites · Metal Alloys Wear and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Université de Nantes, Institut des Matériaux de Nantes – Jean Rouxel (IMN), Polytech Nantes, France

Air Liquide, Centre de Recherche Paris-Saclay, Jouy-en-Josas, France

École Nationale Supérieure des Mines, Saint-Etienne, France

References (46)

Show source-provided references
1. Sullivan CP · Met Eng Q · 1967 · 7 · 36
2. 10.1179/mst.1985.1.5.38510.1179/mst.1985.1.5.385 ↗
3. 10.1016/0921-5093(90)90320-310.1016/0921-5093(90)90320-3 ↗
4. 10.1016/1044-5803(92)90045-J10.1016/1044-5803(92)90045-J ↗
5. 10.1016/1044-5803(93)90039-X10.1016/1044-5803(93)90039-X ↗
6. 10.1016/S1044-5803(03)00013-510.1016/S1044-5803(03)00013-5 ↗
7. Muralidharan G · Proc MS&T’04 Conf · 2004 · 1 · 651
8. 10.1016/j.msea.2008.04.09810.1016/j.msea.2008.04.098 ↗
9. 10.1016/j.matdes.2010.08.03110.1016/j.matdes.2010.08.031 ↗
10. 10.1016/j.msea.2015.01.04910.1016/j.msea.2015.01.049 ↗
11. Laigo J, Tancret F, Le Gall R, Christien F, Furtado J. The influence of phase transformations on creep resistance in Fe-Ni-Cr alloys for reformer tube applications. In: 2007 Proceedings of the ASME Pressure Vessel & Piping Conference/CREEP8 Conference, ISBN 0791838048, paper number CREEP2007-26720.10.1115/CREEP2007-26720 ↗
12. 10.1520/STP28447S10.1520/STP28447S ↗
13. 10.1016/1044-5803(93)90071-310.1016/1044-5803(93)90071-3 ↗
14. 10.1016/j.msea.2004.03.03810.1016/j.msea.2004.03.038 ↗
15. 10.1016/j.matchar.2008.02.00110.1016/j.matchar.2008.02.001 ↗
16. 10.1007/s11661-011-1025-010.1007/s11661-011-1025-0 ↗
17. 10.1007/s11661-014-2285-210.1007/s11661-014-2285-2 ↗
18. 10.1016/j.engfailanal.2007.06.00910.1016/j.engfailanal.2007.06.009 ↗
19. 10.1007/s12666-015-0552-610.1007/s12666-015-0552-6 ↗
20. 10.1515/htmp-2012-001610.1515/htmp-2012-0016 ↗
21. 10.1016/j.actamat.2017.01.04310.1016/j.actamat.2017.01.043 ↗
22. Alvino A, Antonini A, Lega D, Mennuti C, Tonti A. Damage characterization of heat resistant steels after long service in reforming plants. In: ASME 2016 Pressure Vessels and Piping Conference – Volume 6B: Materials and Fabrication, ISBN 978-0-7918-5043-5, paper number PVP2016-63555, pp. V06BT06A032.
23. 10.1016/j.matchar.2009.04.00710.1016/j.matchar.2009.04.007 ↗
24. 10.1016/j.engfailanal.2010.08.01710.1016/j.engfailanal.2010.08.017 ↗
25. 10.1007/s13632-016-0274-010.1007/s13632-016-0274-0 ↗
26. 10.1016/j.actamat.2005.07.03910.1016/j.actamat.2005.07.039 ↗
27. 10.1016/j.actamat.2004.06.00110.1016/j.actamat.2004.06.001 ↗
28. 10.1016/0001-6160(67)90159-910.1016/0001-6160(67)90159-9 ↗
29. 10.1016/S1044-5803(00)00047-410.1016/S1044-5803(00)00047-4 ↗
30. 10.1016/1044-5803(91)90053-710.1016/1044-5803(91)90053-7 ↗
31. Spiegel FX · Trans Metall Soc AIME · 1963 · 227 · 575
32. Goldschmidt HJ. Interstitial alloys, Butterwoths, London, England, 1967, p. 330.10.1007/978-1-4899-5880-8 ↗
33. 10.1007/BF0108648410.1007/BF01086484 ↗
34. 10.1016/0001-6160(88)90105-810.1016/0001-6160(88)90105-8 ↗
35. 10.1016/S1044-5803(01)00166-810.1016/S1044-5803(01)00166-8 ↗
36. 10.1016/S1359-6462(03)00238-010.1016/S1359-6462(03)00238-0 ↗
37. 10.1016/0022-3115(81)90403-710.1016/0022-3115(81)90403-7 ↗
38. 10.1016/0022-3115(79)90055-210.1016/0022-3115(79)90055-2 ↗
39. Binder WO. Some notes on the structure and impact resistance of columbium-bearing 18-8 steels after exposure to elevated temperatures. Symposium on the nature, occurrence and effects of sigma-phase, ASTM STP110, 1950, p. 146–164.10.1520/STP46110S ↗
40. 10.1179/mst.1996.12.7.55210.1179/mst.1996.12.7.552 ↗
41. 10.1007/BF0265804910.1007/BF02658049 ↗
42. Robinson PW · 1985 · 71
43. 10.1179/msc.1977.11.4.11710.1179/msc.1977.11.4.117 ↗
44. Andrén HO · Proc Int Conf Stainless Steels · 1984 · 84 · 91
45. Laigo J. Microstructure, transformations de phases et durabilité à haute température des alliages de la série HP [Microstructure, high temperature phase transformations and durability of HP series alloys], PhD thesis, Université de Nantes, France, 2007.
46. 10.1016/S1044-5803(02)00249-810.1016/S1044-5803(02)00249-8 ↗