Material needs for turbine sealing at high temperature
Source abstract
Abstract
There is considerable interest in reducing the volume of gas escaping around the blade tips in a gas turbine by fixing an abrasive, such as c-BN, onto the blade tip with an alloy, such as MCrAlY. Abrasion testing at 1100°C showed that the MCrAlY deformed and the abrasive particles oxidised. The shear stress in the MCrAlY was estimated by finite element methods to be in the range of 5–30 MPa, while measurements of the frictional heating suggest the local temperature is between 1100 and 1200°C. Creep testing showed that conventional MCrAlYs were too weak under these conditions. However, higher strengths were obtained using a continuous reinforcing phase together with NiAl. An Al2O3/ZrO2 abrasive was investigated as a more oxidation resistant abrasive. In this case, reaction with the MCrAlY caused Ni to diffuse into the abrasive forming layers of NiO, weakening the particles and causing premature failure.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Advanced materials and composites · High Temperature Alloys and Creep
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Gordon Laboratory Department of Materials Science and Metallurgy, University of Cambridge CB3 0FS, UK
Corporate Surface Engineering Group Elton Rd, Rolls-Royce plc, Derby DE24 8BJ, UK
References (40)
Show source-provided references
1. 10.1115/GT2008-5019610.1115/GT2008-50196 ↗
2. 10.2514/1.925510.2514/1.9255 ↗
3. 10.1111/j.1749-6632.2001.tb05843.x10.1111/j.1749-6632.2001.tb05843.x ↗
4. 10.2514/1.1777810.2514/1.17778 ↗
5. 10.1116/1.57282510.1116/1.572825 ↗
6. 10.1023/A:100478021873210.1023/A:1004780218732 ↗
7. Schmid RK: ‘New high temperature abradables for gas turbines’, PhD thesis, Swiss Federal Institute of Technology Zurich, Zurich, Switzerland, 1997.
8. Alpert CP · J. Am. Ceram. Soc. · 1988 · 7110.1111/j.1151-2916.1988.tb06394.x ↗
9. 10.1111/j.1151-2916.1991.tb04049.x10.1111/j.1151-2916.1991.tb04049.x ↗
10. Sporer D, Wilson S, Giovannetti I, Refke A and Giannozzi M: ‘On the potential of metal and ceramic based abradables in turbine seal applications’, Ed. Joanne Burnett, Proc. 36th Turbomachinery Symp., Houston, TX, USA, September 2007, Turbomachinery Laboratory, Texas A&M University, 79–86.
11. 10.1016/j.surfcoat.2006.07.26110.1016/j.surfcoat.2006.07.261 ↗
12. Jaeger JC · J. Proc. Roy. Soc. N.S.W. · 1942 · 76 · 202
13. 10.1016/0001-6160(87)90209-410.1016/0001-6160(87)90209-4 ↗
14. 10.1016/S0043-1648(96)07490-X10.1016/S0043-1648(96)07490-X ↗
15. 10.1088/0022-3727/8/13/00510.1088/0022-3727/8/13/005 ↗
16. 10.1016/S0925-9635(96)00631-010.1016/S0925-9635(96)00631-0 ↗
17. 10.1016/j.actamat.2009.10.02810.1016/j.actamat.2009.10.028 ↗
18. 10.1243/03093247JSA47810.1243/03093247JSA478 ↗
19. 10.1016/j.actamat.2011.08.02210.1016/j.actamat.2011.08.022 ↗
20. 10.1016/S0966-9795(97)00031-910.1016/S0966-9795(97)00031-9 ↗
21. 10.1016/0257-8972(87)90003-X10.1016/0257-8972(87)90003-X ↗
22. Special Metals Corporation. ‘Properties of Inconel 718’, 2007. http://www.specialmetals.com/documents/Inconel%20alloy%20718.pdf (accessed 11 September 2013).
23. 10.1016/0022-3697(73)90092-910.1016/0022-3697(73)90092-9 ↗
24. 10.1016/j.surfcoat.2006.02.01010.1016/j.surfcoat.2006.02.010 ↗
25. 10.1016/0925-8388(95)01988-X10.1016/0925-8388(95)01988-X ↗
26. 10.1016/0025-5416(86)90341-110.1016/0025-5416(86)90341-1 ↗
27. Thompson JA, Tsui YC, Reed RC, Rickerby DS and Clyne TW: ‘Creep of plasma sprayed CoNiCrAlY and NiCrAlY bond coats and its effects on residual stresses during thermal cycling of thermal barrier coating systems’, 1997 Proc. 6th Int. Conf. on ‘Engineering the surface’, London, UK, 2000, IOM Communications, 199–212.10.1201/9780367814069-16 ↗
28. Swanson GA, Linask I, Nissley DM, Norris PP, Meyer TG and Walker KP: ‘Life prediction and constitutive models for engine hot section anisotropic materials program’, Report no. 174952, National Aeronautics and Space Administration, Washington, DC, USA, 1986.10.2514/6.1985-1421 ↗
29. 10.1016/0921-5093(93)90575-Y10.1016/0921-5093(93)90575-Y ↗
30. 10.1016/S0257-8972(96)02961-110.1016/S0257-8972(96)02961-1 ↗
31. 10.1016/S0257-8972(98)00667-710.1016/S0257-8972(98)00667-7 ↗
32. 10.1179/mst.1992.8.4.36710.1179/mst.1992.8.4.367 ↗
33. Dariola R, Walston WS and Nathal MV: ‘NiAl alloys for turbine airfoils’, Proc. 8th Int. Symp. on ‘Superalloys 1996’, Champion, PA, USA, September 1996, The Minerals, Metals & Materials Society, 561–570.10.7449/1996/Superalloys_1996_561_570 ↗
34. 10.1016/S0966-9795(97)00046-010.1016/S0966-9795(97)00046-0 ↗
35. 10.1016/0010-938X(89)90104-210.1016/0010-938X(89)90104-2 ↗
36. 10.1017/CBO978113917013010.1017/CBO9781139170130 ↗
37. 10.1016/0966-9795(96)00023-410.1016/0966-9795(96)00023-4 ↗
38. Tamarin Y: ‘Protective coatings for turbine blades’, 244; 2002, Materials Park, OH, ASM International.
39. 10.1111/j.1151-2916.1993.tb07750.x10.1111/j.1151-2916.1993.tb07750.x ↗
40. Bowden FP and Tabor D: ‘The friction and lubrication of solids’; 1950, Oxford, Clarendon Press.