journal article·2007-11

Hot cracking in tungsten inert gas welding of magnesium alloy AZ91D

W. Zhou, T. Z. Long, C. K. Mark

Materials Science and Technology· Volume 23· Issue 11
Publisher page

Abstract

Plates of 3–5 mm in thickness were extracted from an AZ91D ingot and then butt joints of the plates were produced using tungsten inert gas (TIG) welding method. The TIG arc was also used to deposit welding beads on some of the thin plates. No cracking was found in the butt joints. However, hot cracking was always observed to propagate from the heat affected zone (HAZ) under the welding bead into the weld metal right after a welding bead was deposited on the thin plate. Metallographic and fractographic evidence was obtained to show that the hot cracking is ‘liquation cracking’ in the partially melted HAZ under the high thermal stresses. In the butt joints, the weld metal has the finest grains, highest strength and best ductility, and the HAZ was found to be the ‘weakest link’.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Magnesium Alloys: Properties and Applications · Advanced Welding Techniques Analysis · Aluminum Alloy Microstructure Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (26)

Show source-provided references
1. Ruden T. J. · Adv. Mater. Process · 1994 · 145 · 28
2. VanFleteren R. · Adv. Mater. Process · 1996 · 149 · 33
3. 10.1080/10667857.2003.1175300810.1080/10667857.2003.11753008 ↗
4. 10.1080/1042691000891297510.1080/10426910008912975 ↗
5. 10.1023/A:102269891681710.1023/A:1022698916817 ↗
6. 10.1016/S0010-938X(99)00143-210.1016/S0010-938X(99)00143-2 ↗
7. 10.1023/A:100401191660910.1023/A:1004011916609 ↗
8. Wu G. H., Fan Y., Gao H. T., Zhai C. Q., and Zhu Y. P.: Mater. Set Eng. A, 2005, A408,255–263.10.1016/j.msea.2005.08.011 ↗
9. 10.1023/A:101091901780510.1023/A:1010919017805 ↗
10. Weisheit A., Galun R., and Mordike B. L.: Weld J., 1998,77, (4), 149s-154s.
11. 10.1002/(SICI)1521-4052(199911)30:11<682::AID-MAWE682>3.0.CO;2-910.1002/(SICI)1521-4052(199911)30:11<682::AID-MAWE682>3.0.CO;2-9 ↗
12. American Welding Society: ‘Welding handbook’, 7th edn,Vol. 4, 396; 1989, Miami, FL, AWS.
13. 10.1023/A:100664000891410.1023/A:1006640008914 ↗
14. Munitz A., Cotler C., Stern A., and Kohn G.: Mater. ScL Eng. A, 2001, A302, (1),68–73.10.1016/S0921-5093(00)01356-3 ↗
15. Liu L. M., Zhang Z. D., Shen Y., and Wang L.: Acta MetalL Sin. 2006, 42, 399–404.
16. 10.2320/matertrans.47.44610.2320/matertrans.47.446 ↗
17. 10.1016/j.jmatprotec.2005.06.06810.1016/j.jmatprotec.2005.06.068 ↗
18. Chi C. T., Chao C. G., Huang C. A., and Lee C. H.: Mater. Sci. Forum, 2006, 505-507,193–198.10.4028/www.scientific.net/MSF.505-507.193 ↗
19. Zhu T. P., Chen Z. W., and Gao W.: Mater. Set Eng. A, 2006, A416,246–252.10.1016/j.msea.2005.10.032 ↗
20. Feng J. C., Wang Y. R., and Zhang Z. D.: ScL Technot Weld Join. 2006, 11, 154–162.10.1179/174329306X84364 ↗
21. Munitz A., Cotler C., Shaham H., and Kohn G.: Weld J., 2000,79, (7), 202s-208s.
22. Nayeb-Hashemi A. A., and Clark J. B. ‘Phase diagrams of binary magnesium alloys’, 18; 1988, Metals Park, OH, ASM International.
23. Borland J. C. · Brit. Weld J · 1961 · 8 · 526
24. Prokhorov N. N.: Weld Product. 1962, 9, (4), 1–8.
25. Radhakrishnan B., and Thompson R. G.: MetalL Trans. A, 1992, A23, (6),1783–1799.10.1007/BF02804371 ↗
26. Avedesian M. M. ‘Magnesium and magnesium alloys’, 8–9; 1999, Materials Park, OH, ASM International.