journal article·2013-10

Influence of B and Ti on hot ductility of high Al and high Al, Nb containing TWIP steels

S. E. Kang, J. R. Banerjee, E. M. Maina, B. Mintz

Materials Science and Technology· Volume 29· Issue 10
Publisher page

Abstract

The addition of ∼0·002B and ∼0·04Ti as microalloying additions to improve the poor hot ductility and high risk of cracking on continuous casting of high Al containing twinning induced plasticity (TWIP) steels has been examined. Tensile specimens were either cast in situ or heated to 1250°C before cooling at 60 K min−1 to test temperatures in the range 700–1100°C and strained to failure at 3×10−3 s−1. For tensile specimens reheated to 1250°C, the presence of B with sufficient Ti to combine with all the N improved ductility over the temperature range of 700–950°C, the reduction in area (RA) values being >40. For the higher strength more complex high Al, TWIP steels having Nb present, there was no improvement in ductility with a similar B and Ti addition, when the average cooling rate after melting to the test temperature was 60 K min−1. Reducing the cooling rate to 12 K min−1 resulted in the RA values being close to the minimum required to avoid transverse cracking throughout the temperature range 800–1000°C. Using these additions of B and Ti, transverse cracking was found not to be a problem when continuously casting these high Al containing TWIP steels.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Microstructure and Mechanical Properties of Steels · Microstructure and mechanical properties · Magnetic Properties and Applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

POSCO, Technical Research Laboratories, Korea

City University London, UK

CB&I UK Ltd, 40 Eastbourne Terrace, London W2 6LG, UK

References (27)

Show source-provided references
1. Kim SK, Cho JW, Kwak WJ, Kim G: ‘Development of TWIP steel for automotive applications’, Proc. 3rd Int. Conf. on ‘New developments in metallurgical process technologies’, Dusseldorf, Germany, June 2007, TEMA Marketing AG, Steel Institute VDEH, 690–697.
2. 10.1179/095066009X1257253017062410.1179/095066009X12572530170624 ↗
3. 10.1002/srin.20070624510.1002/srin.200706245 ↗
4. 10.1179/026708309X1250693387338710.1179/026708309X12506933873387 ↗
5. Tuling A · Mater. Sci. Technol. · 2011 · 27 · 90910.1179/026708309X12595712305915 ↗
6. 10.1007/s11661-002-0133-210.1007/s11661-002-0133-2 ↗
7. 10.1016/S0921-5093(03)00438-610.1016/S0921-5093(03)00438-6 ↗
8. Yamamato K · Tetsu-to-Hagane · 1987 · 73 · 111
9. 10.1016/j.msea.2007.01.09810.1016/j.msea.2007.01.098 ↗
10. Chung IS · J. Korean Inst. Metall. Mater. · 1993 · 31 · 64
11. 10.1016/j.msea.2008.04.02610.1016/j.msea.2008.04.026 ↗
12. Perrot-Simonetta MT · J. Phys. IV · 1995 · 5
13. 10.1179/02670830110151062710.1179/026708301101510627 ↗
14. 10.2355/isijinternational1966.25.14910.2355/isijinternational1966.25.149 ↗
15. Yue S · ISIJ Int. · 2006 · 46 · 91
16. 10.1016/j.msea.2011.02.04010.1016/j.msea.2011.02.040 ↗
17. 10.2355/isijinternational.50.83910.2355/isijinternational.50.839 ↗
18. ‘Precipitation behaviour of complex B compounds in steels’, Nippon Steel technical report no. 21, Nippon Steel, Tokyo, Japan, 1983, 331–337.
19. Abushosha R · Mater. Sci. Technol. · 1991
20. 10.1179/02670839910150678810.1179/026708399101506788 ↗
21. 10.1179/02670839910150678810.1179/026708399101506788 ↗
22. 10.1179/1743284711Y.000000010910.1179/1743284711Y.0000000109 ↗
23. 10.1007/BF0266751810.1007/BF02667518 ↗
24. Yue S, Jonas JJ, Mintz B: ‘Relationship between hot ductility and cracking during continuous casting of steel’, Proc. 13th Process Technology Conference, Nashville, Iron and Steel Society, Nashville, TN, USA, April 1995, pp. 45–52.
25. 10.1016/0001-6160(88)90023-510.1016/0001-6160(88)90023-5 ↗
26. 10.1179/02670830010150769510.1179/026708300101507695 ↗
27. Turkdogan ET · Proc. AIME Steelmaking Conf. · 1987 · 70 · 399