Fracture behaviour of radiolytically oxidised reactor core graphites: A view
Source abstract
Abstract
This paper provides a view on the fracture behaviour of polygranular graphites, used to moderate gas cooled nuclear reactors. Graphite is often cited as a classic example of a brittle material because failure, in tension, is associated with small strains. However, attempts to characterise the fracture behaviour of graphite by linear elastic fracture mechanics methods have been largely unsuccessful. Observations of graphite fracture show that elastic strain energy may be dissipated by the formation of distributed microcracks, and their formation may be responsible for non-linearity in the rising load–displacement curve. Progressive softening behaviour may also be observed in some specimens after the peak load. This type of load–displacement behaviour is a characteristic of quasi-brittle materials. Radiolytic oxidation increases the proportion of porosity within reactor core graphite so that the microstructure becomes increasingly skeletal. Consideration is given to the fracture of radiolytically oxidised graphite to support an argument for quasi-brittle behaviour.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Graphite, nuclear technology, radiation studies · Nuclear and radioactivity studies · Nuclear Materials and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Serco TAS, Faraday Street, Birchwood Park, Warrington, WA3 66A, UK;, Email: Andrew.hodgkins@Sercoassurance.com
Materials Performance Centre, School of Materials, The University of Manchester, Manchester, M13 9PL, UK
Magnox North Ltd, Oldbury Naite, Oldbury-on-Severn, Bristol, BS35 1RQ, UK
Magnox North Ltd, Oldbury Naite, Oldbury-on-Severn, Bristol, BS35 1RQ, UK, Departmet of Physics, HH Wills Laboratory, University of Bristol, Bristol, BS8 1TL, UK
References (38)
Show source-provided references
1. ‘Nuclear graphite production’ · Nuclear Eng · 1957 · 175 · 8
2. Fazluddin S. · 2002
3. 10.1016/0149-1970(85)90002-210.1016/0149-1970(85)90002-2 ↗
4. Mantell C. L. ‘Carbon and graphite handbook’, 9; 1968, New York, John Wiley.
5. Brocklehurst J. · Chem. Phys. Carbon · 1977 · 13 · 145
6. Vatter I. A. ‘Oldbury reactor 2 2005 installed sets — phase 3’, Measurements. Part 3. Flexural tests — fractography. British Nuclear Group/Report MEN/ESTD/OLA/REP/0058/07, British Nuclear Group, 2007.
7. Yaghi A. H., Hyde T. H., Becker A. A., and Walker G. ‘The integrity of graphite blocks in nuclear reactors’, University of Nottingham report, GRA/AHY/040806, August 2004.
8. Kelly B. T. ‘Physics of graphite’; 1981, London, Applied Science.
9. Lynch C., and Neighbour G. B.: in ‘Management of ageing processes in graphite reactor cores’, (ed. Neighbour G. B.), 91; 2007, London, RSC Publishing.10.1039/9781847557742 ↗
10. Lynch C., and Neighbour G. B. ‘Modelling crack growth in complex heterogeneous brittle materials’, First year progress report, University of Hull/Eng/Nuc/R009, 2005.
11. Burton B. ‘Crack propagation and arrest in porous graphite, MEN/ESTD/GEN/REP/0027/07, Issue 2, 2007.
12. 10.1016/0022-3115(82)90145-310.1016/0022-3115(82)90145-3 ↗
13. 10.1016/0008-6223(95)00171-910.1016/0008-6223(95)00171-9 ↗
14. Tsang D. K. L. · 2003
15. 10.1016/S0013-7944(97)00010-610.1016/S0013-7944(97)00010-6 ↗
16. Schlangen E. · Key Eng. Mater · 2008 · 69 · 385
17. Schlangen E. · Key Eng. Mater · 2008 · 73 · 385
18. Mar A.: Addressing NRE issues on graphite as per NRS/GRA/ GNSR/6009, 2006.
19. 10.1016/j.cma.2005.04.02010.1016/j.cma.2005.04.020 ↗
20. Anderson T. L. ‘Fracture mechanics’; 1991, Boston, CRC Press.
21. Karihaloo B. L. ‘Fracture mechanics and structural concrete’; 1995, Harlow, Longmans Scientific and Technical.
22. Irwin G. R. ‘Fracture’, in ‘Handbuch der Physik VI’, 551; 1958, Berlin, Springer-Verlag.10.1007/978-3-642-45887-3_5 ↗
23. Committee ACI: Report 446.1 R91, Detroit, MI, American Concrete Institute, 1991.
24. 10.1016/S0013-7944(99)00139-310.1016/S0013-7944(99)00139-3 ↗
25. 10.1016/0022-5096(60)90013-210.1016/0022-5096(60)90013-2 ↗
26. 10.1016/S0065-2156(08)70121-210.1016/S0065-2156(08)70121-2 ↗
27. 10.1007/s00419005025210.1007/s004190050252 ↗
28. Brown M., Payne J. F. B., Sowerbutts T., Lingham I. J., and Bannister G. ‘Investigation into graphite material variability’, British Nuclear Group Report RS/E&TS/GEN/REP/0026/06, Issue 1, 2006.
29. Ouagne P. · 2001
30. 10.1111/j.1151-2916.1988.tb06377.x10.1111/j.1151-2916.1988.tb06377.x ↗
31. 10.1016/j.engfracmech.2007.11.00310.1016/j.engfracmech.2007.11.003 ↗
32. Li H., Duff J., and Marrow T. J. ‘In-situ observation of crack nucleation in nuclear graphite by digital image correlation’, Proceedings of ASME Conf. PVP2008, PVP2008-61136, Vol 6A8B,813–820.10.1115/PVP2008-61136 ↗
33. Hodgkins A. · 2006
34. 10.1179/174328406X11412610.1179/174328406X114126 ↗
35. Flewitt P. E. J., Moskovic R., and Wootton M. R. ‘A consideration of the effect of radiolytic oxidation on the directionality of fracture strength of PGA graphite’, Magnox Electric North Report MEN/ ESTD/GEN/EAN/0069/07, 2007
36. 10.1179/174328405X6954210.1179/174328405X69542 ↗
37. Heard P. J. · 2008 · Bristol
38. ‘Collins English Dictionary’, 3rd edn; 1991, Glasgow, Harper Collins.