Effect of annealing temperature on the structure and coke-resistance of nickel–iron bimetallic catalytic layer for in situ methane steam reforming in SOFC operation

Xuehua Liu, Hanqing Zhang, DanDan Zhao, Dian Tang, Teng Zhang

Publisher page

Abstract

Abstract In this paper, the effect on coke formation of adding a Ni 0.75 Fe 0.25 catalyst layer to the anode side of a fuel cell running on methane is investigated. The formation of an intermediate FeNi 3 phase can be observed in catalysts annealed at different temperatures. The catalyst annealed at 705 °C has the smallest calculated surface energy and grain size among all catalysts annealed at different temperatures. In addition, the O 2 -TPO profiles and Raman spectra of spent anode material reveal that the catalyst annealed at 705 °C has the best coke resistance among all catalysts. Moreover, the cell with catalyst layer annealed at 705 °C, under a current density of 600 mA cm −2 at 650 °C, experiences a decrease of 10% after operating in methane for 260 min, which is much more stable than that without catalyst layer (a decrease of 50%).
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Electrocatalysts for Energy Conversion · Advancements in Solid Oxide Fuel Cells · Fuel Cells and Related Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (30)

Show source-provided references
1. Liu · J. Power Sources · 2011 · 196 · 996510.1016/j.jpowsour.2011.08.023 ↗
2. Smorygo · Int. J. Hydrog. Energy · 2009 · 34 · 950510.1016/j.ijhydene.2009.09.079 ↗
3. Su · J. Power Sources · 2011 · 196 · 760110.1016/j.jpowsour.2011.04.056 ↗
4. Ahrenfeldt · Appl. Therm. Eng. · 2013 · 50 · 140710.1016/j.applthermaleng.2011.12.040 ↗
5. Choudhury · Sustain. Energy Rev. · 2013 · 20 · 43010.1016/j.rser.2012.11.031 ↗
6. Zhao · Int. J. Hydrog. Energy · 2013 · 38 · 1649810.1016/j.ijhydene.2013.07.077 ↗
7. Wang · Int. J. Hydrog. Energy · 2011 · 36 · 1095810.1016/j.ijhydene.2011.05.109 ↗
8. Wang · J. Power Sources · 2010 · 195 · 40210.1016/j.jpowsour.2009.07.053 ↗
9. Liao · J. Power Sources · 2011 · 196 · 617710.1016/j.jpowsour.2011.03.018 ↗
10. Wang · Int. J. Hydrog. Energy · 2012 · 37 · 860310.1016/j.ijhydene.2012.02.138 ↗
11. Zhu · Int. J. Hydrog. Energy · 2013 · 38 · 374110.1016/j.ijhydene.2013.01.032 ↗
12. Wang · J. Power Sources · 2011 · 196 · 9010.1016/j.jpowsour.2010.07.033 ↗
13. Wang · Int. J. Hydrog. Energy · 2011 · 36 · 563210.1016/j.ijhydene.2011.01.163 ↗
14. Wang · J. Power Sources · 2011 · 196 · 385510.1016/j.jpowsour.2010.12.072 ↗
15. Wang · Int. J. Hydrog. Energy · 2011 · 36 · 75510.1016/j.ijhydene.2010.09.048 ↗
16. Lin · Catal. Commun. · 2012 · 18 · 16810.1016/j.catcom.2011.12.002 ↗
17. Profeti · Int. J. Hydrog. Energy · 2009 · 34 · 274710.1016/j.ijhydene.2009.01.011 ↗
18. Lin · J. Power Sources · 2012 · 205 · 10010.1016/j.jpowsour.2012.01.033 ↗
19. Wu · Int. J. Hydrog. Energy · 2012 · 37 · 928710.1016/j.ijhydene.2012.03.034 ↗
20. Wang · Electrochim. Acta · 2009 · 54 · 387210.1016/j.electacta.2009.02.002 ↗
21. Kan · Catal. Commun. · 2010 · 12 · 3610.1016/j.catcom.2010.07.014 ↗
22. Park · J. Power Sources · 2009 · 186 · 13310.1016/j.jpowsour.2008.09.080 ↗
23. Zhu · Int. J. Hydrog. Energy · 2012 · 37 · 980110.1016/j.ijhydene.2012.03.060 ↗
24. Evarestov · Int. J. Quantum Chem. · 2004 · 100 · 45210.1002/qua.20188 ↗
25. Singh-Miller · Phys. Rev. B · 2009 · 80 · 23540710.1103/PhysRevB.80.235407 ↗
26. Yan · Phys. Rev. B · 2000 · 61 · 259510.1103/PhysRevB.61.2595 ↗
27. Zhang · Int. J. Hydrog. Energy · 2014 · 39 · 946710.1016/j.ijhydene.2014.03.263 ↗
28. Cuesta · Carbon · 1994 · 32 · 152310.1016/0008-6223(94)90148-1 ↗
29. Chen · J. Am. Ceram. Soc. · 2008 · 91 · 415410.1111/j.1551-2916.2008.02808.x ↗
30. Zhang · J. Am. Ceram. Soc. · 2007 · 90 · 98910.1111/j.1551-2916.2007.01503.x ↗