Influence of Mo and Al co-addition on the crystallization behavior and soft magnetic properties of FeBSiCuNb alloys
Source abstract
Abstract
The synergistic co-addition of trace Mo and Al provides an effective pathway to regulate nanocrystallization in Fe-based soft magnetic alloys through concurrent thermodynamic and kinetic control. In this work, the crystallization behavior, microstructural evolution, and soft magnetic properties of Fe 80.5 B 12 Si 4 Cu 1.5 Nb 1 Mo x Al 1- x ( x = 0.2, 0.4, 0.6 & 0.8 at.%) alloys were systematically investigated. Differential scanning calorimetry reveals a typical two-stage crystallization behavior, in which the primary crystallization peak originates from the overlap of pre-existing nucleus growth and newly activated nucleation processes. The Mo/Al ratio is found to strongly affect the thermal stability of the amorphous precursor and the nanocrystallization temperature window. Al addition promotes the formation of high-density pre-existing nuclei, while Mo effectively suppresses grain coarsening by increasing the kinetic barrier for atomic diffusion during annealing. As a result, an optimized nanocrystalline α-Fe(Si) structure is obtained after annealing. Among all the investigated alloys, the one with x = 0.6 exhibits a refined nanocrystalline microstructure with an average grain size of approximately 20.9 nm, achieving a favorable combination of high saturation magnetic flux density (1.671 T) and low coercivity (12.45 A/m). These results demonstrate that balancing thermodynamically promoted nucleation and kinetically inhibited growth via Mo/Al co-addition is an effective strategy for developing high-performance Fe-rich nanocrystalline soft magnetic alloys.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Metallic Glasses and Amorphous Alloys · Microstructure and mechanical properties · Magnetic Properties of Alloys
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (37)
Show source-provided references
1. Advances in high magnetic induction and low loss Fe-based nanocrystalline alloys
2. Effect of Fe content on crystallization behavior and soft magnetic properties in FINEMET-type alloys10.1016/j.matlet.2021.130759 ↗
3. Enhanced Ms of Fe-rich Fe-B-cu amorphous/nanocrystalline alloys achieved by annealing treatments10.1016/j.jallcom.2022.168621 ↗
4. Modern soft magnets: amorphous and nanocrystalline materials10.1016/j.actamat.2012.10.040 ↗
5. Random anisotropy effects in soft magnetic nanocrystalline materials10.1016/j.physb.2005.10.061 ↗
6. The microstructure evolution of a Fe73.5Si13.5B9Nb3Cu1 nanocrystalline soft magnetic material10.1016/0956-7151(92)90131-W ↗
7. Modulating magnetic properties of high entropy soft FeSiB(P)cu alloys with excellent GFA via α-Fe(Si) grain preferential growth mechanism10.1007/s42114-024-00952-0 ↗
8. Formation and crystallization behavior of Fe-based amorphous precursors with pre-existing α-Fe nanoparticles—structure and magnetic properties of high-cu-content Fe-Si-B-cu-Nb nanocrystalline alloys10.1016/j.jmst.2020.05.049 ↗
9. Optimizing nanostructure and magnetic softness of Fe-Si-B-cu nanocrystalline alloys via tailoring melt-spun structure by Al microalloying
10. Ultrahigh permeability at high frequencies via a magnetic-heterogeneous nanocrystallization mechanism in an iron-based amorphous alloy10.1002/adma.202304490 ↗
11. Microstructure and magnetic properties of Fe72.5Cu1M2V2Si13.5B9 (M=Nb, Mo, (NbMo), (MoW)) nanocrystalline alloys10.1016/j.jmmm.2010.05.008 ↗
12. Fine-grained high-permeability Fe73.5−xB9Si14Cu1Nb2.5Mx (M=Mo or W) nanocrystalline alloys with co-added heterogeneous transition metal elements10.3390/met14121424 ↗
13. Composition dependence of the microstructure and soft magnetic properties of Fe-based amorphous/nanocrystalline alloys: a review study10.1016/j.jnoncrysol.2014.03.010 ↗
14. Influence of boron content on glass forming ability and soft magnetic properties in Fe-Si-B-Nb-cu nanocrystalline alloys for gas atomization10.4283/JMAG.2025.30.3.249 ↗
15. Theoretical prediction and experimental validation of the glass-forming ability and magnetic properties of Fe-Si-B metallic glasses from atomic structures10.3390/ma15093149 ↗
16. Finemet nanocrystalline soft magnetic alloy: investigation of glass forming ability, crystallization mechanism, production techniques, magnetic softness and the effect of replacing the main constituents by other elements10.1016/j.jmmm.2016.02.057 ↗
17. Crystallization behavior, soft magnetic properties and good bending ductility of high Fe content FeSiBCuPC alloys induced by composition design10.1016/j.jallcom.2020.157850 ↗
18. Effect of Mo addition on thermal stability and magnetic properties in FeSiBPCu nanocrystalline alloys10.1016/j.jnoncrysol.2023.122279 ↗
19. Glass-forming ability and crystallization behavior of Mo-added Fe82−xSi4B12Nb1MoxCu1 (x = 0–2) nanocrystalline alloy10.3390/met15070744 ↗
20. Soft magnetic Fe-Si-B-cu nanocrystalline alloys with high cu concentrations10.1016/j.jallcom.2017.06.128 ↗
21. Al addition effect on structure and magnetic properties in high Bs Fe-cu-Si-B alloys10.1016/j.materresbull.2018.11.036 ↗
22. Scherrer grain-size analysis adapted to grazing-incidence scattering with area detectors10.1107/S0021889809040126 ↗
23. The effect of grain-size distribution on coercivity in nanocrystalline soft magnetic alloys10.1016/j.jmmm.2003.12.368 ↗
24. Recent advances in nanocrystalline soft magnetic materials: a critical review for way forward10.1016/j.jmmm.2023.171677 ↗
25. Magnetic softening of the Fe83Si3B11P2Cu1 amorphous/nanocrystalline alloys with large-size pre-existing α-Fe grains by high heating-rate annealing10.1016/j.jmrt.2022.07.051 ↗
26. High Bs nanocrystalline alloy with excellent soft magnetic properties achieved based on regulating amorphous matrix structure via two-step annealing10.1016/j.intermet.2025.108813 ↗
27. Effect of 0.5 at.% cu addition on the crystallization behavior and soft magnetic properties of Fe83B11C1Si2P3 alloy10.1016/j.jallcom.2024.174267 ↗
28. A method for kinetic analysis of thermoanalytical data of competitive reactions10.1016/0040-6031(94)85134-4 ↗
29. Structural evolution and crystallization kinetics of Fe-based amorphous alloys under ultrasonic vibrations treatment10.1016/j.jallcom.2025.180928 ↗
30. Effect of pre-existing nuclei on microstructure and magnetic properties of high bs FINEMET-like nanocrystalline alloys10.1007/s10853-021-05861-x ↗
31. Non-isothermal crystallization behavior of poly(ethylene terephthalate)/poly(trimethylene terephthalate) blends10.1007/s00289-007-0832-3 ↗
32. Nanocrystallization kinetics of amorphous Fe-based multicomponent alloy by non-isothermal analysis10.4028/www.scientific.net/MSF.570.109 ↗
33. Effect of Ge addition on magnetic properties and crystallization mechanism of FeSiBPNbCu nanocrystalline alloy with high Fe content10.3390/met12040640 ↗
34. Nonisothermal crystallization kinetics by DSC: practical overview10.3390/pr11051438 ↗
35. The applicability of Johnson-Mehl-Avrami model in the thermal analysis of the crystallization kinetics of glasses10.1016/0040-6031(95)02466-2 ↗
36. AI-driven precision annealing for high performance Fe-based amorphous alloys10.1002/eem2.70227 ↗
37. A method for the non-isothermal crystallization kinetics of polymers10.3724/SP.J.1105.2008.00656 ↗