The present work shows a comparative study regarding the mechanical properties of 25 as cast ferritic ductile iron alloys, nine of them with silicon contents higher than 3·00 and carbon contents lower than 3·60. In a first step, different carbon equivalent values have been used in order to analyse the effect of this parameter on the mechanical properties. After this comparative analysis, the composition ranges C = 3·30–3·40 wt- and Si = 3·75–3·80 wt- have been selected as the most proper ones to optimise the tensile and impact properties among the high silicon ductile iron alloys. Finally, a second study was carried out to compare the tensile and fatigue properties of the optimised high silicon alloy with the corresponding ones obtained from an EN GJS 400-18-LT grade alloy with low silicon content. Although the room temperature impact values obtained from the high silicon ductile iron are lower than 6 J cm−2, the measured fatigue limit of this alloy (358 MPa) is clearly higher than the one obtained from the low silicon cast iron (170 MPa). A discussion about the benefits and advantages of the high silicon alloy is included.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Metal Alloys Wear and Properties · Microstructure and Mechanical Properties of Steels · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Área de Ingeniería, I+D y Procesos Metalúrgicos, IK4-Azterlan, Aliendalde Auzunea 6, E- 48200 Durango (Bizkaia), Spain

CIRIMAT, Université de Toulouse, BP 44362, F-31030 Toulouse, France

References (16)

Show source-provided references
1. 10.4028/www.scientific.net/KEM.457.36110.4028/www.scientific.net/KEM.457.361 ↗
2. 10.1179/1743284711Y.000000001410.1179/1743284711Y.0000000014 ↗
3. 10.1179/1743284711Y.000000010010.1179/1743284711Y.0000000100 ↗
4. Hayrynen KL · AFS Trans. · 2002 · 110
5. 10.1007/s11661-001-0261-010.1007/s11661-001-0261-0 ↗
6. 10.1179/174328407X23654410.1179/174328407X236544 ↗
7. 10.1179/174328408X36578410.1179/174328408X365784 ↗
8. Stets W, Löblich H, Gassner G and Schumacher P: Proc. Keith Millis Symp. on ‘Ductile cast iron’, Nashville, TN, USA, October 2013, AFS.
9. Björkegren LE · AFS Trans. · 1996 · 104 · 139
10. Björkegren LE and Hamberg K: ‘Silicon alloyed ductile iron with excellent ductility and machinability’, Proc. Keith Millis Symp. on ‘Ductile cast iron’, Hilton Head Island, SC, USA, October 2003, AFS.
11. Ryntz EF · AFS Trans. · 1976 · 82 · 551
12. ‘Reference microstructure for measurement of pearlite and ferrite content in ductile iron microstructures’, AFS current information report, Quality Control Committee 12-E, Ductile Iron Division, AFS, Schaumburg, IL, USA, 1984.
13. ASM International: ‘ASM specialty handbook: cast irons’, 60–64; 1996, Materials Park, OH, ASM International.
14. 10.4028/www.scientific.net/MSF.636-637.52310.4028/www.scientific.net/MSF.636-637.523 ↗
15. ASM International: ‘ASM specialty handbook: cast irons’, 67–70; 1996, Materials Park, OH, ASM International.
16. Gilbert GNJ · BCIRA J. · 1960 · 8 · 401