Abstract
This paper investigates the effect of post-deposition heat treatment on porosity, microstructure, and mechanical properties of Ti–6Al–4V produced via an Electron Beam Melting process. Samples were studied in the conditions of as-built and heat treated at 920°C and 1030°C. The as-built samples were characterised by columnar β grains consists of α+β microstructure with Widmanstätten and colony morphologies were found. Heat treatment resulted in increased α lath width. The yield strength and ultimate tensile strength was greater in the as-built condition than wrought material. Porosity re-growth occurred after heat treatment but it did not affect the tensile properties. Greater ductility after heat treatment was attributed to the larger α lath width which increases effective slip length.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Titanium Alloys Microstructure and Properties · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Faculty of Engineering, Environment and Computing, Coventry University, Coventry, UK
Department of Materials Test Engineering, TU Dortmund University, Dortmund, Germany
References (27)
Show source-provided references
1. Lutjering G · 2007
2. 10.1016/j.matchar.2013.07.01210.1016/j.matchar.2013.07.012 ↗
3. 10.1016/j.matchar.2011.12.00810.1016/j.matchar.2011.12.008 ↗
4. 10.1007/s11661-010-0397-x10.1007/s11661-010-0397-x ↗
5. 10.1016/j.msea.2013.02.06410.1016/j.msea.2013.02.064 ↗
6. 10.1016/j.msea.2013.02.06510.1016/j.msea.2013.02.065 ↗
7. 10.1080/09506608.2016.117628910.1080/09506608.2016.1176289 ↗
8. 10.1016/j.matchar.2008.07.00610.1016/j.matchar.2008.07.006 ↗
9. 10.1016/J.JALLCOM.2015.05.17810.1016/J.JALLCOM.2015.05.178 ↗
10. 10.1007/s11661-015-2976-310.1007/s11661-015-2976-3 ↗
11. 10.1016/j.actamat.2015.06.03610.1016/j.actamat.2015.06.036 ↗
12. 10.1016/J.MSEA.2018.12.01610.1016/J.MSEA.2018.12.016 ↗
13. 10.1108/1355254091096026210.1108/13552540910960262 ↗
14. 10.1016/j.jmatprotec.2011.03.01310.1016/j.jmatprotec.2011.03.013 ↗
15. 10.1016/j.proeng.2015.08.00710.1016/j.proeng.2015.08.007 ↗
16. 10.1016/j.msea.2015.11.05210.1016/j.msea.2015.11.052 ↗
17. 10.1179/1432891713Z.00000000030210.1179/1432891713Z.000000000302 ↗
18. Gong H, Gu H, Zeng K, Melt pool characterization for selective laser melting of Ti-6Al-4 V pre-alloyed powder. 25th Annu. Int. Solid Free. Fabr. Symp., 2014, p. 256–67.
19. 10.1016/j.addma.2014.08.00210.1016/j.addma.2014.08.002 ↗
20. 10.1016/j.scriptamat.2016.05.00210.1016/j.scriptamat.2016.05.002 ↗
21. 10.1080/1478643070137367210.1080/14786430701373672 ↗
22. 10.1179/mtlr.1965.10.1.27110.1179/mtlr.1965.10.1.271 ↗
23. 10.1007/s11661-015-2965-610.1007/s11661-015-2965-6 ↗
24. 10.1016/j.ijfatigue.2016.04.02210.1016/j.ijfatigue.2016.04.022 ↗
25. 10.1016/j.ijfatigue.2016.05.00110.1016/j.ijfatigue.2016.05.001 ↗
26. 10.1080/1478643620820185710.1080/14786436208201857 ↗
27. 10.1016/S0921-5093(96)10446-910.1016/S0921-5093(96)10446-9 ↗