Abstract

Many attempts were conducted to improve Cu–Cr alloys’ softening temperature, strength, and electrical conductivity. After homogenised treatment at 900°C for 4 h, hot rolled by 80% at 900°C, solid solution treated at 940°C for 2 h, cold rolled by 50%, and aged at 450°C for 1 h, cold rolled by 50%, and aged at 450°C for 0.5 h, the tensile strength, yield strength, microhardness, and electrical conductivity of the fabricated Cu–2Cr–1Zn alloy were 616.7, 540.1 MPa, 176.7 HV, and 71.5% IACS, respectively, with a softening temperature of 530°C. Orowan precipitation strengthening was the primary strengthening mechanism. These findings bring an effective way to improve the strength and softening temperature with a small loss of electrical conductivity.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Aluminum Alloys Composites Properties · Microstructure and mechanical properties · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

State Key Laboratory for Powder Metallurgy, Central South University, Changsha, People's Republic of China

Hunan Aircraft Maintenance Engineering Technology Research Center, Changsha Aeronautical Vocational and Technical College, Changsha, People's Republic of China

School of Materials Science and Engineering, Central South University, Changsha, People's Republic of China

Funding

the Key Technologies R&D Program of Yunnan Province · the National MCF Energy R&D Program of China

References (64)

Show source-provided references
1. 10.1109/20.80065010.1109/20.800650 ↗
2. 10.3390/en1501031710.3390/en15010317 ↗
3. 10.1049/iet-pel.2017.018110.1049/iet-pel.2017.0181 ↗
4. 10.21122/2227-1031-2017-16-1-73-8210.21122/2227-1031-2017-16-1-73-82 ↗
5. 10.1016/j.carbon.2018.03.01810.1016/j.carbon.2018.03.018 ↗
6. 10.1063/1.487465510.1063/1.4874655 ↗
7. 10.1134/S0031918X1409006310.1134/S0031918X14090063 ↗
8. Xiao P, You J, Zou J. In-situ synthesis and the vacuum electrical performances of Cr2Nb/CuCr composite. Rare Met Mater Eng. 2012;41(9):1666–1671.
9. 10.1016/j.msea.2022.14303810.1016/j.msea.2022.143038 ↗
10. 10.1179/174328408X36582910.1179/174328408X365829 ↗
11. 10.1179/02670830422501661710.1179/026708304225016617 ↗
12. 10.1016/j.jallcom.2019.01.17910.1016/j.jallcom.2019.01.179 ↗
13. Feng Y, Zhang CY, Ding BJ. Preparation of nanocrystalline CuCr contact materials and their chopping currents. Rare Met Mater Eng. 2005;34(9):1439–1442.
14. Zhao HL, Meng DL, Hao W. Effect of heat treatment on hardness and impact toughness of CuCr containing RE alloy. J Rare Earths. 2005;23:445–448.
15. 10.1016/j.matchar.2021.11110410.1016/j.matchar.2021.111104 ↗
16. 10.3390/ma1323553210.3390/ma13235532 ↗
17. 10.1016/j.jallcom.2022.16711110.1016/j.jallcom.2022.167111 ↗
18. Xie H, Guan W, Lv H CuCr/Cu contact material fabricated via high-speed laser cladding. Int J Adv Manuf Technol. 2022;124:394–410.
19. 10.1179/026708310X1281599241821010.1179/026708310X12815992418210 ↗
20. 10.1016/j.msea.2011.06.08610.1016/j.msea.2011.06.086 ↗
21. 10.2320/jinstmet.74.35610.2320/jinstmet.74.356 ↗
22. 10.1088/2053-1591/ab825910.1088/2053-1591/ab8259 ↗
23. Fan ZK, Yang HW, Liang SH Effects of extrusion on chromium precipitation in Cu–Cr alloy. Trans Nonferr Metal Soc China. 2003;13(2):267–270.
24. Su JH, Dong QM, Liu P Aging precipitation of lead frame Cu–Cr–Sn–Zn alloy. J Rare Earths. 2003;21:182–184.
25. Yuan J-h, Chen H-m, Xie W-b Work-softening mechanism of Cu–Cr–Ti–Si alloy. Cailiao Gongcheng—J Mater Eng. 2020;48(11):140–146.
26. 10.1016/j.mtcomm.2021.10226610.1016/j.mtcomm.2021.102266 ↗
27. 10.1002/mawe.20170020110.1002/mawe.201700201 ↗
28. 10.1007/s11041-007-0032-710.1007/s11041-007-0032-7 ↗
29. 10.1016/j.matdes.2009.04.01710.1016/j.matdes.2009.04.017 ↗
30. 10.1016/j.msea.2017.05.11410.1016/j.msea.2017.05.114 ↗
31. 10.1016/j.jallcom.2017.11.30910.1016/j.jallcom.2017.11.309 ↗
32. 10.1016/j.msea.2020.14062810.1016/j.msea.2020.140628 ↗
33. 10.1016/j.jallcom.2020.15700410.1016/j.jallcom.2020.157004 ↗
34. Zhang SL, Yin ZM, Song LP Aging characteristics of the alloys Cu–Zn–Cr. Rare Met Mater Eng. 2003;32(2):126–129.
35. 10.1016/S1001-0521(08)60178-310.1016/S1001-0521(08)60178-3 ↗
36. 10.1016/j.actamat.2007.09.02010.1016/j.actamat.2007.09.020 ↗
37. 10.1016/j.engfracmech.2010.06.00610.1016/j.engfracmech.2010.06.006 ↗
38. 10.1016/S0022-3115(99)00285-810.1016/S0022-3115(99)00285-8 ↗
39. 10.1016/j.msea.2018.06.07510.1016/j.msea.2018.06.075 ↗
40. 10.1016/j.scriptamat.2004.06.00210.1016/j.scriptamat.2004.06.002 ↗
41. 10.1016/j.jallcom.2020.15375910.1016/j.jallcom.2020.153759 ↗
42. 10.1016/j.euromechsol.2022.10454010.1016/j.euromechsol.2022.104540 ↗
43. 10.1016/j.actamat.2020.02.01910.1016/j.actamat.2020.02.019 ↗
44. 10.1111/j.1365-2818.2005.01449.x10.1111/j.1365-2818.2005.01449.x ↗
45. 10.1016/j.jnucmat.2018.06.02010.1016/j.jnucmat.2018.06.020 ↗
46. 10.1016/j.msea.2019.02.03610.1016/j.msea.2019.02.036 ↗
47. 10.1016/j.msea.2018.04.07710.1016/j.msea.2018.04.077 ↗
48. 10.1016/j.actamat.2010.06.02810.1016/j.actamat.2010.06.028 ↗
49. 10.1016/0956-7151(91)90179-510.1016/0956-7151(91)90179-5 ↗
50. 10.1023/A:101798911868610.1023/A:1017989118686 ↗
51. 10.1361/10599490277034389010.1361/105994902770343890 ↗
52. 10.1557/jmr.2017.1710.1557/jmr.2017.17 ↗
53. 10.3390/ma1312286010.3390/ma13122860 ↗
54. 10.1016/j.vacuum.2017.12.03510.1016/j.vacuum.2017.12.035 ↗
55. 10.1016/j.msea.2018.10.09310.1016/j.msea.2018.10.093 ↗
56. 10.1016/j.msea.2020.13900910.1016/j.msea.2020.139009 ↗
57. 10.1016/S1003-6326(20)65490-510.1016/S1003-6326(20)65490-5 ↗
58. 10.1016/j.jallcom.2020.15576210.1016/j.jallcom.2020.155762 ↗
59. 10.1007/s10853-007-2159-810.1007/s10853-007-2159-8 ↗
60. 10.1016/j.msea.2020.14012010.1016/j.msea.2020.140120 ↗
61. 10.1016/j.jallcom.2017.03.06910.1016/j.jallcom.2017.03.069 ↗
62. 10.1016/j.jallcom.2017.01.35510.1016/j.jallcom.2017.01.355 ↗
63. 10.1016/j.jallcom.2020.15677610.1016/j.jallcom.2020.156776 ↗
64. 10.1016/j.jallcom.2018.04.15910.1016/j.jallcom.2018.04.159 ↗