Abstract

The effects of Ti 3 AlC 2 content on the physical, mechanical, and arc ablation resistance properties of a fabricated Cu–Ti 3 AlC 2 composite are investigated in detail. Composite samples containing 10, 15, 20, 25, 30, and 35 vol.-% Ti 3 AlC 2 are sintered at 800°C without decomposition of Ti 3 AlC 2 . It is demonstrated that with increasing Ti 3 AlC 2 content, the relative density, electrical conductivity, and flexural strength of Cu–Ti 3 AlC 2 decrease but the Brinell hardness first increases and then decreases. After eroded by an electric arc, Cu–Ti 3 AlC 2 oxidises to CuO, TiO 2 , and Al 2 O 3 . Meanwhile, field emission-SEM observations reveal that the dimensions of protrusions and the percentage of TiO 2 increase with increasing Ti 3 AlC 2 content. Remarkably, the electric arc mainly occurs at the Ti 3 AlC 2 particles, and the Cu matrix remains well protected.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: MXene and MAX Phase Materials · Aluminum Alloys Composites Properties · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

School of Materials Science and Engineering, Hefei University of Technology, Hefei, People's Republic of China

Instrumental Analysis Center, Hefei University of Technology, Hefei, People's Republic of China

Funding

National Natural Science Foundation of China

References (24)

Show source-provided references
1. 10.1016/S0924-0136(00)00639-710.1016/S0924-0136(00)00639-7 ↗
2. 10.1007/s11431-013-5362-710.1007/s11431-013-5362-7 ↗
3. 10.3901/CJME.2013.02.38410.3901/CJME.2013.02.384 ↗
4. 10.1016/S1003-6326(15)63807-910.1016/S1003-6326(15)63807-9 ↗
5. 10.1016/S1002-0721(14)60421-X10.1016/S1002-0721(14)60421-X ↗
6. 10.1016/j.wear.2007.11.01210.1016/j.wear.2007.11.012 ↗
7. 10.1016/S0079-6786(00)00006-610.1016/S0079-6786(00)00006-6 ↗
8. 10.1111/j.1151-2916.2000.tb01281.x10.1111/j.1151-2916.2000.tb01281.x ↗
9. 10.1179/1743280410Y.000000000110.1179/1743280410Y.0000000001 ↗
10. 10.1111/j.1151-2916.1998.tb02413.x10.1111/j.1151-2916.1998.tb02413.x ↗
11. Radovic M · Am Ceram Soc Bull · 2013 · 92 · 20
12. 10.1016/j.tsf.2009.07.18410.1016/j.tsf.2009.07.184 ↗
13. 10.1016/j.ceramint.2011.10.09110.1016/j.ceramint.2011.10.091 ↗
14. 10.1016/S0167-577X(03)00258-110.1016/S0167-577X(03)00258-1 ↗
15. 10.1016/j.matlet.2006.05.06010.1016/j.matlet.2006.05.060 ↗
16. 10.1039/b101520f10.1039/b101520f ↗
17. 10.1016/S0010-938X(02)00177-410.1016/S0010-938X(02)00177-4 ↗
18. 10.1016/j.scriptamat.2015.10.03110.1016/j.scriptamat.2015.10.031 ↗
19. 10.1016/j.ceramint.2016.06.14410.1016/j.ceramint.2016.06.144 ↗
20. 10.1016/j.ceramint.2017.05.01810.1016/j.ceramint.2017.05.018 ↗
21. 10.1016/j.jallcom.2013.03.12210.1016/j.jallcom.2013.03.122 ↗
22. 10.1557/jmr.2008.012610.1557/jmr.2008.0126 ↗
23. 10.1002/jrs.303610.1002/jrs.3036 ↗
24. 10.1557/JMR.1989.124610.1557/JMR.1989.1246 ↗