Hot ductility of TWIP steels
Source abstract
Abstract
The hot ductility of twin induced plasticity (TWIP), 0·6 wt-C steels containing 18–22 wt-Mn with N levels in the range 0·005–0·023 wt- and the Al additions either low (<0·05 wt-) or high (1·5 wt-) has been examined. Little change in ductility occurred in the temperature range 1100–650°C as the structure was always fully austenitic. Ductility was generally poor (<40), reduction of area values, the best ductility at the higher Al level being given by the steel with the lowest N and S levels. Because the steel is fully austenitic, the ductility is solely dependent on that for unrecrystallised austenite. Therefore, to avoid transverse cracking the volume of second phase particles should be kept to a minimum, i.e. the N should be low to reduce the amount of AlN that can be precipitated out and the S level should be as low as possible to limit the amount of MnS inclusions. Metallographic and TEM studies were carried out and the poor ductility was found to be due to extensive precipitation of AlN at the austenite grain boundaries. Increasing the cooling rate from the melting point to the test temperature from 60 to 180°C min−1 or introducing an undercooling step both led to even worse ductility.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Microstructure and Mechanical Properties of Steels · Metal Alloys Wear and Properties · Metallurgical and Alloy Processes
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Senior Research Scientist, POSCO, Korea
University of Pretoria, South Africa
City University London, UK
References (13)
Show source-provided references
1. Kim S.K., Cho J.W., Kwak W.J., and Kim G. ‘Development of TWIP steel for automotive applications’, Proc. 3rd Int. Conf. on ‘New developments in metallurgical process technologies’, Dusseldorf, Germany, June 2007, TEMA Technologie Marketing AG, Steel Institute VDEH, 690–697.
2. 10.2355/isijinternational.43.43810.2355/isijinternational.43.438 ↗
3. 10.1179/imr.1991.36.1.18710.1179/imr.1991.36.1.187 ↗
4. Banks K. M. · 42nd MWSP Conf. Proc., · 2000 · 38 · 329
5. 10.1179/174328105X4801610.1179/174328105X48016 ↗
6. 10.1179/174367507X24735910.1179/174367507X247359 ↗
7. 10.1179/mst.1986.2.7.67110.1179/mst.1986.2.7.671 ↗
8. 10.2355/isijinternational.39.83310.2355/isijinternational.39.833 ↗
9. Leslie W. C. · Trans. ASM · 1954 · 46 · 1470
10. 10.1179/174328407X17973710.1179/174328407X179737 ↗
11. Cardoso G. I. S. L. · Ironmaking Steelmaking · 1995 · 32 · 365
12. 10.1179/mst.1998.14.4.34610.1179/mst.1998.14.4.346 ↗
13. Becker J. J. · AISI Tech. Proc. · 2005 · 99