Abstract

Intermetallic titanium aluminides have attracted considerable industrial interest for aero and automotive applications owing to their specific strength. These alloys are candidates for high-temperature applications such as turbine blades and turbocharger turbine wheels. In this work, the mechanical behaviour of an as-cast Ti–47Al–3Cr–3Nb (at.-%) alloy was studied. Four-point bending tests were performed to determine the mechanical properties of the alloy at both room and high temperatures. Microhardness and Young's modulus were evaluated by dynamic indentation tests at room temperature. Analyses of the as-cast alloy showed that, with the selected production process conditions, it has a duplex microstructure. Tests revealed that, while at room temperature the alloy is brittle, between 700 and 900°C it exhibits good ductility and mechanical properties.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Intermetallics and Advanced Alloy Properties · MXene and MAX Phase Materials · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Dipartimento ICMA, Sapienza Università di Roma, Roma, Italy

INSTM Reference laboratory for Engineering of Surface Treatment, Roma, Italy

References (33)

Show source-provided references
1. 10.1016/j.matdes.2013.08.08310.1016/j.matdes.2013.08.083 ↗
2. 10.1016/j.intermet.2013.07.02310.1016/j.intermet.2013.07.023 ↗
3. 10.1016/j.intermet.2012.03.00810.1016/j.intermet.2012.03.008 ↗
4. 10.1016/j.intermet.2014.06.00710.1016/j.intermet.2014.06.007 ↗
5. 10.1016/j.msea.2015.09.07710.1016/j.msea.2015.09.077 ↗
6. 10.1016/j.msea.2014.11.03710.1016/j.msea.2014.11.037 ↗
7. 10.1016/j.matdes.2016.03.07910.1016/j.matdes.2016.03.079 ↗
8. 10.1016/S1003-6326(11)61208-910.1016/S1003-6326(11)61208-9 ↗
9. 10.1016/j.intermet.2016.11.00910.1016/j.intermet.2016.11.009 ↗
10. 10.1016/S0921-5093(01)01152-210.1016/S0921-5093(01)01152-2 ↗
11. 10.1016/j.intermet.2013.09.01010.1016/j.intermet.2013.09.010 ↗
12. 10.1016/j.jallcom.2015.05.16010.1016/j.jallcom.2015.05.160 ↗
13. 10.1016/j.intermet.2014.11.00810.1016/j.intermet.2014.11.008 ↗
14. 10.1016/j.intermet.2014.10.00510.1016/j.intermet.2014.10.005 ↗
15. 10.1016/0966-9795(95)94254-C10.1016/0966-9795(95)94254-C ↗
16. 10.1016/j.intermet.2010.08.02910.1016/j.intermet.2010.08.029 ↗
17. 10.1016/j.intermet.2004.02.04210.1016/j.intermet.2004.02.042 ↗
18. 10.3139/146.01799210.3139/146.017992 ↗
19. 10.1016/j.matdes.2016.06.06410.1016/j.matdes.2016.06.064 ↗
20. 10.1016/j.intermet.2012.07.01210.1016/j.intermet.2012.07.012 ↗
21. 10.1007/s11837-018-2747-x10.1007/s11837-018-2747-x ↗
22. 10.1115/1.403589410.1115/1.4035894 ↗
23. Capata R, Sciubba E, Menna L, Design, prototyping and preliminary testing of A TI-AL gas turbine blade (2015) ASME International Mechanical Engineering Congress and Exposition, Proceedings (IMECE), 6A-2015.10.1115/IMECE2015-50058 ↗
24. Standard Test Method for Flexural Strength of Advanced Ceramics at Ambient Temperature; ASTM C1161-13; ASTM International: West Conshohocken, PA, USA, 2013.
25. Standard Test Method for Flexural Strength of Advanced Ceramics at Elevated Temperatures; ASTM C1211-13; ASTM International: West Conshohocken, PA, USA, 2013.
26. 10.1007/s11666-010-9578-910.1007/s11666-010-9578-9 ↗
27. 10.1016/j.surfcoat.2015.07.07110.1016/j.surfcoat.2015.07.071 ↗
28. 10.1016/j.ceramint.2014.03.11010.1016/j.ceramint.2014.03.110 ↗
29. Instrumented Indentation Test for Hardness and Materials Parameters; ISO 14577; International Organization for Standardization: Genève, Switzerland, 2007.
30. 10.1557/jmr.2004.19.1.310.1557/jmr.2004.19.1.3 ↗
31. 10.1557/JMR.1992.156410.1557/JMR.1992.1564 ↗
32. 10.1002/crat.20090038510.1002/crat.200900385 ↗
33. 10.1016/j.msea.2014.05.03910.1016/j.msea.2014.05.039 ↗