journal article·2004-01

Low K dielectrics in sintered Al–Zr oxide composites processed by thermal plasma heating

D.R. Sahu, S.K. Singh, R.N.P. Choudhury, B.K. Roul

Publisher page

Abstract

Abstract A simple and low cost heating technique based on extended arc thermal plasma heating (EATPH) source has been developed to sinter high temperature Al x –Zr 100− x ( x =0, 10, 20, …, 100) oxides. Structure and morphology of sintered Al–Zr oxide samples were studied by X-ray diffraction (XRD) and scanning electron microscope (SEM). Interesting result pertaining to the reduction of dielectric constant ( K ) and dielectric loss (tan δ ) were noted in thermal plasma sintered specimen as compared to the conventional sintered sample using resistive heating. It is observed that values of K are reduced up to 40% (maximum) w.r.t. conventional sintering. This low K behavior observed in thermal plasma sintered sample may be attributed to the incorporation of dynamic inclusion in different defect form during thermal plasma heating within a short sintering time. It is also further observed from the frequency and temperature variation of K and tan δ that surface charge polarization along with dipole screening play an important role at high frequencies and temperatures which can be explained by dipole pinning and depinning mechanisms.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Semiconductor materials and devices · Ferroelectric and Piezoelectric Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (28)

Show source-provided references
1. Morgan · JOM · 1999 · 51 · 3710.1007/s11837-999-0158-8 ↗
2. Treichel · J. Electron. Mater. · 2001 · 30 · 29010.1007/s11664-001-0033-z ↗
3. Li · Mater. Lett. · 2002 · 54 · 2510.1016/S0167-577X(01)00531-6 ↗
4. Grill · Appl. Phys. Lett. · 2001 · 79 · 80310.1063/1.1392976 ↗
5. Mckittrick · Mater. Res. Symp. Proc. · 1992 · 274 · 14810.1557/PROC-274-149 ↗
6. Freim · Nano Struct. Mater. · 1994 · 4 · 37110.1016/0965-9773(94)90108-2 ↗
7. J. Freim, J. McKittrick, J. Katz, K. Sickafus, Mater. Res. Soc. Proc. 347 (1994).10.1557/PROC-347-525 ↗
8. Wore · Met. Powder Rep. · 1999 · 54 · 24
9. Roul · J. Mater. Synth. Proc. · 1998 · 6 · 910.1023/A:1022698823898 ↗
10. Jain · Res. Ind. · 1990 · 35 · 23
11. Sisson · Nano Struct. Mater. · 1998 · 10 · 82910.1016/S0965-9773(98)00119-6 ↗
12. Saha · J. Mater. Sci. · 1998 · 17 · 1333
13. Gavruilov · J. Am. Ceram. Soc. · 1999 · 72 · 100110.1111/j.1151-2916.1999.tb01866.x ↗
14. Becher · J. Am. Ceram. Soc. · 1998 · 76 · 65710.1111/j.1151-2916.1993.tb03656.x ↗
15. Lamas · J. Mater. Sci. · 2000 · 35 · 556310.1023/A:1004896727413 ↗
16. P.R. Taylor, M. Manrique, JOM (June 1996) 43.10.1007/BF03222966 ↗
17. Taylor · Adv. Perform. Mater. · 1994 · 1 · 3510.1007/BF00705312 ↗
18. Kong · Ceram. Trans. · 1988 · 1 · 939
19. Bhattacharjee · Mater. Lett. · 1991 · 11 · 5910.1016/0167-577X(91)90190-H ↗
20. Sahu · J. Mater. Design Applic. · 2002 · 216L · 127
21. P. Debye, Polar Molecules, Chemical Catalog Company, New York, 1929.
22. Szigeti · Trans. Faraday Soc. · 1949 · 45 · 15510.1039/tf9494500155 ↗
23. Szigeti · Proc. R. Soc. (Lond.) · 1950 · A204 · 5110.1098/rspa.1950.0161 ↗
24. Szigeti · Proc. R. Soc. (Lond.) · 1959 · A252 · 21710.1098/rspa.1959.0148 ↗
25. Szigeti · Proc. R. Soc. (Lond.) · 1960 · A258 · 37710.1098/rspa.1960.0194 ↗
26. Rao · J. Appl. Phys. · 1965 · 36 · 203110.1063/1.1714397 ↗
27. A.K. Janscher, Universal Relaxation Law Chelsea Dielectric Press, London, 1996.
28. Sahu · Mater. Lett. · 2002 · 56 · 81710.1016/S0167-577X(02)00620-1 ↗