journal article·2001-09

Large current density and anodization time needed for strong photoluminescence in porous silicon

Masato Ohmukai, Masaki Taniguchi, Yasuo Tsutsumi

Publisher page

Abstract

Abstract We investigated the relation between anodization conditions and photoluminescent characteristics including spatial variations. The current density was between 7.9 and 39 mA cm −2 , and the anodization time between 10 and 60 min. We clarified a generous tendency as follows: as the current density or the anodization time increases, the edge of the anodized area gives the stronger photoluminescence at first, and then the center also gives the stronger photoluminescence. In addition, we reported the difference between luminescing and non-luminescing porous silicon, from the aspects of photoluminescent, photoacoustic, and Raman spectra.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Silicon Nanostructures and Photoluminescence · Nanowire Synthesis and Applications · Semiconductor materials and devices

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (6)

Show source-provided references
1. Fauchet · 1998 · 49 · 206
2. Namavar · Appl. Phys. Lett. · 1992 · 60 · 251410.1063/1.106951 ↗
3. Linnros · Appl. Phys. Lett. · 1995 · 66 · 304810.1063/1.114273 ↗
4. Fujiwara · Jpn. J. Appl. Phys. · 1992 · 31 · L176310.1143/JJAP.31.L1763 ↗
5. Ohmukai · Thin Solid Films · 1997 · 302 · 5110.1016/S0040-6090(96)09566-1 ↗
6. Ohmukai · Jpn. J. Appl. Phys. · 1997 · 36 · L29210.1143/JJAP.36.L292 ↗