Review Type IV cracking in ferritic power plant steels
Source abstract
Abstract
There have been concerted world wide efforts to develop steels suitable for use in efficient fossil fired power plants. Ferritic alloys containing between 9 and 12 wt-% chromium are seen as the most promising materials in this respect, especially for thick walled components such as headers and the main steam pipe in boilers. However, the performance of the improved steels has often not been realised in service, because premature failures occur in the heat affected zone of welded joints in a phenomenon referred to as type IV cracking. This review assesses the relationship between the composition and microstructure of 9–12 Cr steels, the welding and fabrication procedures and how these factors translate into a propensity for type IV failures.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: High Temperature Alloys and Creep · Hydrogen embrittlement and corrosion behaviors in metals · Microstructure and Mechanical Properties of Steels
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (53)
Show source-provided references
1. Cerjak H.: Proc. Int. Conf. on ‘Achievements and perspectives in producing welded construction for urban environments’, 56th IIW Annual Assembly, Bucharest, Romania, July 2003, ASR,15–24.
2. 10.2355/isijinternational.41.62610.2355/isijinternational.41.626 ↗
3. 10.1179/13621710422501710710.1179/136217104225017107 ↗
4. 10.1179/13621710322500544410.1179/136217103225005444 ↗
5. 10.1016/S0308-0161(01)00090-410.1016/S0308-0161(01)00090-4 ↗
6. Lundin C. D., Liu P., and Cui Y. ‘A literature review on characteristics of high temperature ferritic Cr—Mo steels and weldments’, WRC bulletin 454, Welding Research Council, Inc., New York, NY, USA, 2000.
7. ‘Metals handbook’, 10th edn,Vol. 1, ‘Elevated temperature properties of ferritic steels’, 617-652; 1990, Materials Park, OH, ASM International.10.31399/asm.hb.v01.a0001035 ↗
8. 10.2355/isijinternational.41.Suppl_S12610.2355/isijinternational.41.Suppl_S126 ↗
9. 10.1179/09506600422502193610.1179/095066004225021936 ↗
10. Haarmann K., Vaillant J. C., Vandenberghe B., Bendick W., and Arbab A. ‘The T91/P91 book’; 2002, Boulogne, Vallourec & Mannesmann Tubes.
11. Richardot D., Vaillant J. C., Arbab A., and Bendick W. ‘The T92/ P92 book’; 2000, Boulogne, Vallourec & Mannesmann Tubes.
12. 10.2172/549888510.2172/5498885 ↗
13. Iwanaga K., Tsuchiyama T., and Takaki S.: Key Eng. Mater., 2000, 171-174,477–482.10.4028/www.scientific.net/KEM.171-174.477 ↗
14. Abe F.: Key Eng. Mater., 2000, 171-174,395–402.10.4028/www.scientific.net/KEM.171-174.395 ↗
15. Hasegawa Y., Muraki T., Ohgami M., and Mimura H.: Key Eng. Mater., 2000, 171-174,427–436.10.4028/www.scientific.net/KEM.171-174.427 ↗
16. 10.3139/146.10108610.3139/146.101086 ↗
17. 10.1179/stw.1996.1.1.3610.1179/stw.1996.1.1.36 ↗
18. 10.1179/mst.1996.12.7.55210.1179/mst.1996.12.7.552 ↗
19. Papst I. L. · Metallkd · 2004 · 95 · 1810.3139/146.017905 ↗
20. 10.1179/13621710422501711610.1179/136217104225017116 ↗
21. 10.1007/s11661-004-0299-x10.1007/s11661-004-0299-x ↗
22. 10.1007/s11661-005-0306-x10.1007/s11661-005-0306-x ↗
23. Tabuchi M. · Mater. Sci. Res. Int · 2003 · 9 · 23
24. Marshall A. W., Zhang Z., and Holloway G. B.: Proc. 5th Int. Conf. on ‘Welding and repair technology for power plants’, Point Clear, AL, USA, June 2002, Electric Power Research Institute.
25. Bergquist E. L. · Svetsaren · 1999 · 54 · 22
26. 10.1179/174329305X3603410.1179/174329305X36034 ↗
27. 10.2355/isijinternational.42.149710.2355/isijinternational.42.1497 ↗
28. 10.1016/S0308-0161(03)00072-310.1016/S0308-0161(03)00072-3 ↗
29. Mannan S. L. · Trans. Ind. Inst. Met · 1996 · 49 · 303
30. 10.1016/j.ijpvp.2004.01.00310.1016/j.ijpvp.2004.01.003 ↗
31. Tabuchi M., Watanabe T., Kubo K., Kinugawa J., and Abe F.: Key Eng. Mater., 2000, 171-174,521–528.10.4028/www.scientific.net/KEM.171-174.521 ↗
32. 10.2355/isijinternational.35.128410.2355/isijinternational.35.1284 ↗
33. 10.2355/isijinternational.42.157810.2355/isijinternational.42.1578 ↗
34. 10.1115/1.163102510.1115/1.1631025 ↗
35. 10.2355/isijinternational.44.196610.2355/isijinternational.44.1966 ↗
36. Francis J. A., Mazur W., and Bhadeshia H. K. D. H.: Proc. 7th Int. Conf. on ‘Trends in welding research’, Pine Mountain, GA, USA, May 2005, ASM International.
37. 10.1179/02670839910150608510.1179/026708399101506085 ↗
38. 10.1007/s11661-005-0143-y10.1007/s11661-005-0143-y ↗
39. 10.1179/174329305X2951910.1179/174329305X29519 ↗
40. 10.1179/02670830010150698410.1179/026708300101506984 ↗
41. 10.1007/s11661-005-0305-y10.1007/s11661-005-0305-y ↗
42. 10.1533/wint.2005.337710.1533/wint.2005.3377 ↗
43. 10.1533/wint.2005.337810.1533/wint.2005.3378 ↗
44. 10.1016/S0029-5493(99)00232-010.1016/S0029-5493(99)00232-0 ↗
45. 10.1016/j.ijpvp.2003.12.01710.1016/j.ijpvp.2003.12.017 ↗
46. 10.1179/174329305X2946510.1179/174329305X29465 ↗
47. 10.1115/1.135952710.1115/1.1359527 ↗
48. 10.1243/030932400151442210.1243/0309324001514422 ↗
49. 10.1016/j.jmatprotec.2005.05.03610.1016/j.jmatprotec.2005.05.036 ↗
50. Li D. · Sci. Technol · 2003 · 19 · 1253
51. 10.1243/030932498151291310.1243/0309324981512913 ↗
52. 10.1016/S0308-0161(99)00051-410.1016/S0308-0161(99)00051-4 ↗
53. 10.1016/S0308-0161(03)00134-010.1016/S0308-0161(03)00134-0 ↗