Investigation on interface of Al/Cu couples in compound casting
Source abstract
Abstract
The joining of Al and Cu commercially pure metals using the compound casting process has been investigated where an aluminium melt is cast onto a solid cylindrical copper insert. The microstructure of the interface between copper core and surrounding aluminium was characterised by optical microscopy, scanning electron microscopy, energy dispersive X-ray spectroscopy and Vickers hardness tests. Results showed that five separate reaction layers are formed in the reaction interface of core and surrounding Al. These layers included Cu9Al4, AlCu and Al2Cu intermetallic compounds; a eutectic layer; and a eutectic α-Al dendritic structure layer. Owing to the presence of hard and brittle intermetallic compounds within reaction layers, microhardness profile showed a peak of 300 HV where both parent metals have hardness <50 HV. Microhardness profile also showed that hardness decreases from the copper to the aluminium side.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Aluminum Alloys Composites Properties · Aluminum Alloy Microstructure Properties · Advanced Welding Techniques Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Iran University of Science and Technology, Tehran, Iran
References (30)
Show source-provided references
1. 10.1016/j.matdes.2008.04.07410.1016/j.matdes.2008.04.074 ↗
2. 10.1016/j.intermet.2011.10.01410.1016/j.intermet.2011.10.014 ↗
3. Acarer M · J. Mater. Eng. Perform.
4. 10.1016/j.jallcom.2004.07.05710.1016/j.jallcom.2004.07.057 ↗
5. 10.1109/95.29637210.1109/95.296372 ↗
6. 10.1007/s00170-009-2443-710.1007/s00170-009-2443-7 ↗
7. 10.1016/j.jmatprotec.2005.09.01310.1016/j.jmatprotec.2005.09.013 ↗
8. 10.1016/j.jallcom.2007.06.00910.1016/j.jallcom.2007.06.009 ↗
9. 10.1016/j.jallcom.2009.10.12710.1016/j.jallcom.2009.10.127 ↗
10. 10.1007/BF0111580010.1007/BF01115800 ↗
11. Cheng XL · J. Re. Met. · 2009 · 28 · 478
12. 10.1007/s12540-010-0820-210.1007/s12540-010-0820-2 ↗
13. 10.1016/0022-3697(93)90238-M10.1016/0022-3697(93)90238-M ↗
14. 10.1016/j.compositesb.2011.04.04510.1016/j.compositesb.2011.04.045 ↗
15. 10.1016/j.jmatprotec.2006.04.10710.1016/j.jmatprotec.2006.04.107 ↗
16. Berski S · J. Achiev. Mater. Manuf. Eng. · 2007 · 22 · 73
17. 10.1016/j.actamat.2008.02.04210.1016/j.actamat.2008.02.042 ↗
18. 10.1016/j.intermet.2011.12.00110.1016/j.intermet.2011.12.001 ↗
19. 10.1007/s11431-008-0345-910.1007/s11431-008-0345-9 ↗
20. 10.1016/j.apsusc.2011.01.02410.1016/j.apsusc.2011.01.024 ↗
21. 10.1007/s10853-011-5595-410.1007/s10853-011-5595-4 ↗
22. 10.1016/j.msea.2009.11.06610.1016/j.msea.2009.11.066 ↗
23. 10.1080/13640461.2003.1181961010.1080/13640461.2003.11819610 ↗
24. 10.1016/S1359-835X(02)00158-610.1016/S1359-835X(02)00158-6 ↗
25. 10.1016/j.matdes.2009.01.00810.1016/j.matdes.2009.01.008 ↗
26. ‘ASM metals handbook’, Vol. 2, ‘Casting’; 1992, Metals Park, OH, ASM International.
27. 10.1179/13640460422501754610.1179/136404604225017546 ↗
28. 10.1179/13640460522502300010.1179/136404605225023000 ↗
29. GaskellDR: ‘Introduction to the thermodynamic of materials’, 4th edn; 2003, New York, Taylor and Francis.
30. Fontana MG, Green MD: ‘Corrosion engineering’, 481; 1981, New York, McGraw-Hill.