Morphology of β-AIFeSi intermetallic in AI-7Si alloy castings
Source abstract
Abstract
The morphology of β-AlFeSi phase was investigated in permanent mould castings of an Al-7Si (wt-%) base alloy at the three iron levels of 0.3, 0.6, and 1.0 wt-% and at two mould temperatures of 25 and 400°C. At high cooling rates and low iron levels, the β platelets were found to be at the interface between flake silicon and aluminium. Increasing the iron level and decreasing the cooling rate encouraged the β platelets to crystallise independently of silicon. The pre-eutectic β platelets which form at high iron levels were efficient nucleants for the eutectic silicon in unmodified and strontium modified alloys. The size of the β platelets increased with increase in iron level and with decrease in cooling rate. It is postulated that the silicon content of the alloy will also influence the size of β platelets at high iron levels; the platelet size in this case will increase with increase in silicon content.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties · Intermetallics and Advanced Alloy Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (12)
Show source-provided references
1. 10.1016/B978-0-408-70932-3.50235-710.1016/B978-0-408-70932-3.50235-7 ↗
2. 10.1007/BF0264444110.1007/BF02644441 ↗
3. COUTRE A. · Am. Foundrymen's Soc. Cast Met. J · 1981 · 6 · 9
4. 10.1016/1044-5803(94)90072-810.1016/1044-5803(94)90072-8 ↗
5. MASACRE C. · Fonderie · 1955 · 108
6. 10.1007/BF0266854010.1007/BF02668540 ↗
7. 10.1179/mst.1986.2.10.100910.1179/mst.1986.2.10.1009 ↗
8. YANEVA S. · Z. Metallkd · 1984 · 75 · 395
9. 10.1007/BF0264976010.1007/BF02649760 ↗
10. 10.1016/0079-6425(70)90001-010.1016/0079-6425(70)90001-0 ↗
11. K. F. KOBAYASHI, P. H. SHINGU, and R. OZAKI: in ‘Solidification and casting of metals’, 101–105; 1979, London, The Metals Society.
12. R. ELLIOTT: ‘Eutectic solidification processing’, 177–180; 1983, London, Butterworth.10.1016/B978-0-408-10714-3.50007-1 ↗