journal article·2009-04

Joining of high damage tolerant SiC fabric to high strength SiC

Yoshihiro Hirata, Naoki Matsunaga, Takashi Arima, Soichiro Sameshima

Materials Science and Engineering: B· Volume 161· Issue 1-3
Publisher page

Abstract

Abstract SiC fabric including alumina or alumina–mullite particles was joined to the surfaces of dense SiC compact using an intermediate SiC–Al 2 O 3 or Al 2 O 3 –mullite powder layers under 2–39 MPa of applied pressure. The strength and damage tolerance using Vickers indentor were investigated for these laminates. The SiC fabric layers joined to oxidized dense SiC compact (800 MPa of flexural strength) through SiC–Al 2 O 3 sheet at 1300–1600 °C, prevented the propagation of the cracks formed by Vickers indentor. As a result, no change in the strength was measured before and after the introduction of cracks. However, increased joining pressure resulted in the formation of large crack inside SiC compact. Decrease of the joining pressure was effective to increase the flexural strength. It was also possible to join the SiC fabric layer including mullite powder to oxidized SiC compact through Al 2 O 3 –mullite intermediate layer at 1300 °C under 2 MPa of applied pressure. No cracks were observed inside of dense SiC compact. The key factor to join well the fabric layer was the oxidation condition of inside SiC compact before the joining. The thick layer of SiO 2 on the SiC surface reacted well with Al 2 O 3 powder in the intermediate Al 2 O 3 –mullite sheet to form mullite. The mullite powder in the SiC fabric layer was also connected to the mullite powder in the intermediate Al 2 O 3 –mullite sheet. The control of the above reaction was important to join the SiC fabric layer at a low applied pressure.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (19)

Show source-provided references
1. Dong · J. Ceram. Soc. Jpn. · 2003 · 111 · 91210.2109/jcersj.111.912 ↗
2. Kerans · Compos. Part A · 1999 · 30 · 52110.1016/S1359-835X(98)00144-4 ↗
3. Evan · J. Mater. Sci. · 1994 · 29 · 385710.1007/BF00355946 ↗
4. Davis · J. Am. Ceram. Soc. · 1993 · 76 · 124910.1111/j.1151-2916.1993.tb03749.x ↗
5. Hirata · J. Am. Ceram. Soc. · 2004 · 87 · 99610.1111/j.1551-2916.2004.00996.x ↗
6. Dong · J. Eur. Ceram. Soc. · 2004 · 24 · 5310.1016/S0955-2219(03)00127-4 ↗
7. Dong · J. Ceram. Soc. Jpn. · 2005 · 113 · 13510.2109/jcersj.113.135 ↗
8. Hirata · J. Am. Ceram. Soc. · 2000 · 83 · 104410.1111/j.1151-2916.2000.tb01328.x ↗
9. Hirata · J. Ceram. Soc. Jpn. · 2004 · 112 · S264
10. Arima · Key Eng. Mater. · 2007 · 352 · 4910.4028/www.scientific.net/KEM.352.49 ↗
11. Hirata · Mater. Sci. Forum · 2007 · 561–565 · 48910.4028/www.scientific.net/MSF.561-565.489 ↗
12. Ishikawa · Nature · 1998 · 391 · 77310.1038/35820 ↗
13. Arima · J. Ceram. Soc. Jpn. · 2008 · 116 · 51910.2109/jcersj2.116.519 ↗
14. Hidaka · 2004 · 109
15. Tabata · 2004 · 119
16. Hidaka · J. Ceram. Soc. Jpn. · 2005 · 113 · 46610.2109/jcersj.113.466 ↗
17. Hirata · J. Am. Ceram. Soc. · 2003 · 86 · 510.1111/j.1151-2916.2003.tb03269.x ↗
18. Hirata · Bull. Ceram. Soc. Jpn. · 1999 · 34 · 274
19. Aksay · J. Am. Ceram. Soc. · 1975 · 58 · 50710.1111/j.1151-2916.1975.tb18770.x ↗