Penetration and characteristics of an intergranular-liquid phase during sintering of CaSi2O5-dropped 8 mol%-yttria-stabilized zirconia estimation by impedance spectroscopy
Source abstract
Abstract
Abstract The grain-boundary resistivity of CaSi 2 O 5 -dropped 8 mol%-yttria-stabilized zirconia (8YSZ) was determined by impedance spectroscopy using sub-millimeter-scale electrodes. During sintering, a liquid that formed at the top surface of the specimen penetrated into the 8YSZ and induced enhanced grain growth near the surface region. The grain-boundary resistivity of the specimen surface was observed to be 150 times higher than that of the interior. The deterioration of the grain-boundary conductivity was explained in terms of the presence of an intergranular siliceous phase.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Advanced ceramic materials synthesis · Metal Extraction and Bioleaching
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (9)
Show source-provided references
1. Kuš č er · Solid State Ionics · 1995 · 78 · 7910.1016/0167-2738(95)00010-4 ↗
2. Clausen · Solid State Ionics · 1994 · 70/71 · 5910.1016/0167-2738(94)90287-9 ↗
3. Lee · J. Am. Ceram. Soc. · 2002 · 85 · 162210.1111/j.1151-2916.2002.tb00324.x ↗
4. Lee · J. Eur. Ceram. Soc. · 2001 · 21 · 1310.1016/S0955-2219(00)00167-9 ↗
5. Han · Acta metall. mater. · 1995 · 43 · 3183
6. Shackelford · J. Am. Ceram. Soc. Bull. · 1974 · 53 · 865
7. Aoki · J. Am. Ceram. Soc. · 1996 · 79 · 116910.1111/j.1151-2916.1996.tb08569.x ↗
8. Mecartney · J. Am. Ceram. Soc. · 1987 · 70 · 5410.1111/j.1151-2916.1987.tb04853.x ↗
9. Miyayama · Am. Ceram. Soc. Bull. · 1986 · 65 · 660