Abstract

The study tests the validity of the tensile hot ductility test for assessing cracking during the straightening operation. Steels with a thin film of deformation induced ferrite (DIF) or fully austenitic when straightening were examined. In both cases dynamic recrystallisation (DRX) occurs at high temperatures. However, DRX is not possible on straightening, the grain size being too coarse and strains too low. When, DRX occurs, ductility is overestimated compared to the un-recrystallised condition on bending. For steels with DIF films if the depth of the trough is ≥40%RA (reduction of area) cracking is unlikely. However, for TWIP steels, the estimated RA for unrecrystallised ϒ can be much < 40% causing cracking even though measured ductility is well in excess.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Microstructure and Mechanical Properties of Steels · Magnetic Properties and Applications · Metallurgy and Material Forming

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Mechanical Engineering and Aeronautics, City, University of London, London, UK

References (28)

Show source-provided references
1. 10.1179/imr.1991.36.1.18710.1179/imr.1991.36.1.187 ↗
2. 10.2355/isijinternational.39.83310.2355/isijinternational.39.833 ↗
3. 10.1179/095066009X1257253017062410.1179/095066009X12572530170624 ↗
4. Hernandez V, Mostaghel S, Ge S Innovative and economical approach for the production of mid-and high-manganese steel. AIS Tech. Conference Proceedings, Pittsburgh. PA, May 2016. AISTech.Pr. Published – PR- 370-090.9013.
5. Mintz B · Mater Sci Technol · 2005 · 21 · 110.1179/mst.2005.21.1.1 ↗
6. 10.1179/174328409X43912310.1179/174328409X439123 ↗
7. 10.1179/mst.1996.12.2.13210.1179/mst.1996.12.2.132 ↗
8. 10.1179/174367507X24735910.1179/174367507X247359 ↗
9. 10.2355/isijinternational.32.24110.2355/isijinternational.32.241 ↗
10. 10.1179/026708309X1252662033827810.1179/026708309X12526620338278 ↗
11. 10.1179/mst.1992.8.2.17110.1179/mst.1992.8.2.171 ↗
12. Banks KM, Tuling AS, Mintz B. (2012). Improved laboratory simulation of transverse cracking during continuous casting in microalloyed steels with varying C contents. 3rd Int Conf Thermomechanical simulation and Processing of steels. Sim Proc 12,12–14 Dec 2012. Steel Authority of India Ltd. Ranchi, India p 393–404.
13. 10.1179/mst.1997.13.3.24310.1179/mst.1997.13.3.243 ↗
14. 10.1016/j.jmrt.2019.10.02810.1016/j.jmrt.2019.10.028 ↗
15. 10.1179/026708309X1250693387338710.1179/026708309X12506933873387 ↗
16. 10.1080/02670836.2020.186173610.1080/02670836.2020.1861736 ↗
17. 10.1179/026708309X1259571230591510.1179/026708309X12595712305915 ↗
18. 10.1016/j.msea.2014.05.07210.1016/j.msea.2014.05.072 ↗
19. 10.1016/j.msea.2012.09.10110.1016/j.msea.2012.09.101 ↗
20. 10.1016/j.msea.2015.09.07910.1016/j.msea.2015.09.079 ↗
21. 10.1016/j.msea.2014.08.03010.1016/j.msea.2014.08.030 ↗
22. 10.1002/srin.20110032010.1002/srin.201100320 ↗
23. Mintz B · Ironmak Steelmak · 1993 · 20 · 445
24. 10.1007/s11661-009-0050-810.1007/s11661-009-0050-8 ↗
25. 10.1115/1.403363210.1115/1.4033632 ↗
26. 10.1016/j.msea.2017.10.00110.1016/j.msea.2017.10.001 ↗
27. 10.1179/1743284713Y.000000039910.1179/1743284713Y.0000000399 ↗
28. 10.3390/met1009123010.3390/met10091230 ↗