Processing of dense La0.2Sr0.8Fe0.8Cr0.2O3−δ oxygen membranes
Source abstract
Abstract
Abstract The effects of processing parameters on the microstructure and performance of La 0.8 Sr 0.2 Fe 0.8 Cr 0.2 O 3− δ processed by uni-axial and cold isostatic pressing followed by sintering have been studied. The sintering strain obtained from dilatometry measurements reveals negligible contraction below 1250 K and the commencement of rapid sintering above this temperature. The optimum sintering temperature with respect to density is 1523 K, resulting in 98.9% of the theoretical density. The decrease in density below this temperature is found to be due to open pore development resulting from slower sintering kinetics. Above the optimum temperature, the decrease in density is found to be caused by the close pore development during oxygen desorption. The dependence of the square of grain size on time is nonlinear with the time exponent equal to 0.7, indicating that there is a contribution to grain growth apart from surface free energy that retards the growth rate. The dependence of electrical conductivity on the inverse of absolute temperature exhibits a typical two-region dependence, reaching the maximum of 103 s cm −1 at 805 K.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Electronic and Structural Properties of Oxides · Magnetic and transport properties of perovskites and related materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (21)
Show source-provided references
1. Qiu · Solid State Ionics · 1995 · 76 · 32110.1016/0167-2738(94)00296-5 ↗
2. Balachandran · J. Am. Cer. Soc. Bull. · 1995 · 74 · 71
3. Minh · J. Am. Cer. Soc. Bull. · 1993 · 76 · 56310.1111/j.1151-2916.1993.tb03645.x ↗
4. Steele · Solid State Ionics · 1996 · 86-88 · 122310.1016/0167-2738(96)00291-3 ↗
5. Hiei · Solid State Ionics · 1996 · 86-88 · 126710.1016/0167-2738(96)00299-8 ↗
6. Schafer · Solid State Ionics · 1996 · 86-88 · 123510.1016/0167-2738(96)00292-5 ↗
7. Zhou · Solid State Ionics · 1997 · 93 · 13310.1016/S0167-2738(96)00483-3 ↗
8. Zhang · J. Mat. Sci. · 1999 · 34 · 136710.1023/A:1004518719410 ↗
9. Zhang · Mat. Res. Soc. Sym. Proc. · 2000 · 575 · 31510.1557/PROC-575-315 ↗
10. Garcia-Belmonte · Solid State Ionics · 1998 · 107 · 20310.1016/S0167-2738(97)00541-9 ↗
11. Majkic · Acta Materialia · 2000 · 48 · 190710.1016/S1359-6454(99)00472-3 ↗
12. Wolfenstine · Electrochemical and Solid-State Letters · 1999 · 2 · 21010.1149/1.1390786 ↗
13. Goretta · Solid State Ionics · 1998 · 111 · 29510.1016/S0167-2738(98)00176-3 ↗
14. Minh · 1995
15. Ming · Combustion Sci. Technol. · 1998 · 138 · 27910.1080/00102209808952072 ↗
16. Burke · 1952 · 220
17. Seidensticker · Acta Materialia · 1998 · 46 · 488310.1016/S1359-6454(98)00201-8 ↗
18. Kim · Solid State Ionics · 1997 · 104 · 5710.1016/S0167-2738(97)00427-X ↗
19. Stevenson · J. Electrochemical Soc. · 1996 · 143 · 272210.1149/1.1837098 ↗
20. Chiang · 1997 · 375
21. Gordon · J. Am. Cer. Soc. · 1973 · 56 · 14710.1111/j.1151-2916.1973.tb15431.x ↗