Abstract

Abstract We investigated the relation of potassium contamination on a crystalline silicon (c-Si) surface after potassium hydroxide (KOH) etching to the lifetime of the c-Si solar cell. Alkaline solution was employed for saw damage removal (SDR), texturing, and planarization of a textured c-Si solar wafer prior to atomic layer deposition (ALD) Al 2 O 3 growth. In the solar-cell manufacturing process, ALD Al 2 O 3 passivation is utilized to obtain higher conversion efficiency. ALD Al 2 O 3 shows excellent surface passivation, though minority carrier lifetime varies with cleaning conditions. In the present study, we investigated the relation of potassium contamination to lifetime in solar-cell processing. The results showed that the potassium-contaminated samples, due to incomplete cleaning of KOH, had a short lifetime, thus establishing that residual potassium can degrade Al 2 O 3 surface passivation.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Silicon and Solar Cell Technologies · Integrated Circuits and Semiconductor Failure Analysis · Thin-Film Transistor Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (23)

Show source-provided references
1. Saint-Cast · Appl. Phys. Lett. · 2009 · 95 · 15150210.1063/1.3250157 ↗
2. Schmidt · Prog. Photovolt. Res. Appl. · 2008 · 16 · 46110.1002/pip.823 ↗
3. Dingemans · Electrochem. Solid-State Lett. · 2011 · 14 · H110.1149/1.3501970 ↗
4. Hoex · J. Appl. Phys. · 2008 · 104 · 04490310.1063/1.2963707 ↗
5. Kim · Mat. Sci. Eng. B · 2012 · 177 · 21710.1016/j.mseb.2011.12.027 ↗
6. Agostinelli · Sol. Energy Mater. Sol. Cells · 2006 · 90 · 343810.1016/j.solmat.2006.04.014 ↗
7. Mulligan · Proceedings of the 19th EU-PVSEC · 2004 · 387
8. Hezel · 2000 · 1091
9. Schneiderlöchner · 2004 · 447
10. Blakers · 1989 · 801
11. Werner · J. Appl. Phys. · 2011 · 109 · 11370110.1063/1.3587227 ↗
12. Angermann · Mat. Sci. Eng. B · 2009 · 159–160 · 21910.1016/j.mseb.2008.10.044 ↗
13. Hoex · Phys. Status Solidi · 2012 · 6 · 410.1002/pssr.201105445 ↗
14. Lucovsky · Appl. Surf. Sci. · 2000 · 166 · 49710.1016/S0169-4332(00)00482-7 ↗
15. Bordihn · Energy Procedia · 2011 · 8 · 65410.1016/j.egypro.2011.06.197 ↗
16. Breitenstein · 2011
17. Lee · Korean Chem. Eng. Res. · 2007 · 45 · 203
18. Shah · Cryst. Growth Des. · 2009 · 9 · 431510.1021/cg900137h ↗
19. Ciraci · Phys. Rev. B · 1988 · 37 · 295510.1103/PhysRevB.37.2955 ↗
20. Palik · J. Appl. Phys. · 1991 · 70 · 329110.1063/1.349263 ↗
21. Michel · Phys. Rev. B · 1988 · 38 · 1339910.1103/PhysRevB.38.13399 ↗
22. Papet · Sol. Energy Mater. Sol. Cells · 2006 · 90 · 231910.1016/j.solmat.2006.03.005 ↗
23. Naumann · Energy Procedia · 2012 · 27 · 31210.1016/j.egypro.2012.07.069 ↗