Abstract

Crack initiation and propagation is a common concern for molecular composites such as plastic bonded explosives (PBXs) and pharmaceutical tablets. Under compressive stresses, cracks form at contacts between crystals and propagate along crystal-binder interfaces, causing composite failure. To investigate this process, crystal-binder interfaces have been characterised and their mechanical properties tested. Here, samples were created with interfaces representative of those in PBXs and characterised with surface energy measurements and neutron reflectometry (NR). Nanoindentation was performed to simulate the deformation and cracking that occurs at crystal–crystal contacts through the binder. NR revealed that use of a plasticiser disrupts typical crystal–binder intermixing and results in a mechanically weaker interface. During nanoindentation, a plasticised binder was observed by atomic force microscopy to delaminate around indentation impressions, whereas a non-plasticised binder did not. Differences in interfacial adhesion and incompatible strain, dictated by the elastic–plastic film compliances, were used to explain the contrasting delamination behaviours.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Energetic Materials and Combustion · Metal and Thin Film Mechanics · Force Microscopy Techniques and Applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Shock and Detonation Physics Los Alamos National Laboratory, Los Alamos, NM 87545, USA

Lujan Neutron Scattering Center Los Alamos National Laboratory, Los Alamos, NM 87545, USA

School of Chemistry University of Edinburgh, Edinburgh EH9 3JJ, UK

References (38)

Show source-provided references
1. Rae P. J. · Philos. Trans. R. Soc. Lond. A · 2002 · 458 · 743
2. 10.1063/1.226347110.1063/1.2263471 ↗
3. Palmer S. J. P. · Proc. R. Soc. Lond. A · 1993 · 440 · 39910.1098/rspa.1993.0023 ↗
4. 10.1016/0010-2180(94)00171-N10.1016/0010-2180(94)00171-N ↗
5. 10.1016/S0082-0784(00)80297-010.1016/S0082-0784(00)80297-0 ↗
6. 10.1016/S0040-6031(01)00802-410.1016/S0040-6031(01)00802-4 ↗
7. Davis W. C., and Hill L. G. ‘Joints, cracks, holes, and gaps in detonating explosives’, Proc. 12th Int. Detonation Symp., San Diego, CA, USA, August 2002, Office of Naval Research. 220–229.
8. Bowden F. P., and Yoffe A. D. ‘Initiation and growth of explosion in liquids and solids’, 104; 1952, Cambridge, Cambridge University Press.10.1119/1.1933188 ↗
9. 10.1179/174328406X9112210.1179/174328406X91122 ↗
10. 10.1016/j.jmps.2005.12.00110.1016/j.jmps.2005.12.001 ↗
11. 10.1107/S0365110X6300165110.1107/S0365110X63001651 ↗
12. 10.1107/S056774087000394110.1107/S0567740870003941 ↗
13. Skidmore C. B., Phillips D. S., Howe P. M., Mang J. T., and Romero J. A. ‘The evolution of microstructural changes in pressed HMX explosives’, Proc. 11th Int. Detonation Symp., Snowmass Village, CO, USA, August–September 1998, Office of Naval Research, 556–564.10.2172/334323 ↗
14. 10.1557/jmr.2004.19.1.310.1557/jmr.2004.19.1.3 ↗
15. 10.1016/S1359-835X(01)00134-810.1016/S1359-835X(01)00134-8 ↗
16. 10.1016/j.actamat.2005.02.01310.1016/j.actamat.2005.02.013 ↗
17. 10.1016/S1359-6454(97)00180-810.1016/S1359-6454(97)00180-8 ↗
18. 10.1115/1.400023010.1115/1.4000230 ↗
19. 10.1080/1478643090312033510.1080/14786430903120335 ↗
20. 10.1016/j.polymer.2011.06.03110.1016/j.polymer.2011.06.031 ↗
21. 10.1063/1.220341110.1063/1.2203411 ↗
22. 10.1021/ma800015g10.1021/ma800015g ↗
23. 10.1016/j.jcis.2010.08.06310.1016/j.jcis.2010.08.063 ↗
24. 10.1002/app.1969.07013081510.1002/app.1969.070130815 ↗
25. Yee R. Y., Adicoff A., and Dibble E. J. ‘Surface properties of HMX crystal’, 1981-0125cc, Naval Weapons Center, China Lake, CA, USA, 1981.
26. 10.1016/S1389-0352(00)00011-810.1016/S1389-0352(00)00011-8 ↗
27. 10.1002/polb.2017110.1002/polb.20171 ↗
28. NIST: ‘Scattering length density calculator’, http://www.ncnr.nist.gov/resources/sldcalc.html (accessed 19 September 2011).
29. Singh B. · Defence Sci. J. · 1978 · 28 · 41
30. 10.1063/1.178249110.1063/1.1782491 ↗
31. 10.1063/1.149539910.1063/1.1495399 ↗
32. Vandersall K. S., Tarver C. M., Garcia F., Chidester S. K., Urtiew P. A., and Forbes J. W. ‘Low amplitude single and multiple schock initiation experiments and modeling of LX-04’, Proc. 13th Int. Detonation Symp., Norfolk, VA, USA, July 2006, Office of Naval Research, 904–913.
33. Vandersall K. S., Tarver C. M., Garcia F., Urtiew P. A., and Chidester S. K. ‘Shock initiation experiments on the HMX based explosive LX-10 with associated ignition and growth modeling’, Proc. APS Topical Conf. on ‘Shock compression of condensed matter’, Waikoloa, HI, American Institute of Physics. USA, June–July 2007, 1010–1013.10.1063/1.2832886 ↗
34. Gustavsen R. L., Sheffield S. A., Alcon R. R., and Hill L. G. ‘Shock initiation of new and aged PBX 9501’, Proc. 12th Int. Detonation Symp., San Diego, CA, USA, August 2002, Office of Naval Research, 530–537.
35. 10.1002/prep.20040005810.1002/prep.200400058 ↗
36. 10.1016/j.ijpharm.2008.02.01310.1016/j.ijpharm.2008.02.013 ↗
37. 10.1016/j.addr.2003.10.00710.1016/j.addr.2003.10.007 ↗
38. 10.1016/j.ces.2010.01.03710.1016/j.ces.2010.01.037 ↗