Through-thickness microstructure and mechanical properties in stationary shoulder friction stir processed AA7075
Source abstract
Abstract
Stationary shoulder friction stir processing of high strength thick AA7075 aluminium alloy demonstrated tiny gradient in the microstructure refinement across the thickness, which was attributed to the less heat input and small temperature gradient by the stationary shoulder. Stationary shoulder produced a very smooth surface finish with a little amount of flash throughout the processing area. Probe-dominated stir zone (SZ) resulted in uniform grain refinement as well as hardness distribution across the SZ thickness. The ductility in SZ increased by 48% in comparison to the unprocessed material without costing tensile strength. This tensile behaviour trend maintained throughout the thickness in SZ. GRAPHICAL ABSTRACT
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Advanced Welding Techniques Analysis · Aluminum Alloys Composites Properties · Aluminum Alloy Microstructure Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
State Key Laboratory of Solidification Processing, Shaanxi Key Laboratory of Friction Welding Technologies, School of Materials Science and Engineering, Northwestern Polytechnical University, Xi'an, Shaanxi, People's Republic of China
Mechanical Engineering Department, School of Technology, Pandit Deendayal Petroleum University, Gandhinagar, Gujarat, India
Funding
National Key Research and Development Program of China
References (30)
Show source-provided references
1. 10.1016/j.mser.2005.07.00110.1016/j.mser.2005.07.001 ↗
2. 10.1080/10408436.2017.135814510.1080/10408436.2017.1358145 ↗
3. 10.1080/02670836.2017.130042010.1080/02670836.2017.1300420 ↗
4. 10.1080/10408436.2018.149025110.1080/10408436.2018.1490251 ↗
5. 10.1080/02670836.2016.127625110.1080/02670836.2016.1276251 ↗
6. 10.1080/02670836.2017.136670910.1080/02670836.2017.1366709 ↗
7. 10.1080/02670836.2018.148162510.1080/02670836.2018.1481625 ↗
8. 10.1007/s40195-019-00905-310.1007/s40195-019-00905-3 ↗
9. 10.1007/s11665-017-2572-310.1007/s11665-017-2572-3 ↗
10. 10.1016/j.msea.2017.09.02810.1016/j.msea.2017.09.028 ↗
11. 10.1080/10426914.2015.110386810.1080/10426914.2015.1103868 ↗
12. 10.1016/j.msea.2016.10.11310.1016/j.msea.2016.10.113 ↗
13. 10.1016/j.mser.2005.07.00110.1016/j.mser.2005.07.001 ↗
14. 10.1016/j.msea.2017.12.01810.1016/j.msea.2017.12.018 ↗
15. 10.1016/j.jmatprotec.2015.03.03610.1016/j.jmatprotec.2015.03.036 ↗
16. 10.1016/j.jmatprotec.2018.08.02210.1016/j.jmatprotec.2018.08.022 ↗
17. 10.1016/j.msea.2017.12.01910.1016/j.msea.2017.12.019 ↗
18. 10.1016/j.jmapro.2018.11.01410.1016/j.jmapro.2018.11.014 ↗
19. 10.1080/10426914.2018.154471610.1080/10426914.2018.1544716 ↗
20. 10.1007/s00170-016-8924-610.1007/s00170-016-8924-6 ↗
21. 10.1080/10426914.2018.154471610.1080/10426914.2018.1544716 ↗
22. 10.1080/02670836.2019.157069210.1080/02670836.2019.1570692 ↗
23. 10.1016/S1359-6462(99)00329-210.1016/S1359-6462(99)00329-2 ↗
24. 10.1016/S1359-6454(02)00278-110.1016/S1359-6454(02)00278-1 ↗
25. 10.1016/j.msea.2007.01.14110.1016/j.msea.2007.01.141 ↗
26. 10.1016/j.msea.2008.11.01610.1016/j.msea.2008.11.016 ↗
27. 10.1016/j.scriptamat.2010.11.05010.1016/j.scriptamat.2010.11.050 ↗
28. Burgueño A, Dieguez T, Svoboda H. Effect of processing parameters on superplastic and corrosion behavior of aluminum alloy friction stir processed. Materials Science Forum; 2012 August 1–5, 2011; Quebec City, Canada: Trans Tech Publ.
29. 10.1016/j.matlet.2015.07.07410.1016/j.matlet.2015.07.074 ↗
30. 10.1016/S0921-5093(03)00532-X10.1016/S0921-5093(03)00532-X ↗