Abstract

The effect of 0.5 wt-% SiC nanoparticle addition on microstructure and brazeability of Al–9Si–20Cu alloys has been investigated. The brazing is performed using the filler at 550°C for 30 min. Microstructural observations reveal the refinement of Si and CuAl2 in Al–9Si–20Cu–0.5SiC composite. The average size of Si particles decreases from ∼9 to ∼4 μm. It has been shown that SiC nanoparticles improve the filler brazeability; the spreading ratio increases up to 88.4% as compared to 76.67% over Al–9Si–20Cu alloy. The tensile strength and ductility of Al–9Si–20Cu–0.5SiC are also enhanced by 47 and 53% respectively. The melting point shows a depression ∼4°C in Al–9Si–20Cu–0.5SiC and thus can be a potential filler candidate for brazing industries.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Aluminum Alloys Composites Properties · Aluminum Alloy Microstructure Properties · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Materials Science and Engineering, University of Seoul, Seoul, South Korea

References (20)

Show source-provided references
1. Polmear I. J. ‘Light alloys from traditional alloys to nanocrystals’, 4th edn., 2006, Burlington, MA, Butterworth-Heinemann.
2. Yoo H.-C. · J. Weld. Join · 2011 · 29 · 260
3. 10.1016/0361-3658(83)90015-210.1016/0361-3658(83)90015-2 ↗
4. 10.1016/j.matdes.2009.03.02210.1016/j.matdes.2009.03.022 ↗
5. Musfirah A. H. · J. Appl. Sci. Res · 2012 · 8 · 4865
6. 10.1201/b1487710.1201/b14877 ↗
7. 10.1361/10599490277034386310.1361/105994902770343863 ↗
8. 10.1007/BF0112484010.1007/BF01124840 ↗
9. 10.1016/S1003-6326(10)60578-X10.1016/S1003-6326(10)60578-X ↗
10. 10.1023/A:100464592888610.1023/A:1004645928886 ↗
11. Labisz K. · Arch. Mater. Sci. Eng · 2013 · 63 · 36
12. 10.1007/s10853-011-6143-y10.1007/s10853-011-6143-y ↗
13. 10.1016/S0921-5093(04)00936-010.1016/S0921-5093(04)00936-0 ↗
14. 10.1179/1362171814Y.000000026710.1179/1362171814Y.0000000267 ↗
15. 10.4028/www.scientific.net/AMR.750-752.61910.4028/www.scientific.net/AMR.750-752.619 ↗
16. Miyazawa Y. · Mater. Sci. Eng · 2014 · 61 · 1
17. 10.1007/s11661-011-0905-710.1007/s11661-011-0905-7 ↗
18. Japanese Industrial Standards, JIS Z-3197, 2012.
19. 10.1016/j.jallcom.2009.08.05610.1016/j.jallcom.2009.08.056 ↗
20. 10.1007/s11664-007-0366-310.1007/s11664-007-0366-3 ↗